Rame

Copper is the industry standard for thermal and electrical conductivity, making it essential for electronics and automotive (EV) applications. However, pure copper (like C10100/C11000) is soft and "gummy," making it difficult to machine without deformation. Jucheng Precision has mastered copper machining strategies using specialized sharp carbide tooling and optimized coolant systems. We utilize our 25 sets of 5-axis CNC machines to produce intricate heat sinks with high aspect ratios that standard 3-axis machines cannot achieve. As an IATF 16949 certified manufacturer, we also supply high-volume, high-precision copper busbars and connectors for the electric vehicle industry, ensuring 100% electrical performance and surface integrity.

CNC Copper Machining

I nostri materiali disponibili

Rame C10100

The highest purity copper available (99.99%). Oxygen-Free Electronic copper provides the maximum possible electrical and thermal conductivity (101% IACS). It is indispensable for critical applications in the semiconductor, vacuum, and high-end audio industries, where material purity and micro-machining precision are required.

LEGGI DI PIÙ

Rame C11000

The universal standard for electrical applications. Electrolytic Tough Pitch copper offers 100% IACS conductivity and excellent thermal properties. It is the primary choice for manufacturing high-voltage busbars, power distribution terminals, and high-efficiency heat sinks where reliable performance and industrial durability are essential.

LEGGI DI PIÙ

Rame C14500

The "Free-Machining" alternative to pure copper. By adding tellurium, C14500 achieves an 85% machinability rating while retaining 93% conductivity. This allows for high-speed automated production of intricate electrical connectors, gas nozzles, and welding tips with superior surface finishes and tight tolerances.

LEGGI DI PIÙ

Rame C17200

The strongest copper-based alloy, offering steel-like strength and hardness (up to 45 HRC). It provides excellent fatigue resistance, non-magnetic properties, and is non-sparking. It is the premier material for critical aerospace bushings, high-performance spring contacts, and tools used in hazardous explosive environments.

LEGGI DI PIÙ

Available Copper Grades

Grado Nome comune Caratteristiche principali Applicazioni tipiche
C10100 Oxygen-Free Electronic (OFE) 99.99% pure copper. Highest conductivity rating (101% IACS). No embrittlement. High-end audio, vacuum interrupters, particle accelerators, superconductor components.
C11000 Electrolytic Tough Pitch (ETP) 99.9% pure. Standard grade for electrical use. Excellent conductivity (100% IACS). Busbars, wiring, electrical contacts, heat sinks, gaskets.
C14500 Tellurium Copper Free-machining copper. Contains ~0.5% Tellurium. Machinability rating of 85% (vs 20% for pure copper). High-volume machined parts, welding torch tips, electrical connectors.
C17200 Beryllium Copper High strength (comparable to steel) and hardness, non-sparking, non-magnetic. Hazardous dust. Springs, load cells, oil & gas drilling tools, aerospace bushings.

Copper Machining Capabilities

Capacità Descrizione tecnica Vantaggio Jucheng
High-Efficiency Milling Using 5-axis CNC centers to mill complex cooling channels and thin fins on copper heat sinks. We achieve thin-wall features (down to 0.5mm) without bending the soft copper fins.
EDM Electrode Mfg Machining high-precision copper electrodes for Die Sinking EDM applications. Our precision ensures that the electrode shape is perfect, translating to high-quality molds for clients.
Surface Protection Post-machining Electroless Nickel Plating, Silver Plating, or Passivation. Prevents copper oxidation (green patina) and ensures long-term solderability and conductivity.
Precision Turning Turning of electrical contacts, pins, and terminals with smooth surface finishes (Ra 0.4). Ensures maximum contact area for electrical transmission, critical for high-voltage applications.

Fabrication Guidelines for Copper

Selezione degli utensili:
Copper is “sticky.” We use highly polished carbide tools with sharp, positive rake angles. This helps shear the metal cleanly rather than pushing it, preventing Built-Up Edge (BUE) which ruins surface finish.

Serraggio del pezzo:
Because copper is ductile and heavy, it can deform under clamping pressure. We use custom soft jaws or vacuum fixtures to hold parts securely without leaving clamp marks or distorting the geometry.

Feeds & Speeds:
We optimize speeds to avoid excessive heat which can make copper “gummy.” Aggressive feed rates are often used to break chips, which otherwise tend to be long and stringy.

Drilling Deep Holes:
Drilling copper requires “peck drilling” cycles to clear long chips. We use high-pressure coolant to flush chips out, preventing them from jamming and breaking the drill.

Principali settori di applicazione

Automotive & EV (IATF 16949)
Componenti chiave: High-voltage busbars, battery terminals, charging contacts.
Why Copper: Maximizes efficiency in power transmission and battery charging systems.

Electronics & Semiconductors
Componenti chiave: CPU heat sinks, cold plates, liquid cooling blocks.
Why Copper: Superior thermal conductivity pulls heat away from sensitive chips faster than aluminum.

Industrial Manufacturing
Componenti chiave: Welding electrodes, EDM electrodes, power distribution blocks.
Why Copper: High melting point and conductivity make it ideal for transferring energy (welding/sparking).

Aerospaziale
Componenti chiave: Heat exchangers, avionics cooling systems.
Why Copper: Reliability in thermal management for mission-critical flight electronics.

Proprietà dei materiali

Densità 8.90 - 8.96 g/cm³
Resistenza alla trazione 200 - 350 MPa
Carico di snervamento 60 - 300 MPa
Allungamento a rottura 30 - 50 %
Modulo elastico 110 - 120 GPa
Durezza 40 - 90 HRB
Conduttività termica 350 - 390
Conduttività elettrica 85 - 101 % IACS
Punto di fusione 1083 °C
Dimensione massima del pezzo 2000 mm (L) x 800 mm (L) x 600 mm (A)