{"id":1896,"date":"2026-08-08T17:47:06","date_gmt":"2026-08-08T09:47:06","guid":{"rendered":"https:\/\/www.jccncmachining.com\/?p=1896"},"modified":"2026-08-08T17:47:06","modified_gmt":"2026-08-08T09:47:06","slug":"%eb%b2%84%ec%a7%84-peek-%ea%b0%80%ea%b3%b5-%ec%8b%9c-%ed%9c%a8-%eb%b0%8f-%ea%b3%b5%ea%b5%ac-%eb%a7%88%eb%aa%a8-%ec%a0%95%eb%b0%80-%eb%ac%b8%ec%a0%9c-%ed%95%b4%ea%b2%b0","status":"publish","type":"post","link":"https:\/\/www.jccncmachining.com\/ko\/%eb%b8%94%eb%a1%9c%ea%b7%b8\/%eb%b2%84%ec%a7%84-peek-%ea%b0%80%ea%b3%b5-%ec%8b%9c-%ed%9c%a8-%eb%b0%8f-%ea%b3%b5%ea%b5%ac-%eb%a7%88%eb%aa%a8-%ec%a0%95%eb%b0%80-%eb%ac%b8%ec%a0%9c-%ed%95%b4%ea%b2%b0\/","title":{"rendered":"\ubc84\uc9c4 PEEK \uac00\uacf5: \ub4a4\ud2c0\ub9bc, \uacf5\uad6c \ub9c8\ubaa8 \ubc0f \uc815\ubc00\ub3c4 \ubb38\uc81c \ud574\uacb0"},"content":{"rendered":"<p>\uc5ec\ub7ec\ubd84\uc740 \uc911\uc694\ud55c \ubd80\ud488\u2014\uc218\uc220 \uae30\uad6c \uc190\uc7a1\uc774, \ud56d\uacf5\uc6b0\uc8fc \uc13c\uc11c \ud558\uc6b0\uc9d5 \ub610\ub294 \ubc18\ub3c4\uccb4 \uc6e8\uc774\ud37c \uce90\ub9ac\uc5b4\u2014\uc744 \uc124\uacc4\ud558\ub294 \ub370 \uba87 \uc8fc\ub97c \ubcf4\ub0c8\uc2b5\ub2c8\ub2e4. \uc7ac\ub8cc \uc0ac\uc591\uc740 \ubc84\uc9c4 PEEK\ub97c \uc694\uad6c\ud558\uba70, \uac12\ube44\uc2fc \uc6d0\uc790\uc7ac\ub97c \uc870\ub2ec\ud588\uc2b5\ub2c8\ub2e4. \uadf8\ub7f0 \ub2e4\uc74c CNC \uac00\uacf5\uc774 \uc2dc\uc791\ub418\uace0, \uba87 \uc2dc\uac04 \uc548\uc5d0 \ubd80\ud488\uc740 \ud718\uace0, \ud45c\uba74 \uc870\ub3c4\ub294 \uc0ac\ud3ec\ucc98\ub7fc \ubcf4\uc774\uba70, \uacf5\uad6c\ub294 \ud5c8\uc6a9 \ud55c\uacc4\ub97c \ub118\uc5b4 \ub9c8\ubaa8\ub429\ub2c8\ub2e4. \uc774 \uc2dc\ub098\ub9ac\uc624\ub294 \uc804 \uc138\uacc4\uc758 \uae30\uacc4 \uacf5\uc791\uc18c\uc5d0\uc11c \ub9e4\uc77c \ubc8c\uc5b4\uc9d1\ub2c8\ub2e4. \uc88b\uc740 \uc18c\uc2dd\uc740? \uc774\uac83\uc740 \uc644\uc804\ud788 \uc608\ubc29 \uac00\ub2a5\ud558\ub2e4\ub294 \uac83\uc785\ub2c8\ub2e4. \uc774 \uac00\uc774\ub4dc\ub294 \uc774 \uc7ac\ub8cc\ub97c \ud2b9\ubcc4\ud558\uac8c \ub9cc\ub4dc\ub294 \uc694\uc18c\ub97c \uc774\ud574\ud558\ub294 \uac83\ubd80\ud130 \uc77c\uad00\ub418\uace0 \uc815\ubc00\ud55c \uacb0\uacfc\ub97c \uc81c\uacf5\ud558\ub294 \uc18d\ub3c4, \uc774\uc1a1 \ubc0f \uae30\ubc95\uc744 \uc219\ub2ec\ud558\ub294 \uac83\uae4c\uc9c0, \ubc84\uc9c4 PEEK\ub97c \uc131\uacf5\uc801\uc73c\ub85c \uac00\uacf5\ud558\ub294 \ubc29\ubc95\uc744 \uc815\ud655\ud788 \uc548\ub0b4\ud569\ub2c8\ub2e4.<\/p>\n<p><img src=\"https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/08\/machining-virgin-peek.webp\" alt=\"\ubc84\uc9c4 PEEK \uac00\uacf5\" class=\"alignnone size-full wp-image-1898\" width=\"1024\" height=\"768\" loading=\"lazy\" decoding=\"async\" srcset=\"https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/08\/machining-virgin-peek.webp 1024w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/08\/machining-virgin-peek-300x225.webp 300w, https:\/\/www.jccncmachining.com\/wp-content\/uploads\/2026\/08\/machining-virgin-peek-768x576.webp 768w\" sizes=\"(max-width: 1024px) 100vw, 1024px\" \/><\/p>\n<hr \/>\n<h2>\uac00\uacf5\ud574 \ubcf8 \ub2e4\ub978 \ubaa8\ub4e0 \ud50c\ub77c\uc2a4\ud2f1\uacfc \ubc84\uc9c4 PEEK\uac00 \ub2e4\ub978 \uc810<\/h2>\n<p>\ubc84\uc9c4 PEEK\u2014\uc21c\uc218\ud558\uace0 \ucda9\uc804\ub418\uc9c0 \uc54a\uc740 \ud615\ud0dc\uc758 \ud3f4\ub9ac\uc5d0\ud14c\ub974\uc5d0\ud14c\ub974\ucf00\ud1a4\u2014\uc740 \uc5d4\uc9c0\ub2c8\uc5b4\ub9c1 \uc5f4\uac00\uc18c\uc131 \uc218\uc9c0 \ud53c\ub77c\ubbf8\ub4dc\uc758 \uc815\uc0c1\uc5d0 \uc704\uce58\ud569\ub2c8\ub2e4. \uc774\ub294 \ubc18\uacb0\uc815\uc131 \ud3f4\ub9ac\uba38\ub85c, \uc5f0\uc18d \uc0ac\uc6a9 \uc628\ub3c4\ub294 260\u00b0C(500\u00b0F)\uc774\uace0 \uc735\uc810\uc740 \uc57d 343\u00b0C(649\u00b0F)\uc785\ub2c8\ub2e4. \uc774 \uc7ac\ub8cc\ub294 \ub6f0\uc5b4\ub09c \ub0b4\ud654\ud559\uc131, \uc6b0\uc218\ud55c \ub9c8\ubaa8 \ud2b9\uc131 \ubc0f \ub180\ub77c\uc6b4 \uce58\uc218 \uc548\uc815\uc131\uc744 \uc81c\uacf5\ud569\ub2c8\ub2e4. \uac00\uc218\ubd84\ud574, \uacfc\uc5f4 \uc99d\uae30 \ubc0f \ub2e4\uc591\ud55c \uacf5\uaca9\uc801\uc778 \ud654\ud559\ubb3c\uc9c8\uc5d0 \uc800\ud56d\ud569\ub2c8\ub2e4. \ubc84\uc9c4 \uc0c1\ud0dc\uc5d0\uc11c\ub294 \ubaa8\ub4e0 PEEK \ub4f1\uae09 \uc911 \uac00\uc7a5 \ub192\uc740 \uc778\uc131\uacfc \uc2e0\uc728\uc744 \uc81c\uacf5\ud558\ubbc0\ub85c \uc758\ub8cc\uc6a9 \uc784\ud50c\ub780\ud2b8, \uc804\uae30 \uc808\uc5f0\uccb4 \ubc0f \uc2dd\ud488 \uac00\uacf5 \ubd80\ud488\uc5d0 \ud2b9\ud788 \uc801\ud569\ud569\ub2c8\ub2e4.<\/p>\n<p>\ud558\uc9c0\ub9cc \uc7ac\ub8cc \ub370\uc774\ud130\uc2dc\ud2b8\uac00 \uc54c\ub824\uc8fc\uc9c0 \uc54a\ub294 \uac83\uc774 \uc788\uc2b5\ub2c8\ub2e4. \ubc84\uc9c4 PEEK\ub294 \uc5ec\ub7ec\ubd84\uc774 \uac00\uacf5\ud574 \ubcf8 \uc544\uc138\ud0c8, \ub098\uc77c\ub860 \ub610\ub294 \uae30\ud0c0 \uc5d4\uc9c0\ub2c8\uc5b4\ub9c1 \ud50c\ub77c\uc2a4\ud2f1\uacfc \uc804\ud600 \ub2e4\ub974\uac8c \uac70\ub3d9\ud569\ub2c8\ub2e4. \uc720\ub9ac \uc804\uc774 \uc628\ub3c4\uac00 143\u00b0C(289\u00b0F)\ub77c\ub294 \uac83\uc740 \ub2e4\ub978 \ud3f4\ub9ac\uba38\uac00 \ub048\uc801\ud574\uc9c0\ub294 \uc628\ub3c4\uc5d0\uc11c\ub3c4 \ub2e8\ub2e8\ud558\uac8c \uc720\uc9c0\ub41c\ub2e4\ub294 \ub73b\uc785\ub2c8\ub2e4. \uc774\ub294 \uc644\uc131\ub41c \ubd80\ud488\uc5d0\ub294 \ud0c1\uc6d4\ud558\uc9c0\ub9cc \ud604\uc7a5\uc5d0\uc11c\ub294 \uc2e4\uc81c\uc801\uc778 \uc5b4\ub824\uc6c0\uc744 \ub9cc\ub4ed\ub2c8\ub2e4. \uc774 \uc7ac\ub8cc\ub294 \uc544\uc138\ud0c8\uc774 \uc0dd\uc131\ud558\ub294 \ubd80\uc11c\uc9c0\uae30 \uc26c\uc6b4 \uce69\uc744 \ud615\uc131\ud558\uc9c0 \uc54a\uc2b5\ub2c8\ub2e4\u2014\uce69\uc740 \uc2e4\ucc98\ub7fc \ub298\uc5b4\uc9c8 \uc218 \uc788\uc73c\uba70 \uc808\uc0ad \uc18d\ub3c4\uac00 \ub108\ubb34 \ub0ae\uc73c\uba74 \ud45c\uba74\uc5d0 \ub2e4\uc2dc \uc735\ucc29\ub420 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<p>\uc544\ub9c8\ub3c4 \uc131\uacf5\uc801\uc778 \ubc84\uc9c4 PEEK \uac00\uacf5\uacfc \uac12\ube44\uc2fc \uc2e4\ud328\ub97c \uac00\ub974\ub294 \uac00\uc7a5 \uc911\uc694\ud55c \uc694\uc778\uc740 \ub0b4\ubd80 \uc751\ub825\uc785\ub2c8\ub2e4. \uc555\ucd9c\ub41c PEEK \ubd09 \ubc0f \ud310\uc7ac\ub294 \uc678\ubd80\uc5d0\uc11c \ub0b4\ubd80\ub85c \ub0c9\uac01\ub418\uba74\uc11c \ud45c\uba74\uce35\uc5d0\ub294 \uc555\ucd95 \uc751\ub825\uc744, \ucf54\uc5b4\uc5d0\ub294 \uc778\uc7a5 \uc751\ub825\uc744 \uace0\uc815\uc2dc\ud0b5\ub2c8\ub2e4. \uc7ac\ub8cc\ub97c \uac00\uacf5\ud558\uc5ec \uc81c\uac70\ud558\uba74 \uc774 \uc751\ub825 \uade0\ud615\uc774 \uae68\uc9d1\ub2c8\ub2e4. \uc5b4\ub2d0\ub9c1\ub418\uc9c0 \uc54a\uc740 \uc6d0\uc790\uc7ac\uc758 \uc9c1\uacbd 100mm \ubd09\uc5d0\uc11c \ud669\uc0ad \uac00\uacf5 \ud6c4 0.13~0.38mm\uc758 \ubcc0\ud615\uc774 \ucda9\ubd84\ud788 \uac00\ub2a5\ud569\ub2c8\ub2e4. \uc774\ub294 \ub9ce\uc740 \ud45c\uc900 CNC \uacf5\ucc28\ubcf4\ub2e4 \ud070 \uac12\uc785\ub2c8\ub2e4. \uc9c1\uc120 \uc808\ub2e8\uc774 \ub208\uc55e\uc5d0\uc11c \ubc14\ub098\ub098 \ubaa8\uc591\uc774 \ub420 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<p>\uadf8\ub9ac\uace0 \ube44\uc6a9 \uace0\ub824 \uc0ac\ud56d\ub3c4 \uc788\uc2b5\ub2c8\ub2e4. \ucda9\uc804\ub418\uc9c0 \uc54a\uc740 \ubc84\uc9c4 PEEK\uc758 \uc9c1\uacbd 50mm x \uae38\uc774 300mm \ubd09\uc740 \ub4f1\uae09\uc5d0 \ub530\ub77c $150~$300\uc785\ub2c8\ub2e4. \ubd80\ud488\uc744 \ud3d0\uae30\ud558\uba74 \uc0ac\uc774\ud074 \uc2dc\uac04\ub9cc \uc190\ud574\uac00 \uc544\ub2c8\ub77c \uc6d0\uc790\uc7ac\ub9cc\uc73c\ub85c\ub3c4 $100 \uc774\uc0c1\uc758 \ube44\uc6a9\uc774 \ub4ed\ub2c8\ub2e4. \uc774\uac83\uc774 \ubc84\uc9c4 PEEK \uac00\uacf5\uc774 \ub2e4\ub978 \uc5b4\ub5a4 \uc5d4\uc9c0\ub2c8\uc5b4\ub9c1 \ud50c\ub77c\uc2a4\ud2f1\ubcf4\ub2e4 \ub354 \ub9ce\uc740 \uacc4\ud68d, \ub354 \ub9ce\uc740 \uacf5\uc815 \uc81c\uc5b4 \ubc0f \ub354 \ub9ce\uc740 \uc7ac\ub8cc\ubcc4 \uc9c0\uc2dd\uc744 \uc694\uad6c\ud558\ub294 \uc774\uc720\uc785\ub2c8\ub2e4.<\/p>\n<hr \/>\n<h2>\ubc84\uc9c4 PEEK \uac00\uacf5\uc758 \ub2e4\uc12f \uac00\uc9c0 \ud575\uc2ec \uacfc\uc81c<\/h2>\n<p>\uc7a5\uc560\ubb3c\uc744 \uc774\ud574\ud558\ub294 \uac83\uc774 \uc774\ub97c \uadf9\ubcf5\ud558\ub294 \uccab\uac78\uc74c\uc785\ub2c8\ub2e4. \uad11\ubc94\uc704\ud55c \ud604\uc7a5 \uacbd\ud5d8\uacfc \uac00\uacf5 \ucee4\ubba4\ub2c8\ud2f0\uc758 \uc758\uacac\uc744 \ubc14\ud0d5\uc73c\ub85c, \uc791\uc5c5\uc7a5\uc5d0\uc11c \ubc84\uc9c4 PEEK \uac00\uacf5\uc744 \uc2dc\ub3c4\ud560 \ub54c \uc77c\uad00\ub418\uac8c \ub098\ud0c0\ub098\ub294 \ub2e4\uc12f \uac00\uc9c0 \uacfc\uc81c\ub294 \ub2e4\uc74c\uacfc \uac19\uc2b5\ub2c8\ub2e4.<\/p>\n<h3>1. \uc5f4 \ucd95\uc801 \ubc0f \uc5f4 \uad00\ub9ac<\/h3>\n<p>\ubc84\uc9c4 PEEK\ub294 \uc5f4\uc804\ub3c4\uc728\uc774 \ub0ae\uc2b5\ub2c8\ub2e4. \uae08\uc18d\ucc98\ub7fc \uc5f4\uc744 \ubc1c\uc0b0\ud558\uc9c0 \uc54a\uc2b5\ub2c8\ub2e4. \uc808\uc0ad \uacc4\uba74\uc5d0\uc11c \ubc1c\uc0dd\ud55c \uc5f4\uc740 \uc9d1\uc911\ub41c \ucc44\ub85c \ub0a8\uc544 \ud3f4\ub9ac\uba38\ub97c \uc5f0\ud654\uc2dc\ud0a4\uace0 \uc2a4\ubbf8\uc5b4\ub9c1, \uc6a9\uc735 \ub610\ub294 \ubcc0\ud615\uc744 \uc77c\uc73c\ud0b5\ub2c8\ub2e4. \uc774\ub294 PEEK \uac00\uacf5\uc5d0\uc11c \uc5f4\uc545\ud55c \ud45c\uba74 \uc870\ub3c4\uc640 \uce58\uc218 \ub4dc\ub9ac\ud504\ud2b8\uc758 \uac00\uc7a5 \ud754\ud55c \ub2e8\uc77c \uc6d0\uc778\uc785\ub2c8\ub2e4.<\/p>\n<p>\ud3ec\ub7fc\uc758 \uc219\ub828\ub41c \uae30\uacc4\uacf5\ub4e4\uc740 \uc5f4 \uad00\ub9ac\uac00 \ub2e4\ub978 \uc5b4\ub5a4 \ub9e4\uac1c\ubcc0\uc218\ubcf4\ub2e4 \uc911\uc694\ud558\ub2e4\uace0 \uc790\uc8fc \uac15\uc870\ud569\ub2c8\ub2e4. \ud55c Reddit \uc0ac\uc6a9\uc790\ub294 \u201cPEEK\ub97c \uc798\ubabb \ubcf4\uba74 \ub179\uc744 \uac83\ucc98\ub7fc \ub300\ud558\ub77c\u2014\uc798\ubabb\ub41c \uc18d\ub3c4\uc640 \uc774\uc1a1\uc5d0\uc11c\ub294 \uc2e4\uc81c\ub85c \uadf8\ub807\uac8c \ub418\uae30 \ub54c\ubb38\uc774\ub2e4\u201d\ub77c\uace0 \uc5b8\uae09\ud588\uc2b5\ub2c8\ub2e4. \uc804\ubb38\uac00\ub4e4\uc758 \uc758\uacac\uc740 \ubd84\uba85\ud569\ub2c8\ub2e4: \uacf5\uad6c\ub97c \uacc4\uc18d \uc6c0\uc9c1\uc774\uace0, \uc815\uc9c0 \uc2dc\uac04\uc744 \ud53c\ud558\uba70, \uce69 \ubc30\ucd9c\uc744 \uc6b0\uc120\uc2dc\ud558\uc2ed\uc2dc\uc624.<\/p>\n<h3>2. \uc794\ub958 \uc751\ub825 \ubc0f \ud728<\/h3>\n<p>\uc55e\uc11c \uc5b8\uae09\ud588\ub4ef\uc774, \uc555\ucd9c \uacf5\uc815\uc5d0\uc11c \ube44\ub86f\ub41c \ub0b4\ubd80 \uc751\ub825\uc740 \uc815\ubc00 PEEK \uac00\uacf5\uc758 \uc228\uc740 \uc801\uc785\ub2c8\ub2e4. \ubc84\uc9c4 PEEK\ub97c \ub2e4\ub978 \ud50c\ub77c\uc2a4\ud2f1\ucc98\ub7fc \ucde8\uae09\ud558\ub294 \uc77c\ubc18 \uc791\uc5c5\uc7a5\uc740 \uc885\uc885 \ubd80\ud488\uc744 \ud53d\uc2a4\ucc98\uc5d0\uc11c \uc81c\uac70\ud55c \ud6c4\uc5d0\uc57c \ud728\uc744 \ubc1c\uacac\ud569\ub2c8\ub2e4\u2014\uadf8\ub54c\ub294 \uc774\ubbf8 \ub108\ubb34 \ub2a6\uc2b5\ub2c8\ub2e4. \uc587\uc740 \ubcbd \ubd80\ud488\uc740 \ud2b9\ud788 \ucde8\uc57d\ud569\ub2c8\ub2e4.<\/p>\n<p>\ud55c \ud56d\uacf5\uc6b0\uc8fc \uacf5\uae09\uc5c5\uccb4\ub294 \uc5b4\ub2d0\ub9c1 \ub2e8\uacc4\ub97c \uac74\ub108\ub6f4 \uacb0\uacfc \ud0c0\uc6d0\ub3c4 \ubc0f \ubcc0\ud615\uc73c\ub85c \uc778\ud574 22%\uc758 \ubd88\ub7c9\ub960\uc774 \ubc1c\uc0dd\ud588\ub2e4\uace0 \ubcf4\uace0\ud588\uc2b5\ub2c8\ub2e4. \uc801\uc808\ud55c \uc751\ub825 \uc644\ud654 \uc808\ucc28\ub97c \uc2dc\ud589\ud55c \ud6c4 \uadf8 \ube44\uc728\uc740 1% \ubbf8\ub9cc\uc73c\ub85c \ub5a8\uc5b4\uc84c\uc2b5\ub2c8\ub2e4.