{"id":3808,"date":"2026-11-11T18:02:34","date_gmt":"2026-11-11T10:02:34","guid":{"rendered":"https:\/\/www.jccncmachining.com\/?p=3808"},"modified":"2026-11-11T14:11:27","modified_gmt":"2026-11-11T06:11:27","slug":"%ec%83%a4%ed%94%84%ed%8a%b8-%ed%82%a4%ed%99%88-%ec%b9%98%ec%88%98","status":"publish","type":"post","link":"https:\/\/www.jccncmachining.com\/ko\/%eb%b8%94%eb%a1%9c%ea%b7%b8\/%ec%83%a4%ed%94%84%ed%8a%b8-%ed%82%a4%ed%99%88-%ec%b9%98%ec%88%98\/","title":{"rendered":"\ub9de\ucda4 \ubb38\uc81c\ub97c \ubc29\uc9c0\ud558\ub294 \uc0e4\ud504\ud2b8 \ud0a4\ud648 \uce58\uc218"},"content":{"rendered":"<p>\uc0e4\ud504\ud2b8 \ud0a4\ud648 \ub3c4\uba74\uc740 \uc2ac\ub86f \ud3ed \uc774\uc0c1\uc744 \uad00\ub9ac\ud574\uc57c \ud569\ub2c8\ub2e4. \ud0a4\uac00 \uc758\ub3c4\ud55c \ub300\ub85c \uc548\ucc29\ud558\uace0 \ud1a0\ud06c\ub97c \uc804\ub2ec\ud558\ub3c4\ub85d \uc0dd\uc0b0\ud558\ub824\uba74, \uc0ac\uc591\uc11c\uc5d0 \uc801\uc6a9 \uac00\ub2a5\ud55c \ud0a4\/\ud0a4\uc2dc\ud2b8 \ud45c\uc900 \ub610\ub294 \ub9de\ucda4 \ud615\uc0c1, \ud0a4\ud648 \ud3ed\uacfc \uae4a\uc774, \uac01\ub3c4 \ubc0f \ucd95 \ubc29\ud5a5 \uc704\uce58, \ub07c\uc6cc\ub9de\ucda4 \uad00\uacc4, \uadf8\ub9ac\uace0 \uac80\uc0ac\uc5d0 \uc0ac\uc6a9\ub418\ub294 \ub370\uc774\ud140\uc744 \uba85\uc2dc\ud574\uc57c \ud569\ub2c8\ub2e4. \uc0e4\ud504\ud2b8 \uc9c1\uacbd\ub9cc\uc73c\ub85c\ub294 \ubaa8\ub4e0 \ud0a4\uc2dc\ud2b8 \uc694\uad6c\uc0ac\ud56d\uc774 \uc815\uc758\ub418\uc9c0 \uc54a\uc73c\uba70, \ud45c\uc900 \ud45c\ub97c \uc870\ub9bd\uccb4\uc758 \uc2e4\uc81c \uc124\uacc4 \uc758\ub3c4\ub97c \ub300\uccb4\ud558\ub294 \uac83\uc73c\ub85c \ucde8\uae09\ud574\uc11c\ub294 \uc548 \ub429\ub2c8\ub2e4. \uba3c\uc800 \uacb0\ud569 \ud5c8\ube0c\uc640 \ud0a4\uc5d0\uc11c \uc2dc\uc791\ud55c \ub2e4\uc74c, \uc5b4\ub5a4 \uce58\uc218\uac00 \uc120\ud0dd\ub41c \ud45c\uc900\uc5d0\uc11c \ub098\uc628 \uac83\uc774\uace0 \uc5b4\ub5a4 \uac83\uc774 \ud504\ub85c\uc81d\ud2b8 \uace0\uc720\uc758 \uac83\uc778\uc9c0 \uba85\uc2dc\ud558\uc2ed\uc2dc\uc624. \ub9c8\uc9c0\ub9c9\uc73c\ub85c, \uacf5\uae09\uc5c5\uccb4\uac00 \uc0e4\ud504\ud2b8 \ud45c\uba74\uc73c\ub85c\ubd80\ud130\uc758 \uae4a\uc774\uc640 \uc2dc\ud2b8 \ubc18\ub300\ud3b8\uc73c\ub85c\ubd80\ud130\uc758 \uae4a\uc774\ub97c \ud63c\ub3d9\ud558\uc9c0 \uc54a\uace0 \uc2ac\ub86f\uc744 \uac80\uc99d\ud560 \uc218 \uc788\ub3c4\ub85d \uac80\uc0ac \ubc29\ubc95\uc744 \uc815\uc758\ud558\uc2ed\uc2dc\uc624.