PC GF30 is a 30% glass fiber reinforced polycarbonate that offers a significant leap in mechanical performance compared to standard unfilled grades. By incorporating glass fibers, this material achieves exceptional rigidity, high tensile strength, and a drastically reduced thermal expansion coefficient. It maintains the inherent impact resistance and flame retardancy of polycarbonate while providing the structural integrity required for heavy-duty industrial housings. At Jucheng Precision, we specialize in the high-tolerance CNC machining of this abrasive reinforced polymer. Utilizing advanced diamond-coated tooling and rigid machine setups, we deliver precision-engineered PC GF30 components that excel in demanding structural applications within the automotive, electrical, and industrial sectors.
| Grade | Common Name | Key Characteristics | Typical Applications |
|---|---|---|---|
| PC GF30 | 30% Glass Filled PC | Highest rigidity and dimensional stability. Exceptional heat resistance and tensile strength. Opaque. | Industrial brackets, structural housings, electrical equipment frames. |
| Machine Grade PC | Stress-Relieved PC | Unfilled and transparent. Specially annealed to remove internal stress for precision machining. | Manifolds, sight glasses, semiconductor components. |
| Optical Grade PC | Lexan® / Makrolon® | Highest light transmission and clarity. Optimized for vapor polishing to achieve mirror finishes. | Lenses, light pipes, windows, automotive lighting. |
| Возможность | Техническое описание | Преимущество Jucheng |
|---|---|---|
| Abrasive-Resistant Milling | The 30% glass fiber content is highly abrasive. We utilize diamond-coated (CVD) or sub-micrograin carbide cutters. | Ensures consistent dimensions and sharp edges over long production runs by preventing tool blunting. |
| Rigid Structural Machining | Leveraging PC GF30’s high modulus to machine thin-walled structural housings that maintain their shape. | Our 5-axis machines achieve tight tolerances (+/- 0.02mm), preventing the part flexing common in unfilled plastics. |
| Precision Boring & Reaming | Creating accurate bearing seats and fastener holes in reinforced polycarbonate. | Specialized reaming strategies prevent glass fiber “tear-out,” ensuring perfectly smooth internal diameters and secure fits. |
| High-Speed Finishing | Optimized tool paths to achieve a clean matte finish without the “fuzzy” surface common with filled plastics. | Delivers professional, industrial-grade aesthetics directly off the machine for visible structural components. |
Abrasiveness Management:
PC GF30 wears down standard tools rapidly. Совет: We frequently monitor tool life and use automated compensation to ensure “size drift” does not occur during large batch production.
Non-Transparent Nature:
Adding glass fiber makes the PC opaque (usually grey or black). Совет: This grade cannot be polished to transparency. Design for mechanical performance rather than optical clarity.
Brittle Behavior:
Reinforced PC is more brittle than standard polycarbonate. Совет: We avoid sharp internal corners and use generous radii to prevent stress concentrations that could lead to cracking under structural load.
Chemical Sensitivity:
Like all polycarbonates, GF30 is sensitive to certain oils and solvents. Совет: We use strictly compatible, water-soluble coolants to prevent chemical stress cracking (crazing).
Industrial Equipment
Heavy-duty structural brackets, mounting plates, and pump components requiring high rigidity and dimensional stability.
Electrical & Electronics
High-load connector housings, circuit breaker components, and standoff insulators that must resist heat and impact.
Automotive Engineering
Under-the-hood struct
| Плотность | 1.42 - 1.45 g/cm³ |
| Предел прочности на растяжение | 100 - 120 MPa |
| Elastic Modulus | 5.5 - 6.5 GPa |
| Твёрдость | 90 Rockwell M |
| Heat Deflection Temp | 145 - 150 °C |
| Continuous Service Temp | 120 °C |
| Water Absorption | 0.10% |
| Dielectric Strength | 18 kV/mm |
| Flammability Rating | UL94 V-0 |
| Макс. размер детали | 2000 x 800 x 600 мм |