Zinc Zamak 3

Zamak 3 is the world's most widely used zinc alloy for die casting and precision CNC prototyping. Known for its excellent balance of physical and mechanical properties, it offers superior dimensional stability, high impact strength, and exceptional finishability. At Jucheng Precision, we specialize in both the functional CNC prototyping of Zamak 3 from solid billets and high-precision secondary machining for die-cast parts. As an IATF 16949 certified manufacturer, we leverage high-speed CNC centers to deliver zinc components for the automotive and electronics industries that require tight tolerances, complex internal features, and premium surfaces ready for decorative plating.

Zamak 3

Zamak 3 Machining Capabilities

القدرة الوصف الفني ميزة Jucheng
Functional Prototyping CNC machining solid Zamak 3 billets to simulate die-cast parts for fit and function testing before tooling. We provide accurate physical models that match the mechanical properties of final die-cast components, reducing development risk.
Secondary Operations Precision post-machining of die-cast zinc parts, including boring, facing, and high-tolerance tapping. Our automated setups ensure high repeatability for large batches of automotive and electronic housings.
ثقب عالي السرعة Zamak 3 is highly machinable. We utilize high-speed spindles for rapid drilling of intricate hole patterns. Significantly reduces cycle times and costs for parts requiring multiple assembly points or fastening features.
Surface Prep for Plating Machining surfaces to Ra 0.8μm or better to ensure high-quality adhesion for Chrome or Nickel plating. Delivers “Class A” cosmetic surfaces for consumer hardware and luxury automotive trim.

Fabrication Guidelines for Zamak 3 Zinc Alloy

Soft Material Strategy:
Zamak 3 is non-abrasive and relatively soft. نصيحة: We use sharp, uncoated carbide tools with high rake angles to prevent material smearing and ensure crisp exit edges.

حساسية تثبيت قطعة العمل:
Zinc is dense but can be more brittle than aluminum under high point loads. نصيحة: We use custom soft jaws to distribute clamping pressure evenly, preventing deformation or cracking of thin-walled housing sections.

Coolant Usage:
While zinc can be machined dry, water-soluble coolant is recommended to keep the part cool and flush away chips. نصيحة: This maintains dimensional stability and prevents the material from building up on the cutting edge.

Threading & Tapping:
Zamak 3 accepts threads excellently. نصيحة: We use roll taps (forming taps) for smaller holes to create stronger threads without producing extra chips in blind holes.

التطبيقات الأساسية

Automotive Components
Door lock housings, mirror brackets, and fuel system parts that require high dimensional stability and strength.

الإلكترونيات الاستهلاكية
Shielding cans, connector housings, and internal frames that benefit from zinc’s excellent EMI/RFI shielding properties.

Hardware & Locks
Precision lock cylinders, handles, and decorative bathroom fixtures that will be polished and Chrome plated.

الآلات الصناعية
Small gears, pulleys, and complex levers where zinc’s self-lubricating properties reduce wear on moving parts.

الخصائص

الكثافة 6.60 g/cm³
مقاومة الشد 283 MPa
مقاومة الخضوع 221 MPa
الصلابة 82 HB (Brinell)
الاستطالة عند الكسر 10%
التوصيل الحراري 113 W/m-K
التوصيل الكهربائي 27% IACS
نقطة الانصهار 381 - 387 °C
تقييم قابلية التشغيل جيد
مقاومة التآكل جيد
أقصى حجم للقطعة 2000 × 800 × 600 مم