Copper C10100, known as Oxygen-Free Electronic (OFE), is the pinnacle of high-purity copper, refined to 99.99% purity with virtually zero oxygen or volatile impurities. It offers the highest possible electrical and thermal conductivity (minimum 101% IACS), making it indispensable for critical electronic, semiconductor, and vacuum applications. Jucheng Precision specializes in the complex CNC machining of C10100, overcoming its inherent "gummy" nature with specialized sharp diamond tooling and advanced cooling strategies. Whether you require micro-milled heat sinks or high-precision electrical contacts, our ISO 9001 certified facility ensures your OFE copper parts are delivered with mirror finishes and total dimensional integrity.

نحاس C10100

C10100 Machining Capabilities

القدرة الوصف الفني ميزة Jucheng
Micro-Channel Milling C10100 is ideal for thermal management. We utilize 5-axis CNC machines to mill micro-channels (down to 0.3mm width) for liquid cooling plates. Our high-speed spindles ensure burr-free edges and smooth channel walls, maximizing thermal transfer efficiency for semiconductor cooling.
High-Precision Turning Turning small-diameter electrical pins and connectors with tolerances of +/- 0.005mm. We utilize specialized diamond tooling to achieve mirror-like surface finishes (Ra 0.2μm) directly off the machine, critical for electrical contact integrity.
Contamination-Free Machining Processing electronic grade copper in a strictly controlled environment to prevent carbon or ferrous contamination. Jucheng uses dedicated tooling and high-purity synthetic coolants to ensure the 99.99% purity of C10100 is maintained throughout the process.
Secondary Surface Finishing In-house capabilities for Silver Plating, Gold Plating, and Electroless Nickel Plating. Provides a one-stop solution to enhance solderability and prevent oxidation on critical electronic components.

Fabrication Guidelines for C10100 Copper

Handling Material Gummyness:
C10100 is extremely pure and “gummy.” Standard tools will push the metal rather than cut it. نصيحة: We use ultra-sharp carbide tools with high positive rake angles to shear the material cleanly and prevent deformation.

Thermal Conductivity Challenges:
Heat dissipates into the entire part instantly during machining. نصيحة: We utilize high-pressure through-spindle coolant to keep the part temperature stable, ensuring dimensional accuracy across the entire production run.

Zero Built-Up Edge (BUE):
Pure copper tends to weld itself to the tool edge. نصيحة: Highly polished tool flutes and specialized lubrication are mandatory to prevent BUE, which ruins surface finish and tolerance.

حساسية تثبيت قطعة العمل:
Being soft, C10100 can be easily marked by vice jaws. نصيحة: We use custom-machined soft jaws or vacuum fixtures to hold thin copper plates without leaving surface indentations.

التطبيقات الأساسية

High-End Audio Components
Vacuum tube bases, high-purity terminals, and audio cable connectors where 101% IACS conductivity is essential for signal purity.

Semiconductor & Electronics
Wafer handling tools, micro-channel cold plates, and CPU heat sinks for high-performance computing.

Medical & Laboratory
Components for MRI machines and particle accelerators requiring non-magnetic properties and absolute material purity.

Aerospace Avionics
Heat exchangers and power distribution blocks for satellite and flight control systems operating in extreme environments.

الخصائص

الكثافة 8.94 g/cm³
مقاومة الشد 220 - 340 MPa
مقاومة الخضوع 69 - 280 MPa
الصلابة 40 - 85 HB (Brinell)
الاستطالة عند الكسر 35 - 55%
التوصيل الحراري 391 W/m-K
التوصيل الكهربائي 101% IACS
نقطة الانصهار 1083 °C
تقييم قابلية التشغيل 20%
Purity Level 99.99% Cu
أقصى حجم للقطعة 2000 × 800 × 600 مم