<\/p>\n<nav class=\"article-toc\" aria-label=\"\ubaa9\ucc28\"><strong>\uc774 \ud398\uc774\uc9c0\uc5d0\uc11c<\/strong><\/p>\n<ul>\n<li><a href=\"#section-1\">\ud0a4\uc640 \uc801\uc6a9 \ud45c\uc900 \uc120\ud0dd<\/a><\/li>\n<li><a href=\"#section-2\">\ud3ed, \uae4a\uc774 \ubc0f \ub07c\uc6cc\ub9de\ucda4 \uc758\ub3c4 \uba85\uc2dc<\/a><\/li>\n<li><a href=\"#section-3\">\uae30\ub2a5 \ub370\uc774\ud140\uc5d0\uc11c \uc2ac\ub86f \uc704\uce58 \uc9c0\uc815<\/a><\/li>\n<li><a href=\"#section-4\">\uac00\uacf5\uacfc \uac80\uc0ac\ub97c \ud568\uaed8 \uacc4\ud68d\ud558\uc2ed\uc2dc\uc624<\/a><\/li>\n<li><a href=\"#section-5\">\uac80\uc0ac \uac00\ub2a5\ud55c \ud0a4\ud648 \uc815\uc758 \ub9b4\ub9ac\uc2a4<\/a><\/li>\n<\/ul>\n<\/nav>\n<h2 id=\"section-1\">\ud0a4\uc640 \uc801\uc6a9 \ud45c\uc900 \uc120\ud0dd<\/h2>\n<p>\uc124\uacc4\uac00 \ud3c9\ud589 \ud0a4, \ud14c\uc774\ud37c \ud0a4 \ub610\ub294 \ud2b9\uc218 \ubc30\uc5f4\uc744 \uc0ac\uc6a9\ud558\ub294\uc9c0 \ud655\uc778\ud558\uc2ed\uc2dc\uc624. \uc801\uc6a9 \ud45c\uc900\uc740 \uadf8 \ubc94\uc704 \ub0b4\uc5d0\uc11c \uc0e4\ud504\ud2b8 \uc9c1\uacbd, \ud0a4 \ud06c\uae30 \ubc0f \ud0a4\uc2dc\ud2b8 \ud615\uc0c1 \uac04\uc758 \uad00\uacc4\ub97c \uc815\ub9bd\ud569\ub2c8\ub2e4. \uc608\ub97c \ub4e4\uc5b4 ASME B17.1\uc740 \ud3c9\ud589 \ud0a4\uc640 \ud14c\uc774\ud37c \ud0a4 \ubc0f \ud0a4\uc2dc\ud2b8\uc758 \ud06c\uae30\uc640 \uacf5\ucc28\ub97c \ub2e4\ub8e8\uba70, \uadf8 \ud45c\uc900 \uce58\uc218\ub294 \ub2e8\uc77c \ud0a4 \uc801\uc6a9\uc744 \uc704\ud55c \uac83\uc784\uc744 \uba85\uc2dc\ud558\uace0 \uc788\uc2b5\ub2c8\ub2e4. \ud45c\ub97c \uc0ac\uc6a9\ud558\uae30 \uc804\uc5d0 \ud604\uc7ac \uacc4\uc57d \uc5d0\ub514\uc158\uacfc \uc124\uacc4\uc758 \ud0a4 \uac1c\uc218\ub97c \ud655\uc778\ud558\uc2ed\uc2dc\uc624.<\/p>\n<p>\ud45c\uc900 \uc120\ud0dd\uc774 \ubaa8\ub4e0 \uc870\ub9bd\uccb4\uc758 \ud1a0\ud06c \uc6a9\ub7c9, \ud5c8\ube0c \uae38\uc774, \uc7ac\ub8cc \uac15\ub3c4, \ud53c\ub85c \uc218\uba85 \ub610\ub294 \ub07c\uc6cc\ub9de\ucda4\uc744 \uc790\ub3d9\uc73c\ub85c \uacb0\uc815\ud558\uc9c0\ub294 \uc54a\uc2b5\ub2c8\ub2e4. \uc774\ub7ec\ud55c \uacb0\uc815\uc740 \ud558\uc911, \uc7ac\ub8cc, \ud615\uc0c1 \ubc0f \uc124\uacc4 \ubc29\ubc95\uc5d0 \ub530\ub77c \ub2ec\ub77c\uc9d1\ub2c8\ub2e4. \ub3c4\uba74\uc740 \u201c\ud45c\uc900 \ud0a4\ud648\u201d\uacfc \uac19\uc740 \ubaa8\ud638\ud55c \uc8fc\uc11d\uc5d0 \uc758\uc874\ud558\uae30\ubcf4\ub2e4 \ud45c\uc900\uacfc \uac1c\uc815\ud310\uc744 \uba85\uc2dc\ud558\uac70\ub098 \uc644\uc804\ud55c \ub9de\ucda4 \uce58\uc218\ub97c \uc81c\uacf5\ud574\uc57c \ud569\ub2c8\ub2e4.