Цинк

Zinc alloys (specifically the Zamak series) are staples in the automotive and consumer electronics industries due to their high strength, ductility, and ability to be cast into complex shapes. While Zinc is predominantly die-cast, CNC machining is critical for creating functional prototypes to validate designs before investing in expensive molds, or for performing precision secondary operations (drilling/tapping) on cast parts. Jucheng Precision, with its IATF 16949 certification, is an expert in machining Zinc automotive components. Our high-speed Haas/Mazak CNC machines effortlessly handle zinc alloys, delivering tight tolerances (+/- 0.01mm) and superior surface finishes. We also offer surface treatments like chromating and plating to enhance corrosion resistance.

CNC Zinc Machining

Наши доступные материалы

Выбрать Zinc Zamak 3 Zinc Zamak 3

The most widely used zinc alloy for functional prototyping. Zamak 3 offers an excellent balance of physical and mechanical properties, including high dimensional stability and impact strength. It is the standard choice for CNC machining prototypes that accurately simulate final die-cast automotive and electronic components.

ПОДРОБНЕЕ

Выбрать Zinc Zamak 5 Zinc Zamak 5

The high-strength variant of the Zamak family. Containing 1% copper, Zamak 5 is harder, stronger, and more creep-resistant than Zamak 3. It is ideally suited for structural automotive housings, heavy-duty latch mechanisms, and gears requiring superior mechanical performance and durable surface finishes.

ПОДРОБНЕЕ

Available Zinc Grades

Марка Обычное название Ключевые характеристики Типичные применения
Zamak 3 Zn-4Al The industry standard. Excellent balance of physical and mechanical properties. High dimensional stability. Automotive components, household hardware, electrical switchgear.
Zamak 5 Zn-4Al-1Cu Contains copper for higher tensile strength and hardness than Zamak 3. Slightly lower ductility. Automotive parts requiring higher strength, accessories, fittings.
ZA-8 Zinc-Aluminum Alloy Higher aluminum content. Can be gravity cast. Superior creep resistance and strength. Hydraulic components, decorative hardware.
ZA-12 Bearing Alloy Excellent bearing properties (good alternative to bronze). High hardness and strength. Bearings, bushings, wear plates.

Zinc Machining Capabilities

Возможность Техническое описание Преимущество Jucheng
Функциональное прототипирование CNC machining solid Zinc blocks to simulate die-cast parts (Zamak 3/5) for fit and function testing. Allows clients to validate designs and mechanical properties physically without paying for expensive die-casting molds.
Последующие операции Precision post-machining of die-cast zinc parts, including facing, boring, and tapping precise threads. Our automated setups ensure high repeatability for large batches of automotive housings.
High-Speed Drilling/Tapping Zinc is easy to machine; we utilize high-speed spindles to drill and tap holes rapidly. Significantly reduces cycle times and costs for parts requiring multiple fastening points.
Отделка поверхности Providing Chromate Conversion, Zinc Plating, or Powder Coating services. Enhances the natural corrosion resistance of Zinc and prepares it for harsh environments (Salt Spray Test compliant).

Fabrication Guidelines for Zinc

Инструмент:
Zinc is non-abrasive and soft. Standard high-speed steel (HSS) or uncoated carbide tools work excellently. Sharp cutting edges are required to prevent burrs on exit.

Закрепление заготовки:
Zinc is dense but can be brittle compared to aluminum. Care must be taken not to over-clamp thin-walled sections to avoid cracking or deformation. Soft jaws are recommended.

Coolant:
Water-soluble coolant is recommended to keep the part cool and flush away chips. While Zinc can be machined dry, coolant prevents the material from smearing on the tool.

Safety Note:
Zinc dust can be flammable, though less so than Titanium/Magnesium. Good housekeeping and chip management are standard protocols at Jucheng.

Основные отрасли применения

Automotive (IATF 16949)
Ключевые детали: Door lock housings, mirror brackets, seat belt components.
Why Zinc: High strength, dimensional stability, and ability to cast complex net-shape parts that require minimal machining.

Потребительская электроника
Ключевые детали: Laptop hinges, connector shields, chassis frames.
Why Zinc: Excellent EMI/RFI shielding properties and high-quality tactile feel (heavy/premium) for user interfaces.

Hardware & Construction
Ключевые детали: Window handles, locks, bathroom fixtures.
Why Zinc: Easily plated (Chrome/Nickel) for a decorative finish and durable enough for daily use.

Industrial Components
Ключевые детали: Gears, pulleys, motor housings.
Why Zinc: Self-lubricating properties (bearing bronze alternative) and vibration damping capabilities.

Свойства материала

Плотность 6.6 - 6.7 g/cm³
Предел прочности на растяжение 220 - 400 MPa
Предел текучести 200 - 300 MPa
Относительное удлинение при разрыве 2 - 10 %
Модуль упругости 85 - 96 GPa
Твёрдость 80 - 100 HB
Теплопроводность 105 - 115 W/m-K
Электропроводность 25 - 27 % IACS
Температура плавления 380 - 420 °C
Макс. размер детали 2000 мм (Д) x 800 мм (Ш) x 600 мм (В)