<\/p>\n<h3>3. \uacf5\uad6c \ub9c8\ubaa8 \ubc0f \uc120\ud0dd<\/h3>\n<p>\ube44\ucda9\uc804 PEEK\ub294 \ud544\ub7ec\uac00 \uc5c6\uc744 \uc218 \uc788\uc9c0\ub9cc, \ud45c\uc900 \uce74\ubc14\uc774\ub4dc \ucee4\ud130\ub97c \ube60\ub974\uac8c \ubb34\ub514\uac8c \ub9cc\ub4e4 \ub9cc\ud07c \uc5ec\uc804\ud788 \uc5f0\ub9c8\uc131\uc774 \uc788\uc2b5\ub2c8\ub2e4. \ubb34\ub518 \uacf5\uad6c\ub294 \uc808\uc0ad\ub825\uc744 \uc99d\uac00\uc2dc\ud0a4\uace0, \ub354 \ub9ce\uc740 \uc5f4\uc744 \ubc1c\uc0dd\uc2dc\ud0a4\uba70, \uc5f4\uc545\ud55c \ud45c\uba74 \uc870\ub3c4\ub97c \ub9cc\ub4e4\uc5b4\ub0c5\ub2c8\ub2e4. \uac00\uacf5 \uc5c5\uacc4\uc5d0\uc11c\ub294 \ube44\ucda9\uc804 PEEK\uc5d0 \ub300\ud574 \uc5f0\ub9c8\ub41c \ud648\uc744 \uac16\ucd98 \ubbf8\ub9bd\uc790 \ucd08\uacbd \uacf5\uad6c\ub97c \uc77c\uad00\ub418\uac8c \uad8c\uc7a5\ud569\ub2c8\ub2e4. \uc2e4\ub9ac\ucf58 \uce74\ubc14\uc774\ub4dc \uacf5\uad6c\ub3c4 \ub610 \ub2e4\ub978 \uc88b\uc740 \uc120\ud0dd\uc785\ub2c8\ub2e4.<\/p>\n<p>\ud55c \uc791\uc5c5\uc7a5 \uad00\ub9ac\uc790\ub294 \uc774\ub807\uac8c \ub9d0\ud588\uc2b5\ub2c8\ub2e4. \u201c\uacf5\uad6c\uc5d0\uc11c \uc090\uac71\uac70\ub9ac\ub294 \uc18c\ub9ac\uac00 \ub4e4\ub9ac\uac70\ub098 \uce69\uc5d0 \ubcc0\uc0c9\uc774 \ubcf4\uc774\uba74 \uc989\uc2dc \uba48\ucd94\uc2ed\uc2dc\uc624. \uacf5\uad6c\ub294 \uc774\ubbf8 \uc218\uba85\uc774 \ub2e4\ud588\uace0, \ub3c8\uc744 \ud0dc\uc6b0\uace0 \uc788\ub294 \uac83\uc5d0 \ubd88\uacfc\ud569\ub2c8\ub2e4.\u201d<\/p>\n<h3>4. \uce69 \uc81c\uc5b4 \ubc0f \ubc30\ucd9c<\/h3>\n<p>\ube44\ucda9\uc804 PEEK\ub294 \uacf5\uad6c\uc5d0 \uac10\uae30\uac70\ub098 \uacf5\uc791\ubb3c \ud45c\uba74\uc5d0 \ub2e4\uc2dc \uc735\ucc29\ub420 \uc218 \uc788\ub294 \uc2e4\ucc98\ub7fc \ub298\uc5b4\uc9c0\ub294 \uc5f0\uc18d \uce69\uc744 \uc0dd\uc131\ud569\ub2c8\ub2e4. \uce69 \ubc30\ucd9c\uc774 \ubd88\ub7c9\ud558\uba74 \uc7ac\uc808\uc0ad, \uc5f4 \uc99d\uac00, \ud45c\uba74 \uacb0\ud568\uc774 \ubc1c\uc0dd\ud569\ub2c8\ub2e4. \uc555\ucd95 \uacf5\uae30 \ub610\ub294 \uc9c4\uacf5 \uc2dc\uc2a4\ud15c\uc740 \uce69\uc744 \ud6a8\uacfc\uc801\uc73c\ub85c \uc81c\uac70\ud558\ub294 \ub370 \ud544\uc218\uc801\uc785\ub2c8\ub2e4.<\/p>\n<h3>5. \ud45c\uba74 \uc870\ub3c4 \ubc0f \ubc84 \ud615\uc131<\/h3>\n<p>PEEK\ub294 \ud2b9\ud788 \uc791\uc740 \ud615\uc0c1, \ub0b4\ubd80 \ub098\uc0ac\uc0b0 \ub610\ub294 \uac00\uc7a5\uc790\ub9ac \uc8fc\ubcc0\uc5d0\uc11c \ud480\ub9bc\uacfc \ubc84\uac00 \uc0dd\uae30\ub294 \uacbd\ud5a5\uc774 \uc788\uc2b5\ub2c8\ub2e4. \uc774\ubb3c\uc9c8\uc774 \ud5c8\uc6a9\ub418\uc9c0 \uc54a\ub294 \uc758\ub8cc \ubc0f \ud56d\uacf5\uc6b0\uc8fc \ubd80\ud488\uc758 \uacbd\uc6b0 \uc774\ub294 \uc0c1\ub2f9\ud55c \ud488\uc9c8 \ubb38\uc81c\ub97c \uc57c\uae30\ud569\ub2c8\ub2e4. \uace0\uc18d \ub9c8\uc774\ud06c\ub85c \ub514\ubc84\ub9c1 \uacf5\uad6c, \ub808\uc774\uc800 \ub514\ubc84\ub9c1, \ub2e8\uc77c \ud648 \ub9ac\uba38\uac00 \uc77c\ubc18\uc801\uc778 \ud574\uacb0\ucc45\uc785\ub2c8\ub2e4.<\/p>\n<hr \/>\n<h2>\ube44\ucda9\uc804 PEEK \uac00\uacf5: \ud6a8\uacfc\uc801\uc778 \uc18d\ub3c4, \uc774\uc1a1 \ubc0f \ub9e4\uac1c\ubcc0\uc218<\/h2>\n<p>\uc218\uce58\ub97c \uc815\ud655\ud788 \ub9de\ucd94\uba74 \ube44\ucda9\uc804 PEEK \uac00\uacf5\uc774 \ub3c4\ubc15\uc5d0\uc11c \uc608\uce21 \uac00\ub2a5\ud55c \uacf5\uc815\uc73c\ub85c \ubc14\ub01d\ub2c8\ub2e4. \ub2e4\uc74c \ub9e4\uac1c\ubcc0\uc218\ub294 \uad11\ubc94\uc704\ud55c \ud14c\uc2a4\ud2b8\uc640 \uc2e4\uc81c \uc0dd\uc0b0 \uacbd\ud5d8\uc744 \ubc14\ud0d5\uc73c\ub85c \ud55c \uc5c5\uacc4 \ud569\uc758\ub97c \ub098\ud0c0\ub0c5\ub2c8\ub2e4.<\/p>\n<h3>\ube44\ucda9\uc804 PEEK \uad8c\uc7a5 \uc808\uc0ad \ub9e4\uac1c\ubcc0\uc218<\/h3>\n<table>\n<thead>\n<tr>\n<th><strong>\uc791\uc5c5<\/strong><\/th>\n<th><strong>\uc808\uc0ad \uc18d\ub3c4 (m\/min)<\/strong><\/th>\n<th><strong>\uc774\uc1a1 \uc18d\ub3c4<\/strong><\/th>\n<th><strong>\uc808\uc0ad \uae4a\uc774<\/strong><\/th>\n<th><strong>\uacf5\uad6c \uad8c\uc7a5 \uc0ac\ud56d<\/strong><\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\ubc00\ub9c1 \u2013 \ud669\uc0ad<\/strong><\/td>\n<td>150 \u2013 300<\/td>\n<td>0.05 \u2013 0.15 mm\/\ub0a0<\/td>\n<td>0.5 \u2013 1.0 mm \ucd95\ubc29\ud5a5<\/td>\n<td>\ubbf8\uc138 \uc785\uc790 \uce74\ubc14\uc774\ub4dc, 2-3 \ub0a0<\/td>\n<\/tr>\n<tr>\n<td><strong>\ubc00\ub9c1 \u2013 \uc815\uc0ad<\/strong><\/td>\n<td>200 \u2013 400<\/td>\n<td>0.05 \u2013 0.10 mm\/\ub0a0<\/td>\n<td>0.1 \u2013 0.3 mm<\/td>\n<td>\ub0a0\uce74\ub85c\uc6b4 \uce74\ubc14\uc774\ub4dc, \uc5f0\ub9c8\ub41c \ud648<\/td>\n<\/tr>\n<tr>\n<td><strong>\uc120\uc0ad<\/strong><\/td>\n<td>200 \u2013 400<\/td>\n<td>0.10 \u2013 0.30 mm\/\ud68c\uc804<\/td>\n<td>0.5 \u2013 2.0 mm<\/td>\n<td>\ud3ec\uc9c0\ud2f0\ube0c \ub808\uc774\ud06c \uce74\ubc14\uc774\ub4dc<\/td>\n<\/tr>\n<tr>\n<td><strong>\ub4dc\ub9b4\ub9c1<\/strong><\/td>\n<td>50 \u2013 100<\/td>\n<td>0.05 \u2013 0.15 mm\/\ud68c\uc804<\/td>\n<td>\ud574\ub2f9 \uc5c6\uc74c<\/td>\n<td>\uc0e4\ud504 HSS \ub610\ub294 \ucd08\uacbd, \ube48\ubc88\ud55c \ud6c4\ud1f4<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>\ucd9c\ucc98: \uc0b0\uc5c5 \uac00\uacf5 \uac00\uc774\ub4dc \ubc0f \ud30c\ub77c\ubbf8\ud130 \ub370\uc774\ud130\ubca0\uc774\uc2a4<\/p>\n<p>\ubbf8\ucda9\uc804 Virgin PEEK \ubc00\ub9c1\uc758 \ucd5c\uc801 \uc870\uac74\uc740 \uc77c\ubc18\uc801\uc73c\ub85c 300\u2013600 SFM(91\u2013183 m\/min)\uc73c\ub85c, \uc774\ub294 \uc544\uc138\ud0c8\uc5d0 \uc0ac\uc6a9\ub418\ub294 \uc18d\ub3c4\uc758 \uc57d \ub450 \ubc30\uc785\ub2c8\ub2e4. 