May 25, 2026
Available LDPE Variants Grade Common Name Key Characteristics Typical Applications Virgin LDPE Natural LDPE Translucent milky-white. FDA compliant. Highest flexibility and impact strength. Gaskets, soft tubing, protective caps. Anti-Static LDPE…
Read More
May 25, 2026
Available HDPE Variants Grade Common Name Key Characteristics Typical Applications Virgin HDPE Natural HDPE Pure white, FDA/USDA compliant. Best for food and medical use. Cutting boards, lab equipment, medical containers.…
Read More
May 25, 2026
Available Polypropylene Types Grade Common Name Key Characteristics Typical Applications PP Homopolymer Rigid PP Higher strength and stiffness. Best for structural chemical tanks and labware. Chemical manifolds, valves, pump parts.…
Read More
January 22, 2026
Available ABS Grades Grade Common Name Key Characteristics Typical Applications Standard ABS General Purpose (GP) Beige or Black color. Excellent impact strength, easy to machine, glue, and paint. Low cost.…
Read More
January 21, 2026
Available Nylon (PA) Grades Grade Common Name Key Characteristics Typical Applications Nylon 6 (PA6) Cast Nylon Excellent toughness, impact resistance, and surface finish. Slightly higher water absorption than PA66. Large…
Read More
January 21, 2026
Available Titanium Grades Grade Common Name Key Characteristics Typical Applications Grade 2 Commercially Pure (CP) Excellent corrosion resistance, good formability, lower strength. Biocompatible. Chemical processing, heat exchangers, medical casing, marine…
Read More
January 15, 2026
Available Aluminum Grades Grade Common Name Key Characteristics Typical Applications Al 6061 Structural Aluminum The most versatile alloy. Good strength, weldability, and high corrosion resistance. Anodizes well. Truck bodies, machine…
Read More