\u201d<\/p>\n<h2 id=\"section-2\">\ud3ed, \uae4a\uc774 \ubc0f \ub07c\uc6cc\ub9de\ucda4 \uc758\ub3c4 \uba85\uc2dc<\/h2>\n<p>\ud0a4\ud648 \ud3ed\uc740 \ud0a4\uc640 \uc2dc\ud2b8 \uc0ac\uc774\uc758 \uce21\uba74 \ub07c\uc6cc\ub9de\ucda4\uc744 \uad00\ub9ac\ud558\uace0, \uae4a\uc774\ub294 \ubc18\uacbd \ubc29\ud5a5 \ub9de\ubb3c\ub9bc\uacfc \ub0a8\uc740 \uc0e4\ud504\ud2b8 \ub2e8\uba74\uc5d0 \uc601\ud5a5\uc744 \uc90d\ub2c8\ub2e4. \ud5c8\ube0c \uc2dc\ud2b8\uc640 \uc0e4\ud504\ud2b8 \uc2dc\ud2b8\ub294 \uad00\ub828\ub418\uc9c0\ub9cc \ub3d9\uc77c\ud558\uc9c0 \uc54a\uc740 \ud53c\ucc98\uc785\ub2c8\ub2e4. \ub3c4\uba74\uc740 \uc0e4\ud504\ud2b8 \uc2dc\ud2b8 \uae4a\uc774\uc640 \uc0e4\ud504\ud2b8 \ubc18\ub300\ud3b8 \ud45c\uba74\uc744 \uae30\uc900\uc73c\ub85c \ud0a4\ud648 \ubc14\ub2e5\uc744 \uc704\uce58\uc2dc\ud0a4\ub294 \ub370 \uc0ac\uc6a9\ub418\ub294 \uce58\uc218\ub97c \uad6c\ubd84\ud574\uc57c \ud569\ub2c8\ub2e4. \uc774 \uad6c\ubd84\uc740 \uc0e4\ud504\ud2b8 \uc704\uc758 \ud0a4 \ub192\uc774\uc640 \ud5c8\ube0c \ub0b4\ubd80\uc758 \uac04\uadf9\uc744 \ud655\uc778\ud560 \ub54c \uc911\uc694\ud569\ub2c8\ub2e4.<\/p>\n<p>\ud0a4\uc640 \ud0a4\uc2dc\ud2b8\uc5d0 \uc801\uc6a9\ub418\ub294 \ud55c\uacc4\uc640 \ub07c\uc6cc\ub9de\ucda4 \ub4f1\uae09\uc744 \uba85\uc2dc\ud558\uc2ed\uc2dc\uc624. \uacb0\ud569 \ud0a4, \ud5c8\ube0c \uc2ac\ub86f, \uc870\ub9bd \ubc29\ubc95 \ubc0f \uc758\ub3c4\ub41c \ud558\uc911 \ubd84\ub2f4\uc744 \uace0\ub824\ud558\uc9c0 \uc54a\uace0 \uc881\uc740 \ud3ed \uacf5\ucc28\ub97c \ucd94\uac00\ud558\uc9c0 \ub9c8\uc2ed\uc2dc\uc624. \ub07c\uc6cc\ub9de\ucda4\uc740 \uae30\uacc4\uacf5\uc758 \uad00\ud589\uc801 \ubc29\uc2dd\uc5d0\uc11c \ucd94\ub860\ud558\ub294 \uac83\uc774 \uc544\ub2c8\ub77c, \uc801\uc6a9 \ud45c\uc900 \ub610\ub294 \uacc4\uc0b0\uc744 \uc0ac\uc6a9\ud558\uc5ec \ucc45\uc784 \uc124\uacc4\uc790\uac00 \uc120\ud0dd\ud574\uc57c \ud569\ub2c8\ub2e4.