Polypropylene (PP) is a lightweight, versatile plastic renowned for its exceptional chemical resistance and unique "living hinge" capability. It is nearly immune to most acids, bases, and organic solvents, making it a staple in the Chemical Processing and Medical sectors. However, PP is notoriously difficult to machine due to its high thermal expansion and tendency to produce burrs. At Jucheng Precision, we have mastered the art of machining PP. Using ultra-sharp tooling and optimized cooling techniques, we produce burr-free PP manifolds, containers, and functional hinges with tight tolerances. Our expertise ensures that your PP parts maintain their lightweight and fatigue-resistant properties while meeting your exact geometric requirements.
| الدرجة | الاسم الشائع | الخصائص الرئيسية | التطبيقات النموذجية |
|---|---|---|---|
| PP Homopolymer | Rigid PP | Higher strength and stiffness. Best for structural chemical tanks and labware. | Chemical manifolds, valves, pump parts. |
| PP Copolymer | Impact PP | Improved impact resistance at low temperatures. More flexible. | Automotive battery cases, protective covers. |
| Glass-Filled PP | PP GF20/30 | Reinforced for much higher rigidity and dimensional stability. | Appliance components, automotive structural parts. |
| القدرة | الوصف الفني | ميزة Jucheng |
|---|---|---|
| Burr-Free Milling | Using specialized high-speed spindles and sharp geometry tools to shear PP cleanly. | Eliminates manual deburring, ensuring smooth internal channels for fluidic manifolds. |
| Living Hinge Fabrication | Precision milling of thin sections (down to 0.3mm) to create durable, integrated hinges. | Ensures thousands of flex cycles without material fatigue or failure. |
| Precision Tank Turning | Turning large-diameter PP cylinders with consistent wall thickness. | Our rigid lathes prevent material “pushing,” achieving perfect roundness for chemical containment. |
التحكم في الحرارة: PP has a low melting point. Standard tools will gum up quickly. نصيحة: We use sharp tools and abundant air-cooling to maintain a cold cutting zone.
استراتيجية التثبيت: PP is soft and easily deformed. We use custom soft jaws and vacuum tables to distribute pressure evenly without marring the waxy surface.
Dimensional Growth: PP has a high thermal expansion coefficient. We machine in temperature-controlled environments to ensure the parts fit correctly at room temperature.
Chemical & Labware: Manifolds, acid-resistant valves, and custom containers for aggressive fluids.
Medical: Orthopedic braces and sterilization-resistant laboratory tools that require low weight.
Consumer Products: Reusable containers and functional prototypes with integrated “living” components.
| الكثافة | 0.90 - 0.92 g/cm³ |
| مقاومة الشد | 30 - 40 MPa |
| معامل المرونة | 1.1 - 1.6 GPa |
| الصلابة | 70 - 100 HRB |
| درجة حرارة الخدمة المستمرة | 100 - 110 °C |
| امتصاص الماء | < 0.01 % |
| نقطة الانصهار | 160 - 170 °C |
| أقصى حجم للقطعة | 2000 x 800 x 600 |