180 m\/min\uc5d0\uc11c 6 mm 2\ub0a0 \ucd08\uacbd \ucee4\ud130\uc758 \uacbd\uc6b0 \uc774\ub294 \uc57d 9,550 RPM\uc73c\ub85c \ud658\uc0b0\ub418\uba70, \uc774\ub54c \uc774\uc1a1 \uc18d\ub3c4\ub294 \ub0a0\ub2f9 0.04 mm\uc5d0\uc11c \uc57d 764 mm\/min\uc785\ub2c8\ub2e4.<\/p>\n<p>\ud074\ub77c\uc784 \ubc00\ub9c1\uc774 \ucee8\ubca4\uc154\ub110 \ubc00\ub9c1\ubcf4\ub2e4 \uac15\ub825\ud788 \uc120\ud638\ub429\ub2c8\ub2e4. \ud074\ub77c\uc784 \ubc00\ub9c1\uc740 \uc808\uc0ad\ub825\uc744 \ub0ae\ucd94\uace0 \ud45c\uba74 \uc870\ub3c4\ub97c \uac1c\uc120\ud558\uba70 \uc5f4 \uc785\ub825\uc744 \uc904\uc785\ub2c8\ub2e4. \ub098\uc0ac \uac00\uacf5\uc758 \uacbd\uc6b0, \uc120\ubc18\uc5d0\uc11c\uc758 \ub2e8\uc77c \ud3ec\uc778\ud2b8 \ub098\uc0ac \uac00\uacf5\uc774 \uac00\uc7a5 \uc815\ud655\ud55c PEEK \ub098\uc0ac\ub97c \uc0dd\uc131\ud569\ub2c8\ub2e4.<\/p>\n<h3>\uacf5\uad6c\uc640 \ubd80\ud488 \ubaa8\ub450\ub97c \ubcf4\ud638\ud558\ub294 \ub0c9\uac01 \uc804\ub7b5<\/h3>\n<p>\ub0c9\uac01 \ubc29\uc2dd\uc740 \uc6a9\ub3c4\uc5d0 \ub530\ub77c \ub2ec\ub77c\uc9d1\ub2c8\ub2e4. \uc0b0\uc5c5\uc6a9 \ub4f1\uae09 Virgin PEEK\uc758 \uacbd\uc6b0, \uc218\uc6a9\uc131 \ub610\ub294 \uacbd\uc720 \uae30\ubc18 \ub0c9\uac01\uc81c\ub97c \uc0ac\uc6a9\ud55c \ud50c\ub7ec\ub4dc \ub0c9\uac01\uc774 \ud6a8\uacfc\uc801\uc785\ub2c8\ub2e4. \uace0\uc555 \ub178\uc990\uc740 \uacf5\uad6c-\uacf5\uc791\ubb3c \uc811\ucd09\uba74\uc744 \uc9c1\uc811 \uaca8\ub0e5\ud574\uc57c \ud569\ub2c8\ub2e4.<\/p>\n<p>\uadf8\ub7ec\ub098 \uc758\ub8cc\uc6a9 \ub4f1\uae09 Virgin PEEK\uc758 \uacbd\uc6b0 \uc0dd\uccb4 \uc801\ud569\uc131\uc744 \uc720\uc9c0\ud558\uae30 \uc704\ud574 \uc720\uc131 \ub0c9\uac01\uc81c\ub97c \ud53c\ud574\uc57c \ud569\ub2c8\ub2e4. 5\u20137 bar\uc758 \uc555\ucd95 \uacf5\uae30 \ub610\ub294 \ud0c8\uc774\uc628\uc218\uac00 \ud45c\uc900 \ubc29\uc2dd\uc785\ub2c8\ub2e4. \uad6d\ubd80\uc801 \uae09\ub0c9\uc740 \ucde8\uc131\uc744 \uc720\ubc1c\ud560 \uc218 \uc788\uc73c\ubbc0\ub85c \uacf5\uae30 \ub178\uc990\uc744 \uacc4\uc18d \uc6c0\uc9c1\uc5ec\uc57c \ud569\ub2c8\ub2e4.<\/p>\n<p>\uc77c\ubd80 \uc791\uc5c5\uc7a5\uc5d0\uc11c\ub294 \ub35c \uacf5\uaca9\uc801\uc778 \uc791\uc5c5\uc5d0 \ub300\ud574 \ucd5c\uc18c\ub7c9 \uc724\ud65c(MQL)\ub85c \uc131\uacf5\ud588\ub2e4\uace0 \ubcf4\uace0\ud569\ub2c8\ub2e4. \ub728\uac70\uc6b4 \ubd80\ud488\uc5d0 \ucc28\uac00\uc6b4 \ub0c9\uac01\uc81c\uac00 \ub2ff\uc544 \ubc1c\uc0dd\ud558\ub294 \uc5f4 \ucda9\uaca9\uc774 \ubbf8\uc138 \uade0\uc5f4\uc744 \uc720\ubc1c\ud560 \uc218 \uc788\uc73c\ubbc0\ub85c PEEK\uc5d0\ub294 \ud50c\ub7ec\ub4dc \ub0c9\uac01\uc774 \uc77c\ubc18\uc801\uc73c\ub85c \uad8c\uc7a5\ub418\uc9c0 \uc54a\uc2b5\ub2c8\ub2e4.<\/p>\n<hr \/>\n<h2>\uc5b4\ub2d0\ub9c1 \ud504\ub85c\ud1a0\ucf5c: \ubcc0\ud615\uc5d0 \ub300\ube44\ud558\ub294 \ubcf4\ud5d8 \uc815\ucc45<\/h2>\n<p>Virgin PEEK \uac00\uacf5\uc5d0\uc11c \uc804\ubb38\uac00\uc640 \uc544\ub9c8\ucd94\uc5b4\ub97c \uad6c\ubd84\ud558\ub294 \ub2e8 \ud55c \uac00\uc9c0 \ub2e8\uacc4\uac00 \uc788\ub2e4\uba74 \ubc14\ub85c \uc5b4\ub2d0\ub9c1\uc785\ub2c8\ub2e4. \uc774 \uc5f4\ucc98\ub9ac\ub294 \ub0b4\ubd80 \uc751\ub825\uc744 \uc644\ud654\ud558\uace0 \uacb0\uc815\ud654\ub3c4\ub97c 35\u201340%\uae4c\uc9c0 \ub192\uc774\uba70 \uc7ac\ub8cc \uad6c\uc870\ub97c \uc548\uc815\ud654\ud569\ub2c8\ub2e4. \uc774\ub97c \uc0dd\ub7b5\ud558\uba74 \ucd5c\uc885 \uac80\uc0ac \uc911 \uce58\uc218 \ubcc0\ub3d9\uacfc \ubd80\ud488 \ubd88\ud569\uaca9 \uc704\ud5d8\uc774 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<p>\uac00\uacf5 \uc804 \uc6d0\uc7ac\ub8cc Virgin PEEK \uc18c\uc7ac\ub97c \uc5b4\ub2d0\ub9c1\ud558\ub294 \uac83\uc774 \ud45c\uc900 \uad00\ud589\uc785\ub2c8\ub2e4. \uc774 \uacf5\uc815\uc740 \ub2e4\uc74c\uc744 \ud3ec\ud568\ud569\ub2c8\ub2e4:<\/p>\n<ul>\n<li><strong>\uc2b9\uc628:<\/strong> \uc81c\uc5b4\ub41c \uc624\ube10\uc5d0\uc11c \uc7ac\ub8cc\ub97c 200\u2013220\u00b0C\uae4c\uc9c0 \uc810\uc9c4\uc801\uc73c\ub85c \uac00\uc5f4<\/li>\n<li><strong>\uc720\uc9c0:<\/strong> \uc7ac\ub8cc \ub450\uaed8 10 mm\ub2f9 \uc57d 30\ubd84\uc744 \uae30\uc900\uc73c\ub85c 1\u20132\uc2dc\uac04 \ub3d9\uc548 \uc628\ub3c4 \uc720\uc9c0<\/li>\n<li><strong>\uc11c\ub0c9:<\/strong> \uc624\ube10\uc744 \ub044\uace0 \uc7ac\ub8cc\uac00 \uc218 \uc2dc\uac04\uc5d0 \uac78\uccd0 \uc2e4\uc628\uc73c\ub85c \ub0c9\uac01\ub418\ub3c4\ub85d \ud558\uc2ed\uc2dc\uc624\u2014\uc808\ub300 \ub728\uac70\uc6b4 \uc0c1\ud0dc\uc5d0\uc11c \ubd80\ud488\uc744 \uaebc\ub0b4\uc9c0 \ub9c8\uc2ed\uc2dc\uc624<\/li>\n<\/ul>\n<p>\ub300\ub7c9\uc758 \uc7ac\ub8cc \uc81c\uac70\uac00 \ud544\uc694\ud55c \ubcf5\uc7a1\ud55c \ubd80\ud488\uc758 \uacbd\uc6b0, \ud669\uc0ad \uac00\uacf5 \ud6c4 \uc815\uc0ad \uac00\uacf5 \uc804\uc5d0 \uc911\uac04 \uc5b4\ub2d0\ub9c1\uc744 \uc2e4\uc2dc\ud560 \uac83\uc744 \uc801\uadf9 \uad8c\uc7a5\ud569\ub2c8\ub2e4. \uc774\ub807\uac8c \ud558\uba74 \ud669\uc0ad \uc911\uc5d0 \ubc29\ucd9c\ub41c \uc751\ub825\uc774 \ucd5c\uc885 \uc815\ubc00 \uc808\uc0ad \uc804\uc5d0 \uc548\uc815\ud654\ub429\ub2c8\ub2e4.<\/p>\n<p>\ud55c Jucheng Precision \uc5d4\uc9c0\ub2c8\uc5b4\ub294 \uc5b4\ub2d0\ub9c1 \uacf5\uc815\uc744 \u201c\ubc84\uc9c4 PEEK\uc758 \uc7a0\uc7ac\ub825\uc744 \ucd5c\ub300\ud55c \ubc1c\ud718\ud558\uac8c \ud558\ub294 \ube44\ubc00\u201d\uc774\ub77c\uace0 \uc124\uba85\ud569\ub2c8\ub2e4. \uc7ac\ub8cc\ub294 \ub208\uc5d0 \ubcf4\uc774\uc9c0 \uc54a\uc9c0\ub9cc \uc2e4\uc81c\ub85c \uc874\uc7ac\ud558\ub294 \ub0b4\ubd80 \uc751\ub825\uc744 \uc9c0\ub2cc \ucc44 \ub3c4\ucc29\ud569\ub2c8\ub2e4. \uba3c\uc800 \uadf8\ub7ec\ud55c \uc751\ub825\uc744 \uc644\ud654\ud558\uc9c0 \uc54a\uc740 \ucc44 \uc751\ub825\uc774 \uc788\ub294 \uc678\uce35\uc744 \uc808\uc0ad\ud558\uba74 \uac00\uacf5 \uc911\uc5d0 \uc7ac\ub8cc\uac00 \uc774\ub3d9\ud558\uac70\ub098 \ud718\uac70\ub098 \uad6c\ubd80\ub7ec\uc9d1\ub2c8\ub2e4.