<\/p>\n<table>\n<thead>\n<tr>\n<th>\ucf5c\uc544\uc6c3 \ud56d\ubaa9<\/th>\n<th>\uc911\uc694\ud55c \uc774\uc720<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>\ud0a4 \ubc0f \ud0a4\uc2dc\ud2b8 \uc720\ud615\/\ud45c\uc900<\/td>\n<td>\uae30\ubcf8 \ud615\uc0c1\uacfc \ub07c\uc6cc\ub9de\ucda4 \uad00\ub840 \uc815\uc758<\/td>\n<\/tr>\n<tr>\n<td>\uc2ac\ub86f \ud3ed \ubc0f \uacf5\ucc28<\/td>\n<td>\uacb0\ud569 \ud0a4\uc640\uc758 \uce21\uba74 \uac04\uadf9 \ub610\ub294 \uac04\uc12d \uad00\ub9ac<\/td>\n<\/tr>\n<tr>\n<td>\uc2dc\ud2b8 \uae4a\uc774 \uae30\uc900<\/td>\n<td>\ud45c\uba74 \uae4a\uc774\uc640 \ubc18\ub300\ucabd \uc704\uce58 \uac04\uc758 \ud63c\ub3d9 \ubc29\uc9c0<\/td>\n<\/tr>\n<tr>\n<td>\uae38\uc774 \ubc0f \ub05d\ub2e8 \uc870\uac74<\/td>\n<td>\uc0ac\uc6a9 \uac00\ub2a5\ud55c \ub9de\ubb3c\ub9bc\uacfc \ud0a4\uc758 \uc885\ub8cc \ubc29\uc2dd\uc744 \uc815\uc758<\/td>\n<\/tr>\n<tr>\n<td>\uc704\uce58 \ub370\uc774\ud140 \ubc0f \uac01\ub3c4 \ubc29\ud5a5<\/td>\n<td>\ud0a4\ud648\uc744 \uc204\ub354, \uad6c\uba4d, \ud50c\ub7ab \ub610\ub294 \uae30\ud0c0 \ud53c\ucc98\uc640 \uc5f0\uad00\uc2dc\ud0b4<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p><img src=\"https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/keyway-width-depth-datum-geometry.webp\" alt=\"\ud0a4\ud648 \ub108\ube44, \uae4a\uc774 \ubc0f \ub370\uc774\ud140 \ud615\uc0c1\" class=\"alignnone size-full wp-image-3837\" width=\"1600\" height=\"900\" loading=\"lazy\" decoding=\"async\" srcset=\"https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/keyway-width-depth-datum-geometry.webp 1600w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/keyway-width-depth-datum-geometry-300x169.webp 300w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/keyway-width-depth-datum-geometry-1024x576.webp 1024w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/keyway-width-depth-datum-geometry-768x432.webp 768w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/keyway-width-depth-datum-geometry-1536x864.webp 1536w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/keyway-width-depth-datum-geometry-18x10.webp 18w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/keyway-width-depth-datum-geometry-800x450.webp 800w\" sizes=\"(max-width: 1600px) 100vw, 1600px\" \/><\/p>\n<h2 id=\"section-3\">\uae30\ub2a5 \ub370\uc774\ud140\uc5d0\uc11c \uc2ac\ub86f \uc704\uce58 \uc9c0\uc815<\/h2>\n<p>\ud5c8\ube0c\ub97c \uc704\uce58\uc2dc\ud0a4\ub294 \uc204\ub354 \ub610\ub294 \ub05d\ub2e8 \ud53c\ucc98\ub85c\ubd80\ud130 \ud0a4\ud648\uc758 \ucd95\ubc29\ud5a5 \uc704\uce58\ub97c \uce58\uc218\ud654\ud558\uc2ed\uc2dc\uc624. \uc870\ub9bd \uc911 \ubc29\ud5a5\uc774 \uc911\uc694\ud55c \uacbd\uc6b0 \ub370\uc774\ud140 \ud50c\ub7ab, \uad00\ud1b5 \uad6c\uba4d, \uc2a4\ud50c\ub77c\uc778 \ub610\ub294 \ub2e4\ub978 \uae30\ub2a5 \uae30\uc900\uc73c\ub85c\ubd80\ud130 \uac01\ub3c4 \ubc29\ud5a5\uc744 \uc815\uc758\ud558\uc2ed\uc2dc\uc624. \ub2e8\uc77c \ud0a4 \uc678\uc5d0 \uac01\ub3c4 \uc694\uad6c\uc0ac\ud56d\uc774 \uc5c6\ub294 \uacbd\uc6b0, \ub370\uc774\ud140 \ucd95 \ub610\ub294 \ub3c4\uba74 \ubdf0\ub97c \uae30\uc900\uc73c\ub85c \uc2ac\ub86f\uc774 \uc5b4\ub5bb\uac8c \uc815\ub82c\ub418\ub294\uc9c0 \uba85\uc2dc\ud558\uc2ed\uc2dc\uc624.<\/p>\n<p>\uc120\uc0ad \ubc0f \ubc00\ub9c1 \uc911 \uc0e4\ud504\ud2b8\uac00 \uc5b4\ub5bb\uac8c \uace0\uc815\ub420\uc9c0 \uace0\ub824\ud558\uc2ed\uc2dc\uc624. \ud0a4\ud648\uc774 \uad00\ud1b5 \uad6c\uba4d \ub610\ub294 \ub2e4\ub978 \ubc00\ub9c1 \ud53c\ucc98\uc640 \uc815\ub82c\uc744 \uc720\uc9c0\ud574\uc57c \ud558\ub294 \uacbd\uc6b0, \uacf5\ud1b5 \ub370\uc774\ud140 \uad6c\uc870 \ub610\ub294 \uc14b\uc5c5 \uac04\uc758 \uc81c\uc5b4\ub41c \uc804\ud658\uc774 \ud544\uc694\ud569\ub2c8\ub2e4. \ud558\ub098\uc758 \uc9c1\uc811\uc801\uc778 \uae30\ub2a5 \uce58\uc218\ub85c \ub354 \uba85\ud655\ud574\uc9c8 \uc218 \uc788\ub294 \uc0c1\ud669\uc5d0\uc11c \ucd5c\uc885 \uad00\uacc4\uac00 \uc5ec\ub7ec \ub3c5\ub9bd \uacf5\ucc28\uc5d0 \uc758\uc874\ud558\uac8c \ub9cc\ub4dc\ub294 \uce58\uc218 \uccb4\uc778\uc740 \ud53c\ud558\uc2ed\uc2dc\uc624.<\/p>\n<p>\uad00\ub828 \uc0e4\ud504\ud2b8 \ud615\uc0c1\uc5d0 \ub300\ud574\uc11c\ub294 \uc0ac\uc774\ud2b8\uc758 <a href=\"https:\/\/www.jccncmachining.com\/ko\/%ed%91%9c%ec%8b%9c\/%ea%b0%80%ea%b3%b5-%ec%83%a4%ed%94%84%ed%8a%b8\/\">\uac00\uacf5 \uc0e4\ud504\ud2b8<\/a> \ubc0f <a href=\"https:\/\/www.jccncmachining.com\/ko\/%ec%97%ad%eb%9f%89\/cnc-%ec%84%a0%eb%b0%98-%ea%b0%80%ea%b3%b5\/\">CNC \uc120\ubc18<\/a> \ud398\uc774\uc9c0\ub97c \uac80\ud1a0\ud558\uc2ed\uc2dc\uc624. \uc2e4\uc81c \uacf5\uc815 \uacbd\ub85c\ub294 \ubd80\ud488\uc758 \uad6c\uc131\uacfc \uc811\uadfc\uc131\uc744 \ub530\ub77c\uc57c \ud569\ub2c8\ub2e4.