Ultem 1000 (Polyetherimide) is a high-performance amorphous thermoplastic that blends exceptional thermal, mechanical, and electrical properties. Renowned for its natural amber transparency and inherent flame resistance (UL94 V-0), it is the material of choice for demanding aerospace, medical, and electronic applications. Jucheng Precision specializes in the precision CNC machining of Ultem 1000, utilizing advanced 5-axis milling and stress-relieving annealing processes. Our expertise ensures that complex PEI components, such as medical manifolds and electrical insulators, are produced with tight tolerances and superior surface finishes while remaining free from the stress cracking common in this high-performance polymer.
| グレード | 一般名 | 主な特性 | 代表的な用途 |
|---|---|---|---|
| Ultem 1000 | Standard Unfilled | Amber translucent. Excellent dielectric strength and flame resistance (UL94 V-0). FDA compliant. | Electrical insulators, medical manifolds, microwave parts. |
| Ultem 2300 | 30% Glass Filled | Highest rigidity and dimensional stability. Opaque tan color. Lower thermal expansion. | Structural aerospace parts, high-load connectors. |
| Ultem 2100 | 10% Glass Filled | Balanced strength and finish. Better impact resistance than 2300. | Electronic housings, industrial brackets. |
| Ultem 9085 | Aerospace Grade | High performance with strict Flame, Smoke, and Toxicity (FST) compliance. | Aircraft interior components, ducting. |
| 能力 | 技術的説明 | Juchengの強み |
|---|---|---|
| Optical Clarity Polishing | Post-machining Vapor Polishing or mechanical buffing to restore transparency to machined features. | We achieve high optical clarity for sight glasses and fluid manifolds, allowing for visual inspection of internal flows. |
| Stress-Free Precision Milling | Using specific tool paths and annealing cycles to prevent “crazing” or stress cracking in Ultem. | Ensures long-term dimensional stability and prevents material failure when exposed to cleaning agents or solvents. |
| High-Aspect Ratio Drilling | Drilling high-precision internal channels for medical fluidics without melting or cracking the brittle amber plastic. | Our Peck-drilling cycles and temperature control ensure straight, clean bores with Ra 0.8μm internal finishes. |
| Micro-Threading | Machining fine external and internal threads (down to M1.6) for electronic connectors. | Jucheng achieves sharp, burr-free thread profiles that maintain high dielectric integrity and secure fitment. |
Coolant Sensitivity:
Ultem is highly sensitive to certain oils and solvents, which can cause immediate stress cracking (crazing). ヒント: We use strictly compatible water-soluble coolants or air-blast cooling to ensure material integrity.
Annealing Requirements:
Machining induces internal stress in PEI. ヒント: For parts with tight tolerances or complex geometry, we perform in-process annealing to relieve stress and prevent warping after the final cut.
工具の選定:
Ultem is relatively brittle and abrasive. ヒント: We use sharp, positive-rake carbide tools with polished flutes to shear the material cleanly, preventing heat buildup and surface smearing.
Clamping Care:
Ultem can crack under localized high pressure. ヒント: We utilize vacuum tables or soft-jaws with distributed pressure to hold parts securely without inducing stress risers.
航空宇宙・航空
Electrical connectors, lighting housings, and thermal insulators requiring high flame resistance and low weight.
Medical Devices (ISO 13485)
Surgical instrument handles, sterilization trays, and manifolds requiring repeated autoclaving resistance.
Electronics & Semiconductor
Burn-in sockets, high-voltage switches, and wafer handling components requiring excellent dielectric properties.
Food Processing
Fluid manifolds and scraper blades requiring FDA compliance and resistance to hot water/steam cleaning.
| 密度 | 1.27 g/cm³ |
| 引張強度 | 105 - 110 MPa |
| Elastic Modulus | 3.2 GPa |
| 硬さ | 109 Rockwell R |
| 熱変形温度 | 200 - 210 °C |
| 連続使用温度 | 170 °C |
| 吸水率 | 0.25% |
| 絶縁破壊強度 | 33 kV/mm |
| 光透過率 | Translucent Amber |
| Flammability Rating | UL94 V-0 |