<\/p>\n<hr \/>\n<h2>\ubc84\uc9c4 PEEK \ubd80\ud488\uc774 \ucc28\uc774\ub97c \ub9cc\ub4dc\ub294 \ubd84\uc57c<\/h2>\n<p>\uc0dd\uccb4 \uc801\ud569\uc131, \ub0b4\ud654\ud559\uc131, \uc5f4 \uc548\uc815\uc131, \uae30\uacc4\uc801 \uac15\ub3c4\uc758 \ub3c5\ud2b9\ud55c \uc870\ud569\uc744 \uac16\ucd98 \ubc84\uc9c4 PEEK\ub294 \uc5ec\ub7ec \uae4c\ub2e4\ub85c\uc6b4 \uc0b0\uc5c5\uc5d0\uc11c \uc120\ud0dd\ub418\ub294 \uc18c\uc7ac\uc785\ub2c8\ub2e4.<\/p>\n<h3>\uc758\ub8cc \ubc0f \ud5ec\uc2a4\ucf00\uc5b4 \uc751\uc6a9 \ubd84\uc57c<\/h3>\n<p>\ubc84\uc9c4 PEEK\uc758 \uc0dd\uccb4 \uc801\ud569\uc131\uacfc \ubc29\uc0ac\uc120 \ud22c\uacfc\uc131(X\uc120\uc5d0 \ub300\ud55c \ud22c\uba85\uc131)\uc740 \uc758\ub8cc\uae30\uae30 \uc81c\uc870\ub97c \ud601\uc2e0\ud588\uc2b5\ub2c8\ub2e4. \uc774 \uc18c\uc7ac\ub294 \ucc99\ucd94 \uc720\ud569 \ucf00\uc774\uc9c0, \ub450\uac1c\uace8 \uc784\ud50c\ub780\ud2b8, \uc218\uc220 \uae30\uad6c, \ub0b4\uc2dc\uacbd \ubd80\ud488\uc5d0 \uc0ac\uc6a9\ub429\ub2c8\ub2e4. \uc774 \uc7ac\ub8cc\ub294 \uc99d\uae30 \uc624\ud1a0\ud074\ub808\uc774\ube0c, \uac10\ub9c8\uc120 \ub610\ub294 \uc0b0\ud654\uc5d0\ud2f8\ub80c\uc744 \ud1b5\ud574 \uc5f4\ud654 \uc5c6\uc774 \ubc18\ubcf5\uc801\uc73c\ub85c \uba78\uade0\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<p>\uc758\ub8cc\uc6a9 \ub4f1\uae09 \ubc84\uc9c4 PEEK\ub294 ISO 10993 \ubc0f USP Class VI \ud45c\uc900\uc744 \ucda9\uc871\ud574\uc57c \ud569\ub2c8\ub2e4. \uc774\ub7ec\ud55c \ubd80\ud488\uc744 \uac00\uacf5\ud558\ub824\uba74 \uc7ac\ub8cc \uc21c\ub3c4\ub97c \uc720\uc9c0\ud558\ub294 \ub9e4\uc6b0 \uccad\uc815\ud55c \ud658\uacbd\uacfc \uacf5\uc815\uc774 \ud544\uc694\ud569\ub2c8\ub2e4.<\/p>\n<h3>\ud56d\uacf5\uc6b0\uc8fc \ubc0f \ubc29\uc704<\/h3>\n<p>\ud56d\uacf5\uc6b0\uc8fc \uc751\uc6a9 \ubd84\uc57c\uc5d0\uc11c \ubc84\uc9c4 PEEK\ub294 \uc784\ubb34 \ud575\uc2ec\uc801\uc774\uc9c0\ub9cc \ube44\uad6c\uc870\uc801\uc778 \ubd80\ud488\u2014\ud074\ub9bd, \uc2a4\ud398\uc774\uc11c, \uc808\uc5f0\uccb4, \uc720\uccb4 \ucee4\ub125\ud130\u2014\uc758 \uae08\uc18d\uc744 \ub300\uccb4\ud569\ub2c8\ub2e4. \uc774 \uc18c\uc7ac\ub294 \uc808\ubc18\uc758 \ubb34\uac8c\ub85c \uc54c\ub8e8\ubbf8\ub284\uc5d0 \ud544\uc801\ud558\ub294 \uac15\ub3c4 \ub300 \uc911\ub7c9 \ube44\uc728\uc744 \uc81c\uacf5\ud569\ub2c8\ub2e4. \ub09c\uc5f0\uc131(UL 94 V-0 \ub4f1\uae09)\uacfc \ub0ae\uc740 \uc5f0\uae30 \ubc29\ucd9c\ub85c \uc778\ud574 \ud56d\uacf5\uae30 \ub0b4\uc7a5\uc7ac \uc751\uc6a9 \ubd84\uc57c\uc5d0 \uc801\ud569\ud569\ub2c8\ub2e4.<\/p>\n<h3>\ubc18\ub3c4\uccb4 \ubc0f \uc804\uc790<\/h3>\n<p>\ubc84\uc9c4 PEEK\uc758 \uc804\uae30 \uc808\uc5f0 \ud2b9\uc131, \ub0b4\ud654\ud559\uc131, \uc5f4 \uc548\uc815\uc131\uc740 \ubc18\ub3c4\uccb4 \uc6e8\uc774\ud37c \uce90\ub9ac\uc5b4, \uc804\uae30 \uc808\uc5f0\uccb4, \ucee4\ub125\ud130 \ud558\uc6b0\uc9d5\uc5d0 \uc774\uc0c1\uc801\uc785\ub2c8\ub2e4. \uc774 \uc18c\uc7ac\ub294 \ud074\ub9b0\ub8f8 \ud658\uacbd\uc5d0\uc11c \ud2b9\uc131\uc744 \uc720\uc9c0\ud558\uba70 \ubc18\ub3c4\uccb4 \uc81c\uc870\uc5d0 \uc0ac\uc6a9\ub418\ub294 \uacf5\uaca9\uc801\uc778 \ud654\ud559\ubb3c\uc9c8\uc5d0 \uc800\ud56d\ud569\ub2c8\ub2e4.<\/p>\n<h3>\uc11d\uc720 \ubc0f \uac00\uc2a4<\/h3>\n<p>\ub2e4\uc6b4\ud640 \uc2dc\ucd94 \ud658\uacbd\uc740 \uadf9\ud55c\uc758 \uc628\ub3c4, \uc555\ub825, \ud654\ud559\ubb3c\uc9c8 \ub178\ucd9c\uc744 \uacac\ub514\ub294 \uc7ac\ub8cc\ub97c \uc694\uad6c\ud569\ub2c8\ub2e4. \ubc84\uc9c4 PEEK \ubd80\ud488\u2014\uc530, \ubc31\uc5c5 \ub9c1, \uc804\uae30 \ucee4\ub125\ud130\u2014\uc740 \ub2e4\ub978 \ud50c\ub77c\uc2a4\ud2f1\uc774 \uc2e4\ud328\ud558\ub294 \uacf3\uc5d0\uc11c\ub3c4 \uc548\uc815\uc801\uc73c\ub85c \uc131\ub2a5\uc744 \ubc1c\ud718\ud569\ub2c8\ub2e4.<\/p>\n<hr \/>\n<h2>\ub2ec\uc131 \uac00\ub2a5\ud55c \uacf5\ucc28 \ubc0f \ud488\uc9c8 \ud45c\uc900<\/h2>\n<p>\uc801\uc808\ud55c \uae30\uc220\uacfc \uacf5\uc815 \uc81c\uc5b4\ub97c \ud1b5\ud574 \ubc84\uc9c4 PEEK\ub294 \ub180\ub78d\ub3c4\ub85d \uc5c4\uaca9\ud55c \uacf5\ucc28\ub97c \uc720\uc9c0\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4. \ub300\ubd80\ubd84\uc758 \uc751\uc6a9 \ubd84\uc57c\uc5d0\uc11c \ud45c\uc900 \uac00\uacf5\uc740 \u00b10.05 mm(\u00b10.002\")\uc758 \uacf5\ucc28\ub97c \ub2ec\uc131\ud569\ub2c8\ub2e4. \uc81c\uc5b4\ub41c \uc870\uac74\uc5d0\uc11c \uace0\uc815\ubc00 \ubd80\ud488\uc758 \uacbd\uc6b0 \u00b10.012 mm(\u00b10.0005\")\ub9cc\ud07c \uc5c4\uaca9\ud55c \uacf5\ucc28\ub3c4 \ub2ec\uc131 \uac00\ub2a5\ud569\ub2c8\ub2e4.<\/p>\n<p>\ud45c\uba74 \uc870\ub3c4 \uc694\uad6c \uc0ac\ud56d\uc740 \uc751\uc6a9 \ubd84\uc57c\uc5d0 \ub530\ub77c \ub2e4\ub985\ub2c8\ub2e4. \uc758\ub8cc \ubc0f \ud56d\uacf5\uc6b0\uc8fc \ubd80\ud488\uc740 \uc885\uc885 0.8 \u03bcm \ubbf8\ub9cc\uc758 Ra \uac12\uc744 \uc9c0\uc815\ud569\ub2c8\ub2e4. \uc774\ub97c \ub2ec\uc131\ud558\ub824\uba74 \ub0a0\uce74\ub85c\uc6b4 \uacf5\uad6c, \uc815\ubc00 \uc815\uc0ad \ud328\uc2a4, \uc801\uc808\ud55c \uce69 \ubc30\ucd9c\uc774 \ud544\uc694\ud569\ub2c8\ub2e4.<\/p>\n<p>\ud488\uc9c8 \uac80\uc99d\uc740 \uc77c\ubc18\uc801\uc73c\ub85c \uc88c\ud45c\uce21\uc815\uae30(CMM) \uac80\uc0ac\ub97c \ud3ec\ud568\ud569\ub2c8\ub2e4. \uc8fc\uccad \ud504\ub9ac\uc2dc\uc804(Jucheng Precision)\uacfc \uac19\uc740 \ucca8\ub2e8 \uc5c5\uccb4\ub294 Zeiss CMM \uacc4\uce21\uc744 \uc0ac\uc6a9\ud558\uc5ec \ubaa8\ub4e0 \uc911\uc694 \uce58\uc218\ub97c \uac80\uc99d\ud569\ub2c8\ub2e4.