{"id":528,"date":"2026-02-24T08:08:11","date_gmt":"2026-02-24T08:08:11","guid":{"rendered":"https:\/\/www.jccncmachining.com\/material\/\/"},"modified":"2026-02-24T08:08:11","modified_gmt":"2026-02-24T08:08:11","slug":"stainless-steel-17-4-ph","status":"publish","type":"material_model","link":"https:\/\/www.jccncmachining.com\/pt\/materials\/stainless-steel\/stainless-steel-17-4-ph\/","title":{"rendered":"Stainless Steel 17-4 PH"},"content":{"rendered":"<p><!-- Section: Machining Capabilities for 17-4 PH --><\/p>\n<div class=\"machining-capabilities\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">17-4 PH Machining Capabilities<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 25%;\">Capability<\/th>\n<th style=\"text-align: left; width: 45%;\">Technical Description<\/th>\n<th style=\"text-align: left; width: 30%;\">Jucheng Advantage<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Hard Machining<\/strong><\/td>\n<td>Machining 17-4 PH after heat treatment (Condition H900, ~44 HRC). Requires rigid machines and specialized carbide.<\/td>\n<td>We eliminate post-heat treat distortion issues by machining the part directly in its hardened state for maximum accuracy.<\/td>\n<\/tr>\n<tr>\n<td><strong>Heat Treatment Management<\/strong><\/td>\n<td>Processing parts from Condition A (Annealed) to various aged conditions (H900, H1025, H1150) to tune strength\/ductility.<\/td>\n<td>We provide turnkey manufacturing, handling the aging process and certifying the final hardness and tensile strength.<\/td>\n<\/tr>\n<tr>\n<td><strong>Precision Grinding<\/strong><\/td>\n<td>Post-machining cylindrical or surface grinding to achieve bearing-grade tolerances (+\/- 0.002mm).<\/td>\n<td>Essential for aerospace actuator shafts and pump components where seal fits are critical.<\/td>\n<\/tr>\n<tr>\n<td><strong>Complex 5-Axis Milling<\/strong><\/td>\n<td>Milling structural brackets and fittings from solid 17-4 blocks.<\/td>\n<td>Our powerful spindles easily handle the high cutting forces required for this tough aerospace alloy.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Fabrication Guidelines --><\/p>\n<div class=\"fabrication-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Fabrication Guidelines for 17-4 PH<\/h3>\n<p><strong>Machinability:<\/strong><br \/>\nIn the annealed state (Condition A), 17-4 PH machines similarly to Stainless 304 but is slightly harder. <strong>Tip:<\/strong> Tool life is shorter than 304; use premium coated carbide tools.<\/p>\n<p><strong>Dimensional Change:<\/strong><br \/>\nOne of 17-4&#8217;s best features is its low distortion during heat treatment. Unlike carbon steels, it shrinks very predictably (approx. 0.0005 in\/in). <strong>Tip:<\/strong> We can often machine to final size before heat treat for H1150 condition.<\/p>\n<p><strong>Magnetic Property:<\/strong><br \/>\nUnlike 304\/316, <strong>17-4 PH is magnetic<\/strong>. <strong>Tip:<\/strong> This allows us to use magnetic workholding for surface grinding, reducing tooling costs.<\/p>\n<\/div>\n<p><!-- Section: Application Scenarios --><\/p>\n<div class=\"application-scenarios\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Primary Applications<\/h3>\n<p><strong>Aerospace &amp; Defense<\/strong><br \/>\nActuators, landing gear components, and structural fasteners requiring high strength up to 315\u00b0C (600\u00b0F).<\/p>\n<p><strong>Oil &amp; Gas<\/strong><br \/>\nValve stems, pump shafts, and downhole tool components that need high hardness to resist wear and slurry erosion.<\/p>\n<p><strong>Power Generation<\/strong><br \/>\nTurbine blades and nuclear reactor components due to excellent corrosion resistance and mechanical properties.<\/p>\n<p><strong>Medical Instruments<\/strong><br \/>\nSurgical tools requiring a sharp cutting edge (hardness) combined with rust resistance (sterilization).<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>17-4 PH Machining Capabilities Capability Technical Description Jucheng Advantage Hard Machining Machining 17-4 PH after heat treatment (Condition H900, ~44 HRC). Requires rigid machines and specialized carbide. We eliminate post-heat treat distortion issues by machining the part directly in its hardened state for maximum accuracy. Heat Treatment Management Processing parts from Condition A (Annealed) to [&hellip;]<\/p>\n","protected":false},"featured_media":529,"template":"","meta":[],"class_list":["post-528","material_model","type-material_model","status-publish","has-post-thumbnail","hentry"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/material_model\/528","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/material_model"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/types\/material_model"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/media\/529"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/pt\/wp-json\/wp\/v2\/media?parent=528"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}