Virgin PEEK (Unfilled) is the premier high-performance thermoplastic for critical engineering applications. It offers a unique combination of exceptional chemical resistance, high-temperature stability, and mechanical strength comparable to some metals. Its inherent biocompatibility and radiolucency make it the industry standard for medical implants. At Jucheng Precision, we specialize in the precision CNC machining of Virgin PEEK under strict ISO 13485 protocols. By utilizing advanced annealing techniques and high-speed 5-axis milling, we deliver complex PEEK components with tight tolerances and superior surface finishes for the medical, aerospace, and semiconductor sectors.
| 能力 | 技術的説明 | Juchengの強み |
|---|---|---|
| Stress-Free Machining | Implementing in-process annealing cycles to relieve internal stresses caused by material removal. | Prevents Virgin PEEK parts from warping or dimensional shifting over time, ensuring long-term precision for medical implants. |
| High-Precision Micro-Milling | Milling tiny, intricate features such as 0.3mm holes and micro-fluidic channels. | Our high-speed 5-axis machines achieve burr-free edges on delicate PEEK components, eliminating the need for manual deburring. |
| Swiss-Style Turning | Turning small-diameter dental implants and bone screws with high-precision thread whirling. | We hold ISO 13485 certification, guaranteeing contamination-free production and full traceability for all medical-grade PEEK parts. |
| 表面平滑化 | Achieving Ra 0.4μm surface finishes through optimized tool paths and fine-grain carbide tooling. | Critical for sealing surfaces in analytical instruments and smooth contact faces in orthopedic devices. |
Thermal Management:
PEEK has low thermal conductivity. Heat generated during cutting stays in the part. ヒント: We use sharp tools and high-flow clean coolant (or air blast) to prevent the plastic from softening or expanding during the cut.
Annealing Requirements:
To achieve tight tolerances, we recommend rough machining, followed by a secondary annealing cycle, and then final finishing. ヒント: This is essential for large PEEK parts to ensure they remain dimensionally stable throughout their service life.
工具の選定:
Virgin PEEK is not as abrasive as filled grades, but it is hard. ヒント: We use polished, high-rake carbide tools to slice the material cleanly, preventing the “smearing” effect that ruins surface quality.
Clamping Strategy:
While hard, PEEK is still a plastic. ヒント: We use vacuum tables or soft-jaws with regulated pressure to hold delicate parts securely without leaving clamp marks or distorting the geometry.
医療用インプラント(ISO 13485)
Spinal cages, suture anchors, and dental implants. Virgin PEEK is biocompatible, radiolucent, and has a bone-like modulus.
航空宇宙・航空
Connectors, bushings, and manifolds where weight reduction and high-temperature resistance (up to 250°C) are required.
Analytical Instrumentation
Fluidic manifolds, rotor valves, and HPLC components requiring extreme chemical resistance to solvents and acids.
Semiconductor Equipment
Wafer handling tools and vacuum wand tips that require high purity, low outgassing, and excellent dielectric properties.
| 密度 | 1.30 - 1.32 g/cm³ |
| 引張強度 | 97 - 100 MPa |
| 熱変形温度 | 152 - 160 °C |
| 硬さ | 85 Shore D |
| 破断伸び | 15 - 40% |
| 熱伝導率 | 0.25 W/m-K |
| 連続使用温度 | 250 - 260 °C |
| 吸水率 | 0.10% |
| 絶縁破壊強度 | 19 - 22 kV/mm |
| Bio-compatibility | 優れている |
| 最大部品サイズ | 2000 x 800 x 600 mm |