{"id":809,"date":"2026-03-12T11:25:36","date_gmt":"2026-03-12T03:25:36","guid":{"rendered":"https:\/\/www.jccncmachining.com\/?post_type=material_model&#038;p=809"},"modified":"2026-11-05T13:42:05","modified_gmt":"2026-11-05T05:42:05","slug":"delrin-150","status":"publish","type":"material_model","link":"https:\/\/www.jccncmachining.com\/pt\/materiais\/pom-delrin-acetal\/delrin-150\/","title":{"rendered":"Delrin 150"},"content":{"rendered":"<p><!-- Section: Available POM Variants --><\/p>\n<div class=\"available-material-types\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Variantes do Material POM \/ Acetal<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left;\">Grau<\/th>\n<th style=\"text-align: left;\">Nome Comum<\/th>\n<th style=\"text-align: left;\">Caracter\u00edsticas Principais<\/th>\n<th style=\"text-align: left;\">Aplica\u00e7\u00f5es T\u00edpicas<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Delrin 150<\/strong><\/td>\n<td>POM-H (Homopol\u00edmero)<\/td>\n<td>Maior resist\u00eancia \u00e0 tra\u00e7\u00e3o, rigidez e dureza do que o copol\u00edmero. Resist\u00eancia \u00e0 fadiga superior.<\/td>\n<td>Engrenagens de precis\u00e3o, buchas de alta carga, cintos de seguran\u00e7a, articula\u00e7\u00f5es mec\u00e2nicas.<\/td>\n<\/tr>\n<tr>\n<td><strong>POM-C<\/strong><\/td>\n<td>Copol\u00edmero de Acetal<\/td>\n<td>Melhor resist\u00eancia qu\u00edmica e livre de porosidade na linha central. Melhor desempenho em \u00e1gua quente.<\/td>\n<td>Conex\u00f5es hidr\u00e1ulicas, pe\u00e7as para processamento de alimentos, cabos de instrumentos m\u00e9dicos.<\/td>\n<\/tr>\n<tr>\n<td><strong>Delrin AF<\/strong><\/td>\n<td>POM com PTFE<\/td>\n<td>Misturado com fibras de Teflon para o menor coeficiente de atrito poss\u00edvel e vida \u00fatil superior contra desgaste.<\/td>\n<td>Rolamentos deslizantes de alta velocidade, arruelas de encosto, componentes de transportadores.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Machining Capabilities for Delrin 150 --><\/p>\n<div class=\"machining-capabilities\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Capacidades de Usinagem do Delrin 150<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 25%;\">Capacidade<\/th>\n<th style=\"text-align: left; width: 45%;\">Descri\u00e7\u00e3o T\u00e9cnica<\/th>\n<th style=\"text-align: left; width: 30%;\">Vantagem Jucheng<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Fresamento de Engrenagens de Alta Velocidade<\/strong><\/td>\n<td>Fresamento de engrenagens retas, helicoidais e sem-fim de precis\u00e3o diretamente de barras ou chapas de Delrin 150.<\/td>\n<td>Alcan\u00e7amos qualidade de engrenagem AGMA 10+ com acabamento superficial de dentes excepcional, garantindo opera\u00e7\u00e3o silenciosa e longa vida \u00fatil contra desgaste.<\/td>\n<\/tr>\n<tr>\n<td><strong><a href=\"https:\/\/www.jccncmachining.com\/pt\/blog\/pequenas-pecas-grande-estabilidade-por-que-o-cnc-suico-funciona\/\">Torneamento Su\u00ed\u00e7o Automatizado<\/a><\/strong><\/td>\n<td>Utilizando tornos su\u00ed\u00e7os com alimenta\u00e7\u00e3o por barra para produzir pinos, espa\u00e7adores e buchas de pequeno di\u00e2metro com tempos de ciclo r\u00e1pidos.<\/td>\n<td>Nossas linhas de produ\u00e7\u00e3o automatizadas 24\/7 oferecem o pre\u00e7o unit\u00e1rio mais competitivo para ferragens de Delrin em alto volume (10.000+ pe\u00e7as).<\/td>\n<\/tr>\n<tr>\n<td><strong>Usinagem de Encaixe por Press\u00e3o e Clipes<\/strong><\/td>\n<td>Aproveitando a alta elasticidade do Delrin para usinar recursos funcionais de encaixe por press\u00e3o e molas integrais.<\/td>\n<td>A fresagem de precis\u00e3o da Jucheng garante que os clipes tenham o \u201cclique\u201d perfeito e for\u00e7a de reten\u00e7\u00e3o sem fadiga do material.<\/td>\n<\/tr>\n<tr>\n<td><strong>Mandrilamento de Toler\u00e2ncia Estreita<\/strong><\/td>\n<td>Mandrilamento de di\u00e2metros internos com toler\u00e2ncias de +\/- 0,02 mm para rolamentos e conjuntos de encaixe por press\u00e3o.