<\/p>\n<hr \/>\n<h2>\ubc84\uc9c4 PEEK \uac00\uacf5\uc744 \uc804\ubb38 \uc5c5\uccb4\uc640 \ud611\ub825\ud574\uc57c \ud558\ub294 \uc774\uc720<\/h2>\n<p>\ubc84\uc9c4 PEEK \uac00\uacf5\uc740 \ud558\ub8fb\ubc24 \uc0ac\uc774\uc5d0 \ubc30\uc6b8 \uc218 \uc788\ub294 \uacf5\uc815\uc774 \uc544\ub2d9\ub2c8\ub2e4. \uc774 \uc18c\uc7ac\ub294 \ud2b9\uc815\ud55c \uc9c0\uc2dd, \uaddc\uc728 \uc788\ub294 \uacf5\uc815, \uadf8\ub9ac\uace0 \uc804\ubb38\ud654\ub41c \uc7a5\ube44\ub97c \uc694\uad6c\ud569\ub2c8\ub2e4. \ubc14\ub85c \uc774 \uc9c0\uc810\uc5d0\uc11c \uacbd\ud5d8 \ub9ce\uc740 CNC \uac00\uacf5 \uacf5\uae09\uc5c5\uccb4\uc640 \ud611\ub825\ud558\ub294 \uac83\uc774 \uc131\uacf5\uacfc \uac12\ube44\uc2fc \uc2e4\ud328\ub97c \uac00\ub974\ub294 \ucc28\uc774\ub97c \ub9cc\ub4ed\ub2c8\ub2e4.<\/p>\n<p><strong>Jucheng Precision<\/strong> \ubc84\uc9c4 PEEK CNC \uac00\uacf5 \uc11c\ube44\uc2a4\uc5d0 \ud3ed\ub113\uc740 \uc804\ubb38\uc131\uc744 \ubcf4\uc720\ud558\uace0 \uc788\uc73c\uba70, \ud45c\uc900 \ubc84\uc9c4 \uc18c\uc7ac\ubd80\ud130 \ud2b9\uc218 \uc774\uc2dd\uc6a9 \ub4f1\uae09\uc5d0 \uc774\ub974\uae30\uae4c\uc9c0 \ud504\ub9ac\ubbf8\uc5c4 PEEK \ub4f1\uae09\uc744 \uac00\uacf5\ud569\ub2c8\ub2e4. \uc774 \ud68c\uc0ac\ub294 \ub2e4\uc74c \uc778\uc99d\uc744 \ubc1b\uc740 \uace0\uc815\ubc00 \uc81c\uc870 \ud604\uc7a5\uc744 \uc6b4\uc601\ud569\ub2c8\ub2e4: <strong>AS9100<\/strong> (\ud56d\uacf5\uc6b0\uc8fc), <strong>ISO 13485<\/strong> (\uc758\ub8cc\uae30\uae30), <strong>IATF 16949<\/strong> (\uc790\ub3d9\ucc28), \ubc0f <strong>ISO 9001<\/strong> \ud488\uc9c8 \ud45c\uc900.<\/p>\n<p>\ubc84\uc9c4 PEEK \uac00\uacf5\uc5d0\uc11c \uc8fc\uccad\uc744 \ucc28\ubcc4\ud654\ud558\ub294 \uac83\uc740 \uc5f4 \uad00\ub9ac\uc5d0 \ub300\ud55c \uccb4\uacc4\uc801\uc778 \uc811\uadfc \ubc29\uc2dd\uc785\ub2c8\ub2e4. \uc774 \ud68c\uc0ac\ub294 \uc5b4\ub2d0\ub9c1\uc744 \uacfc\ud559\uc758 \uacbd\uc9c0\ub85c \ub04c\uc5b4\uc62c\ub824 \ubaa8\ub4e0 \ubd80\ud488\uc774 \uce58\uc218\uc801\uc73c\ub85c \uc548\uc815\uc801\uc774\uace0 \uad6c\uc870\uc801\uc73c\ub85c \u201c\uc8fd\uc5b4 \uc788\ub3c4\ub85d\u201d\u2014\uc989, \ud5a5\ud6c4 \ud728\uc744 \uc720\ubc1c\ud560 \uc794\ub958 \uc751\ub825\uc774 \ub0a8\uc9c0 \uc54a\ub3c4\ub85d\u2014\ubcf4\uc7a5\ud569\ub2c8\ub2e4. \uadf8\ub4e4\uc758 \uc2dc\uc124\uc5d0\ub294 \uc778\uc99d\ub41c \uae30\uc220\uc790\uac00 \uad00\ub9ac\ud558\ub294 \uc804\uc6a9 \ud074\ub9b0\ub8f8 5\ucd95 CNC \uc6cc\ud06c\uc2a4\ud14c\uc774\uc158\uc774 \uac16\ucd94\uc5b4\uc838 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<p>\uc774 \ud68c\uc0ac\uc758 \uc9c0\uc2dd \uae30\ubc18\uc5d0\ub294 PEEK \uc5b4\ub2d0\ub9c1, \uace0\uc628 \uc548\uc815\ud654, \uacf5\uad6c \uc120\ud0dd, \uadf8\ub9ac\uace0 \uc758\ub8cc \ubc0f \ud56d\uacf5\uc6b0\uc8fc \ud504\ub85c\ud1a0\ud0c0\uc785\uc744 \uc704\ud55c \uc18c\ub7c9 \uc815\ubc00 \uac00\uacf5 \ub2ec\uc131\uc5d0 \uad00\ud55c \uc0c1\uc138\ud55c \uac00\uc774\ub4dc\uac00 \ud3ec\ud568\ub418\uc5b4 \uc788\uc2b5\ub2c8\ub2e4. 150\ub300 \uc774\uc0c1\uc758 CNC \uae30\uacc4\uc640 \ucca8\ub2e8 \uacc4\uce21 \uc7a5\ube44\ub97c \uac16\ucd98 \uc8fc\uccad\uc740 \uac00\uc7a5 \uae4c\ub2e4\ub85c\uc6b4 \uc0ac\uc591\uc744 \ucda9\uc871\ud558\ub294 \ubd80\ud488\uc744 \uacf5\uae09\ud569\ub2c8\ub2e4.<\/p>\n<p>\uc124\uacc4 \uc5d4\uc9c0\ub2c8\uc5b4\uc640 \uad6c\ub9e4 \uc804\ubb38\uac00\uc5d0\uac8c \uac00\uce58 \uc81c\uc548\uc740 \uba85\ud655\ud569\ub2c8\ub2e4. \ubc84\uc9c4 PEEK\ub294 \ub108\ubb34 \ube44\uc2f8\uace0 \uc694\uad6c \uc870\uac74\uc774 \uae4c\ub2e4\ub85c\uc6cc \uc77c\ubc18 \uac00\uacf5 \uc5c5\uccb4\uc5d0 \ub9e1\uae30\uae30\uc5d0\ub294 \uc2e0\ub8b0\ud560 \uc218 \uc5c6\uc2b5\ub2c8\ub2e4. \uc18c\uc7ac\uc758 \u201c\uc131\uaca9\u201d\uc744 \uc774\ud574\ud558\uace0 \uc774\uc5d0 \ub9de\ub294 \uacf5\uc815 \uad00\ub9ac\ub97c \uac16\ucd98 \uc804\ubb38 \uc5c5\uccb4\uc640 \ud611\ub825\ud558\uba74 \uc704\ud5d8\uc744 \uc904\uc774\uace0 \ud488\uc9c8\uc744 \ud5a5\uc0c1\uc2dc\ud0a4\uba70 \uad81\uadf9\uc801\uc73c\ub85c \ucd1d\ube44\uc6a9\uc744 \ub0ae\ucd9c \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<hr \/>\n<h2>\ubc84\uc9c4 PEEK \uac00\uacf5\uc5d0 \uad00\ud55c \uc790\uc8fc \ubb3b\ub294 \uc9c8\ubb38<\/h2>\n<h3>1. \ubc84\uc9c4 PEEK\uc640 \ucda9\uc804 PEEK \ub4f1\uae09\uc758 \ucc28\uc774\uc810\uc740 \ubb34\uc5c7\uc785\ub2c8\uae4c?<\/h3>\n<p>\ubc84\uc9c4 PEEK\ub294 \uc21c\uc218\ud55c \ubbf8\ucda9\uc804 \ud3f4\ub9ac\uba38\uc785\ub2c8\ub2e4. \ubaa8\ub4e0 PEEK \ub4f1\uae09 \uc911\uc5d0\uc11c \uac00\uc7a5 \ub192\uc740 \uc778\uc131, \uc5f0\uc2e0\uc728, \ub0b4\ud654\ud559\uc131\uc744 \uc81c\uacf5\ud569\ub2c8\ub2e4. \uc720\ub9ac \ucda9\uc804 PEEK(GF30)\ub294 \uc720\ub9ac \uc12c\uc720\ub97c \ucca8\uac00\ud558\uc5ec \uac15\uc131\uacfc \ub0b4\ud06c\ub9ac\ud504\uc131\uc744 \ub192\uc774\uc9c0\ub9cc \uacf5\uad6c \ub9c8\ubaa8\uac00 \ub354 \uc2ec\ud569\ub2c8\ub2e4. \ud0c4\uc18c \ucda9\uc804 PEEK(CF30)\ub294 \uac00\uc7a5 \ub192\uc740 \uac15\ub3c4, \uac15\uc131, \ub0b4\ub9c8\ubaa8\uc131\uc744 \uc81c\uacf5\ud569\ub2c8\ub2e4. \ubc84\uc9c4 PEEK\ub294 \uc77c\ubc18\uc801\uc73c\ub85c \uac15\ud654 \ubcc0\uc885\ubcf4\ub2e4 \uac00\uacf5\uc774 \ub354 \uc27d\uace0 \uc758\ub8cc, \uc2dd\ud488 \uc811\ucd09, \uc804\uae30 \uc808\uc5f0 \uc751\uc6a9 \ubd84\uc57c\uc5d0 \uc120\ud638\ub429\ub2c8\ub2e4.<\/p>\n<h3>2. \ubc84\uc9c4 PEEK\ub97c \ud45c\uc900 CNC \uc7a5\ube44\uc5d0\uc11c \uac00\uacf5\ud560 \uc218 \uc788\uc2b5\ub2c8\uae4c?