<\/p>\n<h2 id=\"section-4\">\uac00\uacf5\uacfc \uac80\uc0ac\ub97c \ud568\uaed8 \uacc4\ud68d\ud558\uc2ed\uc2dc\uc624<\/h2>\n<p>\uc678\ubd80 \uc0e4\ud504\ud2b8 \ud0a4\ud648\uc740 \uc0e4\ud504\ud2b8\ub97c \uc9c0\uc9c0\ud558\uace0 \ud544\uc694\ud55c \ubc29\ud5a5\uc73c\ub85c \uc778\ub371\uc2f1\ud55c \uc0c1\ud0dc\uc5d0\uc11c \ubc00\ub9c1\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4. \ud5c8\ube0c\uc758 \ub0b4\ubd80 \ud0a4\uc2dc\ud2b8\ub294 \ud615\uc0c1, \uc218\ub7c9 \ubc0f \uc811\uadfc\uc131\uc5d0 \ub530\ub77c \ube0c\ub85c\uce6d\uc774\ub098 EDM\uacfc \uac19\uc740 \ub2e4\ub978 \uacf5\uc815\uc744 \uc0ac\uc6a9\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4. \uc774 \ubb38\uc11c\ub294 \ud53c\ucc98 \uc815\uc758\uc5d0 \ucd08\uc810\uc744 \ub9de\ucd94\uba70, \ud558\ub098\uc758 \uacf5\uc815\uc774 \ubaa8\ub4e0 \uc124\uacc4\uc5d0 \uc801\ud569\ud558\ub2e4\ub294 \uac83\uc744 \uc758\ubbf8\ud558\uc9c0 \uc54a\uc2b5\ub2c8\ub2e4. \ucf54\ub108 \ubc18\uacbd\uacfc \ub05d\ub2e8 \ub9b4\ub9ac\ud504\uac00 \ud0a4, \uc870\ub9bd \ub610\ub294 \uc751\ub825 \uc9d1\uc911\uc5d0 \uc601\ud5a5\uc744 \ubbf8\uce58\ub294 \uacbd\uc6b0 \uc774\ub97c \uc2dd\ubcc4\ud558\uace0, \uac80\ud1a0 \uc5c6\uc774 \uae30\ub2a5 \uc2dc\ud2b8 \uac00\uc7a5\uc790\ub9ac\uc5d0 \uad11\ubc94\uc704\ud55c \ubaa8\uc11c\ub9ac \ucc98\ub9ac \ub178\ud2b8\ub97c \uc801\uc6a9\ud558\uc9c0 \ub9c8\uc2ed\uc2dc\uc624.<\/p>\n<p><img src=\"https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/shaft-keyway-milling-inspection.webp\" alt=\"\uc0e4\ud504\ud2b8 \ud0a4\ud648 \uac00\uacf5 \ubc0f \uac80\uc0ac\" class=\"alignnone size-full wp-image-3838\" width=\"1600\" height=\"900\" loading=\"lazy\" decoding=\"async\" srcset=\"https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/shaft-keyway-milling-inspection.webp 1600w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/shaft-keyway-milling-inspection-300x169.webp 300w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/shaft-keyway-milling-inspection-1024x576.webp 1024w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/shaft-keyway-milling-inspection-768x432.webp 768w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/shaft-keyway-milling-inspection-1536x864.webp 1536w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/shaft-keyway-milling-inspection-18x10.webp 18w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/11\/shaft-keyway-milling-inspection-800x450.webp 