光学グレードPC

Optical Grade PC (Polycarbonate) is engineered for maximum light transmission and minimal haze, making it the premier choice for transparent components. It combines the legendary impact toughness of polycarbonate with the clarity of glass, without the weight or fragility. Jucheng Precision specializes in the ultra-precision machining of optical PC, utilizing high-speed 5-axis milling and specialized vapor polishing to achieve glass-like finishes. Our expertise in producing complex light guides, lenses, and medical sight glasses ensures your optical components deliver perfect light refraction and crystal-clear visibility for critical automotive, medical, and aerospace applications.

Optical PC Machining

ポリカーボネート(PC)材料バリエーション

グレード 一般名 主な特性 代表的な用途
光学グレードPC Lexan® / Makrolon® Highest light transmission and lowest haze. Optimized for optical clarity and vapor polishing. Lenses, light pipes, windows, automotive lighting, protective visors.
機械グレードPC 応力除去PC Annealed to reduce internal stress. Best for machining tight tolerances in complex structural parts. Manifolds, structural housings, semiconductor nests.
ガラス充填PC PC GF10 / GF20 Reinforced with glass fibers for significantly higher stiffness and heat resistance. Non-transparent. Industrial brackets, internal structural frames.

Optical Grade PC Machining Capabilities

能力 技術的説明 Juchengの強み
ベーパーポリッシュ Chemical vapor treatment that melts the surface at a microscopic level to restore 100% transparency. We achieve optical-grade clarity on complex curved lenses and internal ports where manual polishing is impossible.
Micro-Milling Light Guides Milling fine grooves and prisms for light refraction with extremely small step-overs. Our high-speed spindles (up to 30,000 RPM) ensure burr-free edges and sharp prism peaks for maximum light efficiency.
Precision Diamond Turning Utilizing specialized diamond tools to achieve mirror surface finishes directly off the machine. Reduces post-processing time and ensures the highest geometric accuracy for spherical and aspherical lenses.
Anti-Scratch Coating Prep Machining and cleaning surfaces to prepare for secondary hard-coat or anti-reflective (AR) treatments. Jucheng provides a clean-room style finishing environment to ensure optical parts are free from dust and contaminants.

Fabrication Guidelines for Optical Grade PC

Clarity Maintenance:
Tool marks are highly visible in optical parts. ヒント: We use a very small step-over (0.05mm or less) during the finishing pass to minimize tool lines, making the subsequent vapor polishing process more effective.

Scratch Protection:
Optical PC is relatively soft and scratches easily. ヒント: We apply protective adhesive masking immediately after machining and keep the workspace meticulously clean to prevent surface damage.

Coolant Selection:
Non-compatible coolants can turn optical PC cloudy or cause micro-cracking. ヒント: We use only high-purity, plastic-safe water-soluble coolants or chilled air-blast cooling to maintain material transparency.

Annealing for Optics:
Internal stress can distort light paths (birefringence). ヒント: We perform strictly controlled annealing cycles to ensure the light transmission properties are uniform throughout the part.

主な用途

Automotive Lighting
Prototype headlight lenses, interior light guides, and taillight covers requiring optical clarity and high impact resistance.

Medical Diagnostics
Sight glasses, flow cells, and clear reservoirs for blood analyzers where visual monitoring is critical.

航空宇宙・防衛
Cockpit canopies, sensor windows, and camera lenses that must withstand high-speed impacts and thermal cycling.

Industrial Instrumentation
Pressure gauge covers, level indicators, and inspection windows for high-pressure fluid systems.

特性

密度 1.20 g/cm³
引張強度 60 - 70 MPa
光透過率 88 - 90%
Haze Value < 1.0%
硬さ 80 Rockwell M
衝撃強度 650 - 850 J/m
屈折率 1.586
吸水率 0.15%
絶縁破壊強度 15 kV/mm
最大部品サイズ 2000 x 800 x 600 mm