PTFE (テフロン)

PTFE (Polytetrafluoroethylene), commonly known as Teflon, is famous for having the lowest coefficient of friction of any solid material and near-universal chemical resistance. It is the ultimate choice for seals, gaskets, and high-temperature insulators. However, PTFE is notoriously soft and difficult to hold tolerances on due to high thermal expansion and creep ("cold flow"). Jucheng Precision excels in Soft Plastic Machining. We use specialized sharp tooling and temperature-controlled machining environments to prevent deformation. Our CNC turning centers are optimized to produce complex PTFE seals and bushings with burr-free edges and surface finishes that maintain the material's sealing integrity. Whether you need FDA-approved Virgin PTFE or wear-resistant Glass/Bronze Filled grades, we deliver precision parts for chemical and aerospace applications.

CNC PTFE Machining

当社で取り扱う材料

Virgin PTFE

The highest purity grade, offering 99.9% pure Teflon performance. It features the lowest coefficient of friction and near-universal chemical resistance. FDA-compliant and biostable, it is the gold standard for medical fluidics, chemical seals, and high-frequency electrical insulators.

READ MORE

Mechanical PTFE

An economical, reprocessed grade designed for industrial applications. While offering slightly lower mechanical properties than virgin resin, it retains excellent chemical resistance and low friction. It is the cost-effective solution for manufacturing industrial spacers, gaskets, and non-critical wear pads.

READ MORE

Glass Filled PTFE

Reinforced with glass fibers to drastically reduce "cold flow" (creep) and improve compressive strength. This grade maintains the chemical resistance of Teflon while offering the structural integrity required for high-pressure valve seats, gaskets, and structural industrial seals.

READ MORE

Bronze Filled PTFE

The ultimate tribological grade for heavy-duty sliding. The addition of bronze powder maximizes wear life and thermal conductivity, effectively dissipating frictional heat. It is specifically designed for high-load hydraulic guide rings, piston seals, and heavy-duty industrial bearings.

READ MORE

Available PTFE (Teflon) Grades

グレード 一般名 主な特性 代表的な用途
Virgin PTFE Electrical Grade Pure white. Excellent chemical resistance, electrical insulation, and lowest friction. FDA compliant. Chemical seals, electrical insulators, medical tubing, food processing parts.
Mechanical PTFE Reprocessed PTFE Made from recycled resin. Lower tensile strength and purity but more cost-effective. Not FDA compliant. Non-critical spacers, washers, wear pads.
Glass-Filled PTFE 15% / 25% Glass Reinforced with glass fibers to improve compressive strength and reduce cold flow (creep). Valve seats, gaskets, piston rings, structural chemical parts.
Bronze-Filled PTFE Bearing Grade Bronze powder added for superior wear resistance and thermal conductivity. Higher friction than virgin. Hydraulic cylinder guides, bearings, slider plates.

PTFE Machining Capabilities

能力 技術的説明 Juchengの強み
Complex Seal Turning Machining intricate lip profiles and grooves for hydraulic and pneumatic seals. Our specialized lathe setups ensure burr-free cuts, critical for maintaining a perfect vacuum or fluid seal.
Thin-Wall Machining Creating thin insulating sleeves and liners without deforming the soft material. We use air chucks and mandrels to support the part, achieving wall thicknesses as low as 0.5mm.
Surface Finishing Achieving smooth sealing surfaces (Ra 0.8 or better) directly off the machine. Eliminates leakage paths in high-purity chemical or semiconductor applications.
Stress-Free Handling Managing the material’s tendency to “squirm” or change size with temperature. We machine in a temperature-controlled environment to ensure dimensions hold true at 20°C.

Fabrication Guidelines for PTFE

クランプ感度:
PTFE is extremely soft and prone to deformation. Excessive clamping force will ruin the part. We use vacuum fixtures, potting, or soft jaws that encapsulate the part to distribute force.

Thermal Expansion:
PTFE has a very high coefficient of thermal expansion (CTE) and undergoes a phase transition at ~19°C where it expands significantly. We recommend machining and inspecting at stable room temperatures.

工具:
Extremely sharp, high-rake carbide tools are required. Dull tools will compress the material rather than cut it, causing size issues and burrs.

Deburring:
Burrs on PTFE are stringy and difficult to remove. We use cryogenic deburring or manual trimming under microscopes for critical medical parts.

Primary Application Industries

Chemical Processing
Key Parts: Valve seats, pump diaphragms, pipe gaskets.
Why PTFE: Universal chemical inertness prevents corrosion from acids and solvents.

Food & Medical
Key Parts: Mixing paddles, surgical guides, fluid seals.
Why PTFE: FDA compliance, non-stick surface (easy to clean), and high-temperature sterilization resistance.

航空宇宙
Key Parts: Wire insulation, fuel hose liners, standoff insulators.
Why PTFE: Excellent dielectric properties and remains flexible at cryogenic temperatures.

自動車
Key Parts: Shock absorber seals, power steering seals, bearings.
Why PTFE: Low friction coefficient reduces wear and improves efficiency in moving parts.

Material Properties

密度 2.15 - 2.20 g/cm³
引張強度 20 - 35 MPa
破断伸び 200 - 400 %
熱変形温度 50 - 120 °C
硬さ 50 - 65 Shore D
連続使用温度 260 °C
吸水率 < 0.01 %
絶縁破壊強度 20 - 60 kV/mm
融点 327 °C
Max. Part Size 2000 mm (L) x 800 mm (W) x 600 mm (H)