PA66 GF30 stands as the premier choice for engineers seeking the cost-effectiveness of nylon combined with the rigidity of structural composites. By reinforcing Polyamide 6/6 with 30% glass fibers, this material achieves significantly higher tensile strength and a much lower thermal expansion coefficient than unfilled grades. Jucheng Precision specializes in the high-tolerance CNC machining of this abrasive alloy, utilizing specialized diamond-coated tooling and high-torque spindles. Our expertise ensures that your reinforced nylon components—whether for automotive engine zones or heavy-duty industrial pumps—maintain their dimensional integrity and structural performance under the most grueling mechanical loads.
| Марка | Обычное название | Ключевые характеристики | Типичные применения |
|---|---|---|---|
| PA66 GF30 | 30% Glass Filled Nylon | Extreme stiffness and strength. Significantly lower thermal expansion and moisture absorption than virgin nylon. | Pump housings, engine brackets, structural fasteners, power tool components. |
| Nylon 6/6 | Virgin PA66 | High toughness and good wear resistance. More flexible and prone to moisture swell than GF30. | Gears, bushings, electrical insulators. |
| Nylon 6 | Литьевой нейлон | Best for oversized parts. Excellent impact damping but lower mechanical strength than PA66 grades. | Large sheaves, rollers, wear pads. |
| Возможность | Техническое описание | Преимущество Jucheng |
|---|---|---|
| Abrasive-Resistant Milling | Glass fibers are highly abrasive. We utilize diamond-coated or sub-micrograin carbide tools to prevent tool blunting. | Ensures consistent tolerances and sharp features across large production runs, preventing the dimensional drift caused by tool wear. |
| Rigid Structural Machining | Taking advantage of GF30’s high modulus to machine thin-walled housings that maintain their shape. | Our 5-axis machines achieve +/- 0.03mm accuracy on complex brackets, leveraging the material’s superior dimensional stability. |
| Precision Boring & Reaming | Creating tight-tolerance bearing seats and fastener holes in reinforced nylon. | Jucheng uses specialized reaming strategies to prevent glass fiber “tear-out,” ensuring smooth internal diameters and perfect fits. |
| High-Speed Finishing | Optimized tool paths to minimize the “fuzzy” surface finish often associated with glass-filled plastics. | We deliver parts with a clean, professional matte finish that meets aesthetic requirements for industrial equipment. |
Tool Wear Control:
The 30% glass reinforcement acts as an abrasive. Совет: We frequently monitor tool edge integrity and use automated tool-length compensation to ensure every part in a batch remains within specification.
Moisture Absorption:
While GF30 absorbs less moisture than virgin nylon, it is still hygroscopic. Совет: We recommend accounting for a small amount of post-machining expansion (approx. 0.5-1%) depending on the final environment.
Brittle Behavior:
Reinforced nylon is much more brittle than standard PA66. Совет: We avoid sharp internal corners and use generous radii to prevent stress concentrations that could lead to cracking under load.
Fiber Orientation:
The material is stronger in the direction of the extruded fibers. Совет: Jucheng’s engineers analyze part stress requirements to orient the stock material optimally before the first cut.
Automotive Engineering
Engine covers, air intake manifolds, and structural mounting brackets that must withstand heat and vibration.
Power Tools & Industrial Gear
Impact-resistant housings, handles, and internal structural frames for handheld drills and grinders.
Fluid Handling
Pump impellers, valve bodies, and water meter components requiring high stiffness and chemical resistance.
Aerospace Brackets
Lightweight structural supports and cable guides that require a higher strength-to-weight ratio than standard plastics.
| Плотность | 1.35 - 1.41 g/cm³ |
| Предел прочности на растяжение | 150 - 180 MPa |
| Модуль упругости | 9.0 - 11.0 GPa |
| Твёрдость | 120 по шкале Роквелла R |
| Температура тепловой деформации | 240 - 255 °C |
| Температура непрерывной эксплуатации | 110 - 130 °C |
| Водопоглощение | 3.0 - 5.5% |
| Диэлектрическая прочность | 18 - 22 kV/mm |
| Оценка обрабатываемости | Умеренная |
| Макс. размер детали | 2000 x 800 x 600 мм |