800w\" sizes=\"(max-width: 1600px) 100vw, 1600px\" \/><\/p>\n<p>\uac80\uc0ac\ub294 \ud574\ub2f9 \ud53c\ucc98\uc5d0 \uc801\ud569\ud55c \uae30\uae30\ub098 \uac8c\uc774\uc9c0\ub85c \ud3ed, \uae4a\uc774, \uae38\uc774 \ubc0f \uc704\uce58\ub97c \ud3ec\ud568\ud574\uc57c \ud569\ub2c8\ub2e4. \ud540\uc774\ub098 \ud0a4\ub294 \uce58\uc218\uc640 \ub07c\uc6cc\ub9de\ucda4\uc774 \uad00\ub9ac\ub418\ub294 \uacbd\uc6b0\uc5d0\ub9cc \uae30\ub2a5 \uac80\uc0ac\ub85c \uc0ac\uc6a9\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4. \ud0a4\ud648\uc744 \uc9c1\uc811 \uce21\uc815\ud558\uae30 \uc5b4\ub824\uc6b4 \uacbd\uc6b0, \uc0dd\uc0b0 \uc804\uc5d0 \uce21\uc815 \ubc29\ubc95\uacfc \uae30\uc900\uc5d0 \ud569\uc758\ud558\uc2ed\uc2dc\uc624. \ub07c\uc6cc\ub9de\ucda4\uc774 \ud569\uaca9 \uae30\uc900\uc778 \uacbd\uc6b0 \uc0e4\ud504\ud2b8\ubfd0\ub9cc \uc544\ub2c8\ub77c \ud0a4\uc640 \uacb0\ud569 \ud5c8\ube0c\ub3c4 \uac80\uc0ac\ud558\uc2ed\uc2dc\uc624.<\/p>\n<p>\ub514\ubc84\ub9c1\uc740 \uc2dc\ud2b8\ub97c \ub465\uae00\uac8c \ud558\uac70\ub098 \ud3ed\uc744 \ubcc0\uacbd\ud558\uc9c0 \uc54a\uc73c\uba74\uc11c \ub3cc\ucd9c\ub41c \uac00\uc7a5\uc790\ub9ac\ub97c \uc81c\uac70\ud574\uc57c \ud569\ub2c8\ub2e4. \ud45c\uba74 \uc870\ub3c4\uc640 \ubc84 \uc81c\ud55c\uc740 \uc2dc\ud305 \ub610\ub294 \uc870\ub9bd\uc5d0 \uc601\ud5a5\uc744 \ubbf8\uce58\ub294 \uacbd\uc6b0 \uba85\uc2dc\ud574\uc57c \ud558\uba70, \ube44\uae30\ub2a5 \ud45c\uba74\uc5d0 \uc784\uc758\uc758 \uc694\uad6c\uc0ac\ud56d\uc73c\ub85c \ud655\uc7a5\ud574\uc11c\ub294 \uc548 \ub429\ub2c8\ub2e4.<\/p>\n<h2 id=\"section-5\">\uac80\uc0ac \uac00\ub2a5\ud55c \ud0a4\ud648 \uc815\uc758 \ub9b4\ub9ac\uc2a4<\/h2>\n<p>\uc644\uc804\ud55c \ub9b4\ub9ac\uc2a4 \ud328\ud0a4\uc9c0\uc5d0\ub294 \uc0e4\ud504\ud2b8\uc640 \ud5c8\ube0c \uc778\ud130\ud398\uc774\uc2a4, \uc9c0\uc815\ub41c \uacbd\uc6b0 \ud0a4 \uc720\ud615 \ubc0f \uc7ac\uc9c8, \uc801\uc6a9 \ud45c\uc900 \ubc0f \ud310\ubcf8, \ud0a4\ud648 \uce58\uc218 \ubc0f \ud55c\uacc4, \ub370\uc774\ud140 \ubc0f \ubc29\ud5a5, \uac00\uc7a5\uc790\ub9ac \ucc98\ub9ac, \uac80\uc0ac \ubc29\ubc95, \uadf8\ub9ac\uace0 \ubaa8\ub4e0 \uc870\ub9bd \ud569\uaca9 \uac80\uc0ac\uac00 \ud3ec\ud568\ub429\ub2c8\ub2e4. \ud45c\uc900 \ud45c\ub97c \uc0ac\uc6a9\ud558\ub294 \uacbd\uc6b0 \uc5b4\ub5a4 \ud53c\ucc98\uac00 \ud45c\uc900\uc774\uace0 \uc5b4\ub5a4 \uac83\uc774 \uc218\uc815\ub418\uc5c8\ub294\uc9c0 \uba85\uc2dc\ud558\uc2ed\uc2dc\uc624. \ud5a5\ud6c4 \uacf5\uae09\uc5c5\uccb4\uac00 \uc2b9\uc778\ub41c \ud574\uc11d\uc744 \uc7ac\ud604\ud560 \uc218 \uc788\ub3c4\ub85d \ub3c4\uba74 \ub9ac\ube44\uc804\uc744 \uae30\ub85d\ud558\uc2ed\uc2dc\uc624.