Delrin AF is a unique thermoplastic blend of Acetal Homopolymer and high-strength PTFE (Teflon) fibers. It represents the ultimate solution for engineers seeking the stiffness and strength of Delrin combined with the world-class low friction of PTFE. This self-lubricating material eliminates the need for external grease, preventing the "stick-slip" effect and reducing mechanical wear. At Jucheng Precision, we specialize in the high-precision CNC machining of Delrin AF into bushings, thrust washers, and silent-running gears. Our expertise in processing this "super-slippery" polymer ensures that your precision components are delivered with exceptional surface quality and the dimensional integrity required for maintenance-free mechanical assemblies.
| Марка | Обычное название | Ключевые характеристики | Типичные применения |
|---|---|---|---|
| Delrin AF | PTFE-Filled POM | Lowest coefficient of friction. Blended with 13% or 20% Teflon fibers. Extreme wear resistance. | High-speed bearings, thrust washers, moving slide components, silent gears. |
| Delrin 150 | POM-H (Homopolymer) | Highest mechanical strength and stiffness. Best for precision gears. | Structural mechanical parts, precision gears, high-load clips. |
| ПОМ-C | Acetal Copolymer | Zero centerline porosity and superior chemical resistance to hot water and bases. | Fluid manifolds, food processing parts, medical handles. |
| Возможность | Техническое описание | Преимущество Jucheng |
|---|---|---|
| Ultra-Smooth Bore Turning | Machining internal bearing diameters to Ra 0.4μm to maximize the self-lubricating effect of the PTFE fibers. | We utilize specialized diamond-polished inserts to ensure the Teflon fibers are sheared cleanly, creating a slippery, low-friction interface. |
| Precision Thrust Washer Milling | Milling thin, flat washers with strict parallelism (+/- 0.02mm) to prevent uneven wear in rotating assemblies. | Our vacuum workholding systems ensure that thin Delrin AF plates remain perfectly flat during high-speed milling operations. |
| Complex Low-Friction Cams | Using 4-axis CNC milling to create intricate cam profiles that operate without external grease. | Jucheng’s precision ensures smooth profile transitions, reducing mechanical noise and stick-slip vibration in automated machinery. |
| High-Volume Bushing Production | Rapid production of self-lubricating bushings using automated bar-fed Swiss lathes. | Offers high-speed output with extremely consistent dimensions, making Delrin AF a cost-effective alternative to lubricated bronze. |
Distinctive Appearance:
Delrin AF is typically dark brown or chocolate in color due to the PTFE fibers. Совет: This makes it easily distinguishable from standard white or black POM during assembly and inspection.
Cutting Temperature:
While the PTFE fibers provide lubrication, heat buildup can still cause material softening. Совет: We use sharp tools and high-volume air blast or water-soluble coolant to keep the material rigid for accurate cutting.
Avoid Bonding:
Due to the high Teflon content, Delrin AF is almost impossible to glue or bond. Совет: Design your assembly using mechanical fasteners or interference (press) fits.
Environmental Stability:
Like all acetals, Delrin AF has very low moisture absorption. Совет: It maintains its precise dimensions even in submerged or high-humidity environments, unlike Nylon.
High-Speed Sliding Bearings
Bushings and sleeves in office equipment and conveyors that must operate silently without liquid lubricants.
Medical & Laboratory Equipment
Moving parts in diagnostic machines where grease contamination would ruin sensitive samples or sensors.
Потребительская электроника
Internal sliding mechanisms for cameras, lens actuators, and high-end audio-visual equipment.
Industrial Automation
Guide rails, wear strips, and cam followers that require long-term durability and a low “breakaway” force.
| Плотность | 1.54 g/cm³ |
| Предел прочности на растяжение | 50 - 55 MPa |
| Модуль упругости | 2.8 - 3.0 GPa |
| Твёрдость | 115 Rockwell R |
| Коэффициент трения | 0.15 (Dynamic) |
| Скорость износа | Outstanding |
| Температура непрерывной эксплуатации | 90 - 100 °C |
| Водопоглощение | 0.20% |
| Color | Dark Brown / Chocolate |
| Оценка обрабатываемости | Excellent |
| Макс. размер детали | 2000 x 800 x 600 мм |