<\/td>\n<td>Nosso ambiente de usinagem com temperatura controlada evita os problemas de expans\u00e3o t\u00e9rmica comuns ao usinar pl\u00e1sticos.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Fabrication Guidelines --><\/p>\n<div class=\"fabrication-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Diretrizes de Fabrica\u00e7\u00e3o para Delrin 150<\/h3>\n<p><strong>Consci\u00eancia da Porosidade na Linha Central:<\/strong><br \/>\nComo homopol\u00edmero, o Delrin 150 pode apresentar pequenos vazios no centro de hastes ou placas espessas. <strong>Dica:<\/strong> For parts requiring gas-tight sealing or aesthetic perfection in the center, we recommend using <a href=\"https:\/\/www.jccncmachining.com\/pt\/materiais\/pom-delrin-acetal\/pom-c\/\">POM-C<\/a> or designing features away from the centerline.<\/p>\n<p><strong>Excel\u00eancia em Usinabilidade:<\/strong><br \/>\nO Delrin \u00e9 amplamente considerado o pl\u00e1stico \u201cmais f\u00e1cil\u201d de usinar. <strong>Dica:<\/strong> Ele produz cavacos pequenos e limpos e n\u00e3o requer rebarba\u00e7\u00e3o complexa. Usamos ferramentas de a\u00e7o r\u00e1pido ou metal duro n\u00e3o revestido com arestas afiadas para obter os melhores resultados.<\/p>\n<p><strong>Umidade e Estabilidade:<\/strong><br \/>\nO Delrin tem absor\u00e7\u00e3o de umidade muito baixa. <strong>Dica:<\/strong> \u00c9 significativamente mais est\u00e1vel dimensionalmente que o Nylon, tornando-o a escolha preferida para pe\u00e7as expostas a ambientes \u00famidos.<\/p>\n<p><strong>Expans\u00e3o T\u00e9rmica:<\/strong><br \/>\nComo todos os pl\u00e1sticos, o Delrin expande mais do que o metal. <strong>Dica:<\/strong> Utilizamos estrat\u00e9gias de \u201ccorte a frio\u201d e ferramentas afiadas para minimizar a transfer\u00eancia de calor para a pe\u00e7a durante passes de fresagem em alta velocidade.<\/p>\n<\/div>\n<p><!-- Section: Application Scenarios --><\/p>\n<div class=\"application-scenarios\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Aplica\u00e7\u00f5es Principais<\/h3>\n<p><strong>Controle de Movimento de Precis\u00e3o<\/strong><br \/>\nEngrenagens, cames e catracas para impressoras, scanners e equipamentos de dispensa\u00e7\u00e3o automatizados onde \u00e9 necess\u00e1rio baixo atrito.<\/p>\n<p><strong>Interior e Sistemas Automotivos<\/strong><br \/>\nComponentes de cinto de seguran\u00e7a, mecanismos de eleva\u00e7\u00e3o de vidros e pe\u00e7as de sistemas de combust\u00edvel devido \u00e0 excelente resist\u00eancia \u00e0 fadiga e a solventes.<\/p>\n<p><strong>Eletr\u00f4nicos de Consumo<\/strong><br \/>\nInterruptores mec\u00e2nicos, bot\u00f5es e componentes de chassi deslizantes que exigem uma sensa\u00e7\u00e3o t\u00e1til premium e durabilidade.<\/p>\n<p><strong>Fixadores Industriais<\/strong><br \/>\nParafusos, rebites e espa\u00e7adores especializados que devem fornecer isolamento el\u00e9trico enquanto mant\u00eam a rigidez estrutural.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>POM \/ Acetal Material Variants Grade Common Name Key Characteristics Typical Applications Delrin 150 POM-H (Homopolymer) Higher tensile strength, stiffness, and hardness than copolymer. Superior fatigue resistance. Precision gears, high-load bushings, safety restraints, mechanical linkages. POM-C Acetal Copolymer Better chemical resistance and free of centerline porosity. Better performance in hot water. Plumbing fittings, food processing [&hellip;]<\/p>\n","protected":false},"featured_media":810,"template":"","meta":[],"class_list":["post-809","material_model","type-material_model","status-publish","has-post-thumbnail","hentry"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/material_model\/809","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/material_model"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/types\/material_model"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/media\/810"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/media?parent=809"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}