<\/h3>\n<p>\uc608, \ubc84\uc9c4 PEEK\ub294 \ud45c\uc900 \uae08\uc18d \uac00\uacf5 CNC \uc7a5\ube44\ub97c \uc0ac\uc6a9\ud558\uc5ec \uac00\uacf5\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4. \uadf8\ub7ec\ub098 \uc131\uacf5 \uc5ec\ubd80\ub294 \uc62c\ubc14\ub978 \uacf5\uad6c, \ub9e4\uac1c\ubcc0\uc218 \ubc0f \uacf5\uc815\uc744 \uc0ac\uc6a9\ud558\ub294\uc9c0\uc5d0 \ub2ec\ub824 \uc788\uc2b5\ub2c8\ub2e4. \ud45c\uc900 \uae08\uc18d \uc808\uc0ad \ub9e4\uac1c\ubcc0\uc218\ub294 \ud6a8\uacfc\uac00 \uc5c6\uc2b5\ub2c8\ub2e4. PEEK\ub294 \ud2b9\uc815 \uc18d\ub3c4, \uc774\uc1a1 \ubc0f \ub0c9\uac01 \uc804\ub7b5\uc774 \ud544\uc694\ud569\ub2c8\ub2e4. PEEK \uad00\ub828 \uacbd\ud5d8\uc774 \uc5c6\ub294 \uc5c5\uccb4\ub294 \ud728, \uc5f4\uc545\ud55c \ud45c\uba74 \uc870\ub3c4 \ubc0f \uacfc\ub3c4\ud55c \uacf5\uad6c \ub9c8\ubaa8\ub85c \uc5b4\ub824\uc6c0\uc744 \uacaa\ub294 \uacbd\uc6b0\uac00 \ub9ce\uc2b5\ub2c8\ub2e4.<\/p>\n<h3>3. \ubc84\uc9c4 PEEK\uac00 \uac00\uacf5 \uc911\uc5d0 \ud718\ub294 \uc774\uc720\ub294 \ubb34\uc5c7\uc785\ub2c8\uae4c?<\/h3>\n<p>\ud728\uc740 \uc555\ucd9c\ub41c PEEK \uc18c\uc7ac\uac00 \ub0c9\uac01 \uacfc\uc815\uc5d0\uc11c \ubc1c\uc0dd\ud55c \ub0b4\ubd80 \uc751\ub825\uc744 \ud3ec\ud568\ud558\uace0 \uc788\uae30 \ub54c\ubb38\uc5d0 \ubc1c\uc0dd\ud569\ub2c8\ub2e4. \uc18c\uc7ac\ub97c \uac00\uacf5\ud558\uc5ec \uc81c\uac70\ud558\uba74 \uc774\ub7ec\ud55c \uc751\ub825\uc774 \ubd88\uade0\uc77c\ud558\uac8c \ubc29\ucd9c\ub418\uc5b4 \ubd80\ud488\uc774 \ubcc0\ud615\ub429\ub2c8\ub2e4. \ud574\uacb0\ucc45\uc740 \uc5b4\ub2d0\ub9c1\uc785\ub2c8\ub2e4. \uac00\uacf5 \uc804\uc5d0 \uc18c\uc7ac\ub97c 200\u2013220\u00b0C\ub85c \uac00\uc5f4\ud558\uc5ec \ub0b4\ubd80 \uc751\ub825\uc744 \uc644\ud654\ud569\ub2c8\ub2e4. \ubcf5\uc7a1\ud55c \ubd80\ud488\uc758 \uacbd\uc6b0 \ub7ec\ud504 \uac00\uacf5 \ud6c4 \uc911\uac04 \uc5b4\ub2d0\ub9c1\ub3c4 \uad8c\uc7a5\ub429\ub2c8\ub2e4.<\/p>\n<h3>4. \ubc84\uc9c4 PEEK \uac00\uacf5\uc5d0 \uac00\uc7a5 \uc801\ud569\ud55c \uacf5\uad6c\ub294 \ubb34\uc5c7\uc785\ub2c8\uae4c?<\/h3>\n<p>\uc5f0\ub9c8\ub41c \ud648\uc774 \uc788\ub294 \ubbf8\uc138 \uc785\uc790 \ucd08\uacbd \uacf5\uad6c\ub294 \ubc84\uc9c4 PEEK\uc5d0 \ub300\ud574 \ub0a0\uce74\ub85c\uc6c0, \ub0a0 \uc720\uc9c0\ub825 \ubc0f \ube44\uc6a9\uc758 \ucd5c\uc801 \uc870\ud569\uc744 \uc81c\uacf5\ud569\ub2c8\ub2e4. \uc2e4\ub9ac\ucf58 \uce74\ubc14\uc774\ub4dc \uacf5\uad6c\ub3c4 \uc88b\uc740 \uc635\uc158\uc785\ub2c8\ub2e4. \uacf5\uad6c\ub294 \uc591\uc758 \uacbd\uc0ac\uac01\uacfc \ub0a0\uce74\ub85c\uc6b4 \uc808\uc0ad\ub0a0\uc744 \uac00\uc838\uc57c \ud569\ub2c8\ub2e4. \ucda9\uc804\ub41c PEEK \ub4f1\uae09\uc758 \uacbd\uc6b0 \ub2e4\uacb0\uc815 \ub2e4\uc774\uc544\ubaac\ub4dc(PCD) \ub610\ub294 \ub2e4\uc774\uc544\ubaac\ub4dc \ucf54\ud305 \uacf5\uad6c\uac00 \ud544\uc694\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<h3>5. \ubc84\uc9c4 PEEK \ubc00\ub9c1\uc5d0 \uad8c\uc7a5\ub418\ub294 \uc18d\ub3c4\uc640 \uc774\uc1a1\uc740 \ubb34\uc5c7\uc785\ub2c8\uae4c?<\/h3>\n<p>\ubc84\uc9c4 PEEK \ubc00\ub9c1\uc758 \uacbd\uc6b0 \uad8c\uc7a5 \uc808\uc0ad \uc18d\ub3c4\ub294 \ub7ec\ud504 \uac00\uacf5 \uc2dc 150\u2013300 m\/min, \uc815\uc0ad \uc2dc 200\u2013400 m\/min\uc785\ub2c8\ub2e4. \uc774\uc1a1 \uc18d\ub3c4\ub294 \uc77c\ubc18\uc801\uc73c\ub85c 0.05\u20130.15 mm\/\ub0a0\uc785\ub2c8\ub2e4. \ubbf8\ucda9\uc804 PEEK\uc758 \ucd5c\uc801 \uac12\uc740 300\u2013600 SFM(91\u2013183 m\/min)\uc73c\ub85c, \uc544\uc138\ud0c8\uc5d0 \uc0ac\uc6a9\ub418\ub294 \uc18d\ub3c4\uc758 \uc57d \ub450 \ubc30\uc785\ub2c8\ub2e4. \uc77c\ubc18 \ubc00\ub9c1\ubcf4\ub2e4 \ud074\ub77c\uc784 \ubc00\ub9c1\uc774 \uc120\ud638\ub429\ub2c8\ub2e4.<\/p>\n<h3>6. \ubc84\uc9c4 PEEK\uc5d0\ub294 \uc5b4\ub5a4 \ub0c9\uac01 \ubc29\ubc95\uc744 \uc0ac\uc6a9\ud574\uc57c \ud569\ub2c8\uae4c?<\/h3>\n<p>\uc0b0\uc5c5\uc6a9 \ub4f1\uae09 \ubc84\uc9c4 PEEK\uc758 \uacbd\uc6b0 \uc218\uc6a9\uc131 \ub610\ub294 \uacbd\uc720 \uae30\ubc18 \ub0c9\uac01\uc81c\ub97c \uc0ac\uc6a9\ud55c \ud50c\ub7ec\ub4dc \ub0c9\uac01\uc774 \uc798 \uc791\ub3d9\ud569\ub2c8\ub2e4. \uc758\ub8cc\uc6a9 \ub4f1\uae09 PEEK\uc758 \uacbd\uc6b0 \uc0dd\uccb4 \uc801\ud569\uc131\uc744 \uc720\uc9c0\ud558\uae30 \uc704\ud574 5\u20137 bar\uc758 \uc555\ucd95 \uacf5\uae30 \ub610\ub294 \ud0c8\uc774\uc628\uc218\ub97c \uc0ac\uc6a9\ud558\uc2ed\uc2dc\uc624. \uc5f4 \ucda9\uaca9\uc774 \ubbf8\uc138 \uade0\uc5f4\uc744 \uc720\ubc1c\ud560 \uc218 \uc788\uc73c\ubbc0\ub85c \ud50c\ub7ec\ub4dc \ub0c9\uac01\uc740 \uc77c\ubc18\uc801\uc73c\ub85c \uad8c\uc7a5\ub418\uc9c0 \uc54a\uc2b5\ub2c8\ub2e4. \uc8fc\uc694 \ubaa9\ud45c\ub294 \ud6a8\uc728\uc801\uc778 \uce69 \uc81c\uac70\uc785\ub2c8\ub2e4.<\/p>\n<h3>7. \ubc84\uc9c4 PEEK\ub294 \uc5b4\ub5a4 \uacf5\ucc28\ub97c \ub2ec\uc131\ud560 \uc218 \uc788\uc2b5\ub2c8\uae4c?<\/h3>\n<p>\ud45c\uc900 \uac00\uacf5\uc740 \ub300\ubd80\ubd84\uc758 \uc751\uc6a9 \ubd84\uc57c\uc5d0\uc11c \u00b10.05 mm(\u00b10.002\u2033)\uc758 \uacf5\ucc28\ub97c \ub2ec\uc131\ud569\ub2c8\ub2e4. \uc801\uc808\ud55c \uae30\uc220\uacfc \ud1b5\uc81c\ub41c \uc870\uac74\uc5d0\uc11c\ub294 \u00b10.012 mm(\u00b10.0005\u2033)\ub9cc\ud07c \uc5c4\uaca9\ud55c \uacf5\ucc28\ub3c4 \uac00\ub2a5\ud569\ub2c8\ub2e4. \uc774\ub7ec\ud55c \uacf5\ucc28\ub97c \ub2ec\uc131\ud558\ub824\uba74 \uc5b4\ub2d0\ub9c1, \ub0a0\uce74\ub85c\uc6b4 \uacf5\uad6c, \uc801\uc808\ud55c \ub0c9\uac01 \ubc0f \uc548\uc815\uc801\uc778 \ud658\uacbd \uc870\uac74\uc774 \ud544\uc694\ud569\ub2c8\ub2e4.<\/p>\n<h3>8. \ubc84\uc9c4 PEEK\ub294 \uc758\ub8cc\uc6a9 \uc784\ud50c\ub780\ud2b8\uc5d0 \uc801\ud569\ud569\ub2c8\uae4c?<\/h3>\n<p>\uc608, \ud2b9\uc815 \ubc84\uc9c4 PEEK \ub4f1\uae09\uc740 \uc0dd\uccb4 \uc801\ud569\uc131\uc5d0 \ub300\ud55c ISO 10993 \ubc0f USP Class VI \ud45c\uc900\uc744 \ucda9\uc871\ud569\ub2c8\ub2e4. \uc758\ub8cc\uc6a9 \ub4f1\uae09 \ubc84\uc9c4 PEEK\ub294 \ucc99\ucd94 \uc720\ud569 \ucf00\uc774\uc9c0, \ub450\uac1c\uace8 \uc784\ud50c\ub780\ud2b8 \ubc0f \uc218\uc220 \uae30\uad6c\uc5d0 \uc0ac\uc6a9\ub429\ub2c8\ub2e4. \ubc29\uc0ac\uc120 \ud22c\uacfc\uc131(X\uc120\uc5d0 \ud22c\uba85)\uc774 \uc788\uc5b4 \uc601\uc0c1 \ucd2c\uc601 \uc2dc \ubf08\ub97c \ubcfc \uc218 \uc788\uc2b5\ub2c8\ub2e4. \uc758\ub8cc\uc6a9 \ub4f1\uae09 PEEK \uac00\uacf5\uc5d0\ub294 \uccad\uc815 \ud658\uacbd\uacfc \uc18c\uc7ac \uc21c\ub3c4\ub97c \uc720\uc9c0\ud558\ub294 \uacf5\uc815\uc774 \ud544\uc694\ud569\ub2c8\ub2e4.