PEEK CF30

PEEK CF30 is the strongest and most rigid grade of PEEK, reinforced with 30% high-modulus carbon fibers. This high-performance polymer offers mechanical properties that rival many non-ferrous metals while being significantly lighter. It features the lowest thermal expansion coefficient in the PEEK family and superior wear resistance under high-load conditions. Jucheng Precision utilizes specialized diamond tooling and high-torque CNC machines to master the challenges of this abrasive material. We deliver mission-critical PEEK CF30 components for aerospace structural frames, oilfield wear parts, and automotive racing assemblies where failure is not an option.

PEEK CF30

PEEK CF30 Machining Capabilities

역량 기술 설명 Jucheng의 강점
Diamond Tooling (PCD) Carbon fiber is extremely abrasive. We utilize Polycrystalline Diamond (PCD) and specialized CVD diamond-coated tools to maintain edge sharpness. Ensures consistent dimensions and superior surface finish on large batches, preventing tool-wear induced tolerance drift.
High-Load 5-Axis Milling Machining the strongest PEEK variant into complex structural geometries with organic curves and undercuts. Our rigid 5-axis Haas/Mazak machines handle the high-stiffness CF30 without deflection, ensuring perfect alignment of gears and splines.
EMI/RFI Shielding Features Machining internal pockets and fine features in CF30 housings to utilize its inherent electrical conductivity for shielding. We provide precision-milled enclosures that offer built-in electromagnetic protection for sensitive aerospace electronics.
Precision Dimensional Control PEEK CF30 has the lowest thermal expansion coefficient of all PEEK grades. We hold tolerances to +/- 0.01mm. Perfect for components that must transition from cryogenic to high-heat environments without losing fitment or sealing.

Fabrication Guidelines for PEEK CF30

연마성 관리:
The 30% carbon fiber reinforcement acts like a grinding wheel on standard tools. 팁: We use ultra-rigid tool holders and high-performance diamond coatings to ensure the material is cut, not torn.

Dust Management:
Carbon fiber machining produces conductive black dust that can damage electronics. 팁: We utilize high-efficiency wet-milling filtration systems to safely evacuate dust and maintain a clean-room style machining environment.

Brittle Behavior:
PEEK CF30 is more brittle than virgin PEEK. 팁: We use optimized exit strategies and specific ramp-in moves to prevent splintering or “chipping” on sharp external corners.

Orientation Strength:
Like all fiber-filled plastics, strength is highest in the direction of the fibers. 팁: We analyze the part’s stress direction and orient the stock material to maximize mechanical performance in the finished part.

주요 응용 분야

Aerospace Structures
Wing components, engine zone brackets, and high-load pulleys where PEEK CF30 replaces metal to save weight while increasing stiffness.

Oil & Gas Downhole
Centrifugal pump components, wear rings, and seals operating in high-pressure, abrasive slurry environments.

Semiconductor & Vacuum
Wafer handling components and structural supports requiring low outgassing and high rigidity under thermal cycling.

High-Performance Motorsport
Suspension bushings, gears, and engine covers where extreme heat resistance and strength-to-weight ratio are critical.

속성

밀도 1.38 - 1.42 g/cm³
인장 강도 190 - 210 MPa
탄성 계수 13 - 18 GPa
경도 90 Shore D
열변형 온도 315 °C
연속 사용 온도 250 - 260 °C
흡수율 0.05%
전기 전도도 Conductive / Dissipative
열전도율 0.95 W/m-K
기계 가공성 등급 낮음
최대 부품 크기 2000 x 800 x 600 mm