{"id":534,"date":"2026-02-24T08:36:29","date_gmt":"2026-02-24T08:36:29","guid":{"rendered":"https:\/\/www.jccncmachining.com\/material\/\/"},"modified":"2026-02-24T08:36:29","modified_gmt":"2026-02-24T08:36:29","slug":"stainless-steel-440c","status":"publish","type":"material_model","link":"https:\/\/www.jccncmachining.com\/pt\/materials\/stainless-steel\/stainless-steel-440c\/","title":{"rendered":"Stainless Steel 440C"},"content":{"rendered":"<p><!-- Section: Machining Capabilities for SS 440C --><\/p>\n<div class=\"machining-capabilities\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">SS 440C Machining Capabilities<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 25%;\">Capability<\/th>\n<th style=\"text-align: left; width: 45%;\">Technical Description<\/th>\n<th style=\"text-align: left; width: 30%;\">Jucheng Advantage<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Hard Turning<\/strong><\/td>\n<td>Turning 440C in its fully hardened state (58-60 HRC) using PCBN (Polycrystalline Cubic Boron Nitride) inserts.<\/td>\n<td>Eliminates the need for grinding on some geometries, reducing cost while maintaining tight tolerances (+\/- 0.005mm).<\/td>\n<\/tr>\n<tr>\n<td><strong>Bearing-Grade Grinding<\/strong><\/td>\n<td>Precision ID\/OD grinding to achieve roundness and concentricity within 1 micron.<\/td>\n<td>We produce custom bearing races and rollers that meet ABEC dimensional standards.<\/td>\n<\/tr>\n<tr>\n<td><strong>Cryogenic Treatment<\/strong><\/td>\n<td>Deep freezing parts after heat treatment to convert retained austenite to martensite.<\/td>\n<td>Ensures maximum dimensional stability and hardness for parts used in precision metrology or aerospace.<\/td>\n<\/tr>\n<tr>\n<td><strong>Superfinishing<\/strong><\/td>\n<td>Polishing ground surfaces to Ra 0.05\u00b5m to reduce friction and wear.<\/td>\n<td>Essential for high-speed shafts and valve seats to prevent seizing and extend service life.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Fabrication Guidelines --><\/p>\n<div class=\"fabrication-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Fabrication Guidelines for Stainless 440C<\/h3>\n<p><strong>Annealed vs. Hardened:<\/strong><br \/>\nWe machine the general shape in the annealed condition (easy to cut) and finish-grind after heat treatment. <strong>Tip:<\/strong> Always leave 0.3mm &#8211; 0.5mm grinding stock to remove heat-treat distortion.<\/p>\n<p><strong>Corrosion Resistance:<\/strong><br \/>\n440C has better corrosion resistance than tool steels (like D2) but worse than 304. <strong>Tip:<\/strong> Ideally suited for applications involving mild moisture or lubricants, but not saltwater immersion.<\/p>\n<p><strong>Brittleness:<\/strong><br \/>\nAt 60 HRC, 440C is very hard but brittle. <strong>Tip:<\/strong> Avoid thin, unsupported walls or sharp internal corners which can crack during quenching.<\/p>\n<\/div>\n<p><!-- Section: Application Scenarios --><\/p>\n<div class=\"application-scenarios\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Primary Applications<\/h3>\n<p><strong>Rolling Element Bearings<\/strong><br \/>\nBalls, rollers, and races. 440C is the standard for corrosion-resistant bearings.<\/p>\n<p><strong>Valve Components<\/strong><br \/>\nHigh-pressure valve seats and needle tips that must seal perfectly and resist erosion from fluid flow.<\/p>\n<p><strong>Mold Inserts<\/strong><br \/>\nSmall, high-wear cores in plastic injection molds, especially for abrasive glass-filled plastics.<\/p>\n<p><strong>High-End Cutlery<\/strong><br \/>\nPremium knife blades and surgical shears requiring the ultimate razor edge retention.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>SS 440C Machining Capabilities Capability Technical Description Jucheng Advantage Hard Turning Turning 440C in its fully hardened state (58-60 HRC) using PCBN (Polycrystalline Cubic Boron Nitride) inserts. Eliminates the need for grinding on some geometries, reducing cost while maintaining tight tolerances (+\/- 0.005mm). Bearing-Grade Grinding Precision ID\/OD grinding to achieve roundness and concentricity within 1 [&hellip;]<\/p>\n","protected":false},"featured_media":535,"template":"","meta":[],"class_list":["post-534","material_model","type-material_model","status-publish","has-post-thumbnail","hentry"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/material_model\/534","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/material_model"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/types\/material_model"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/media\/535"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/media?parent=534"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}