<\/p>\n<p>\uacf5\uae09\uc5c5\uccb4 \uc9c8\ubb38\uc744 \uac80\ud1a0\ud560 \ub54c \uc2e4\uc81c \uc124\uacc4 \ubcc0\uacbd\uacfc \uce21\uc815 \uae30\uc900\uc758 \uba85\ud655\ud654\ub97c \uad6c\ubd84\ud558\uc2ed\uc2dc\uc624. \ud3ed, \uae4a\uc774 \ub610\ub294 \ub07c\uc6cc\ub9de\ucda4\uc744 \ubcc0\uacbd\ud558\uc790\ub294 \uc81c\uc548\uc740 \ud558\uc911 \uc804\ub2ec\uacfc \uc870\ub9bd\uc5d0 \uc601\ud5a5\uc744 \ubbf8\uce60 \uc218 \uc788\uc2b5\ub2c8\ub2e4. \uc124\uacc4 \uad8c\ud55c\uc790\uc640 \ud568\uaed8 \ud574\uacb0\ud558\uace0, \uc2b9\uc778 \uc2dc \uad00\ub9ac \ub3c4\uba74\uc744 \uc5c5\ub370\uc774\ud2b8\ud558\uba70, \uac80\uc0ac \ubcf4\uace0\uc11c\ub97c \ud574\ub2f9 \ub9ac\ube44\uc804\uacfc \uc5f0\uacb0\ud574 \uc720\uc9c0\ud558\uc2ed\uc2dc\uc624.<\/p>","protected":false},"excerpt":{"rendered":"<p>A shaft keyway drawing should control more than the slot width. To produce a key that seats and transmits torque as intended, the specification must identify the applicable key\/keyseat standard or custom geometry, keyway width and depth, its angular and axial location, the fit relationship, and the datum used to inspect it. The shaft diameter [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1],"tags":[],"class_list":["post-3808","post","type-post","status-publish","format-standard","hentry","category-blog"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/posts\/3808","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/comments?post=3808"}],"version-history":[{"count":3,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/posts\/3808\/revisions"}],"predecessor-version":[{"id":3839,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/posts\/3808\/revisions\/3839"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/media?parent=3808"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/categories?post=3808"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/tags?post=3808"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}