<\/p>\n<h3>9. \ubc84\uc9c4 PEEK\ub294 \uc65c \uadf8\ub807\uac8c \ube44\uc309\ub2c8\uae4c?<\/h3>\n<p>\ubc84\uc9c4 PEEK\ub294 \ubcf5\uc7a1\ud55c \uc911\ud569 \uacf5\uc815\uc744 \ud1b5\ud574 \uc81c\uc870\ub418\ub294 \uace0\uc131\ub2a5 \uc5d4\uc9c0\ub2c8\uc5b4\ub9c1 \uc5f4\uac00\uc18c\uc131 \uc218\uc9c0\uc785\ub2c8\ub2e4. \uc9c1\uacbd 50mm, \uae38\uc774 300mm\uc758 \ubd09\uc7ac \uac00\uaca9\uc740 $150\u2013300\uc785\ub2c8\ub2e4. 260\u00b0C\uae4c\uc9c0\uc758 \uc5f4 \uc548\uc815\uc131, \ub0b4\ud654\ud559\uc131, \uc0dd\uccb4 \uc801\ud569\uc131, \uae30\uacc4\uc801 \uac15\ub3c4 \ub4f1 \uc774 \uc18c\uc7ac\uc758 \ub6f0\uc5b4\ub09c \ud2b9\uc131\uc740 \uc784\ubb34 \uc218\ud589\uc5d0 \uc911\uc694\ud55c \uc560\ud50c\ub9ac\ucf00\uc774\uc158\uc5d0\uc11c\uc758 \ube44\uc6a9\uc744 \uc815\ub2f9\ud654\ud569\ub2c8\ub2e4. \uac00\uacf5 \uc911 \ubd80\ud488\uc744 \ud3d0\uae30\ud558\uba74 \uc0c1\ub2f9\ud55c \ube44\uc6a9\uc774 \ucd94\uac00\ub418\ubbc0\ub85c \uc801\uc808\ud55c \uacf5\uc815 \uad00\ub9ac\uac00 \ud544\uc218\uc801\uc785\ub2c8\ub2e4.<\/p>\n<h3>10. \ubd80\ud488 \uc81c\uc870\uc5d0\uc11c \ubc84\uc9c4 PEEK\ub294 \uae08\uc18d\uacfc \uc5b4\ub5bb\uac8c \ube44\uad50\ub429\ub2c8\uae4c?<\/h3>\n<p>\ubc84\uc9c4 PEEK\ub294 \uc77c\ubd80 \uc54c\ub8e8\ubbf8\ub284 \ud569\uae08\uc5d0 \ud544\uc801\ud558\ub294 \uac15\ub3c4 \ub300 \uc911\ub7c9 \ube44\uc728\uc744 50% \ub354 \uac00\ubcbc\uc6b4 \ubb34\uac8c\ub85c \uc81c\uacf5\ud569\ub2c8\ub2e4. \uae08\uc18d\uc774 \ub530\ub77c\uc62c \uc218 \uc5c6\ub294 \ub0b4\ud654\ud559\uc131\uc744 \uc81c\uacf5\ud558\uace0, \ubd80\uc2dd\uc744 \ubc29\uc9c0\ud558\uba70, \uc758\ub8cc \uc601\uc0c1 \ucd2c\uc601\uc744 \uc704\ud55c \ubc29\uc0ac\uc120 \ud22c\uacfc\uc131\uc744 \uac00\uc9d1\ub2c8\ub2e4. PEEK \ubd80\ud488\uc740 \uac12\ube44\uc2fc \uae08\ud615 \uacf5\uad6c \uc5c6\uc774\ub3c4 \uc5c4\uaca9\ud55c \uacf5\ucc28\ub85c \uac00\uacf5\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4. \uc911\ub7c9 \uac10\uc18c, \ub0b4\ud654\ud559\uc131 \ub610\ub294 \uc0dd\uccb4 \uc801\ud569\uc131\uc774 \uc694\uad6c\ub418\ub294 \uc560\ud50c\ub9ac\ucf00\uc774\uc158\uc5d0\uc11c \ubc84\uc9c4 PEEK\ub294 \uc885\uc885 \uae08\uc18d \ub300\uc548\ubcf4\ub2e4 \uc6b0\uc218\ud55c \uc131\ub2a5\uc744 \ubc1c\ud718\ud569\ub2c8\ub2e4.<\/p>\n<hr \/>\n<h2>\ubaa8\ub4e0 \uac83\uc744 \uc885\ud569\ud558\uae30: \ubc84\uc9c4 PEEK \uac00\uacf5 \uc2e4\ud589 \uacc4\ud68d<\/h2>\n<p>\uc131\uacf5\uc801\uc778 \ubc84\uc9c4 PEEK \uac00\uacf5\uc740 \uaddc\uc728 \uc788\ub294 \uacf5\uc815\uc744 \ub530\ub974\ub294 \ub370 \ub2ec\ub824 \uc788\uc2b5\ub2c8\ub2e4. \ub2e4\uc74c\uc740 \uc5c5\uacc4 \ubaa8\ubc94 \uc0ac\ub840\uc640 \ud604\uc7a5 \uacbd\ud5d8\uc744 \ubc14\ud0d5\uc73c\ub85c \ud55c \uc2e4\uc6a9\uc801\uc778 \uccb4\ud06c\ub9ac\uc2a4\ud2b8\uc785\ub2c8\ub2e4:<\/p>\n<ol>\n<li><strong>\uc5b4\ub2d0\ub9c1\ub41c \uc18c\uc7ac\ub85c \uc2dc\uc791\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\ud1b5\uc81c\ub41c \uc5b4\ub2d0\ub9c1\uc744 \ud1b5\ud574 \ub0b4\ubd80 \uc751\ub825\uc744 \uba3c\uc800 \uc644\ud654\ud558\uc9c0 \uc54a\uace0 \uc6d0\ub8cc PEEK\ub97c \uc808\ub300 \uac00\uacf5\ud558\uc9c0 \ub9c8\uc2ed\uc2dc\uc624<\/li>\n<li><strong>\uc62c\ubc14\ub978 \uacf5\uad6c\ub97c \uc120\ud0dd\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\ubb34\ucda9\uc804 PEEK\uc5d0\ub294 \uc5f0\ub9c8\ub41c \ud648\uc774 \uc788\ub294 \ubbf8\ub9bd \uce74\ubc14\uc774\ub4dc \uc0ac\uc6a9<\/li>\n<li><strong>\uc18d\ub3c4\uc640 \uc774\uc1a1\uc744 \ucd5c\uc801\ud654\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\ubc00\ub9c1\uc758 \uacbd\uc6b0 300\u2013600 SFM, \uc801\uc808\ud55c \uc774\uc1a1 \uc18d\ub3c4 \uc801\uc6a9<\/li>\n<li><strong>\ud074\ub77c\uc784 \ubc00\ub9c1\uc744 \uc0ac\uc6a9\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\uc808\uc0ad\ub825\uacfc \uc5f4 \ubc1c\uc0dd\uc744 \uac10\uc18c\uc2dc\ud0b5\ub2c8\ub2e4<\/li>\n<li><strong>\uc5f4\uc744 \uc801\uadf9\uc801\uc73c\ub85c \uad00\ub9ac\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\uc801\uc808\ud55c \ub0c9\uac01\uacfc \uce69 \ubc30\ucd9c\uc740 \ud611\uc0c1 \ubd88\uac00\uc785\ub2c8\ub2e4<\/li>\n<li><strong>\uc595\uc740 \uc808\uc0ad\uc744 \uc801\uc6a9\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\ud669\uc0ad \uc2dc 0.5\u20131.0mm, \uc815\uc0ad \uc2dc 0.1\u20130.3mm<\/li>\n<li><strong>\uacf5\uad6c \uc815\uccb4\ub97c \ud53c\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\uacf5\uad6c\ub97c \uacc4\uc18d \uc6c0\uc9c1\uc5ec \uad6d\ubd80 \uac00\uc5f4\uc744 \ubc29\uc9c0\ud558\uc2ed\uc2dc\uc624<\/li>\n<li><strong>\uc911\uac04 \uc5b4\ub2d0\ub9c1\uc744 \uace0\ub824\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\ub300\ub7c9 \uc7ac\ub8cc \uc81c\uac70\uac00 \ud544\uc694\ud55c \ubcf5\uc7a1\ud55c \ubd80\ud488\uc758 \uacbd\uc6b0<\/li>\n<li><strong>\uc815\uae30\uc801\uc73c\ub85c \uac80\uc0ac\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014\uac00\uacf5 \uc804 \uacfc\uc815\uc5d0 \uac78\uccd0 \uacf5\uad6c \ub0a0\uacfc \ubd80\ud488 \uce58\uc218\ub97c \ud655\uc778\ud558\uc2ed\uc2dc\uc624<\/li>\n<li><strong>\uc804\ubb38\uac00\uc640 \ud611\ub825\ud558\uc2ed\uc2dc\uc624<\/strong>\u2014PEEK\uc758 \uace0\uc720\ud55c \uc694\uad6c \uc0ac\ud56d\uc744 \uc774\ud574\ud558\ub294 \uac00\uacf5\uc5c5\uccb4\uc640 \ud611\ub825\ud558\uc2ed\uc2dc\uc624<\/li>\n<\/ol>\n<p>\ubc84\uc9c4 PEEK \uac00\uacf5\uc740 \uc5b4\ub835\uc9c0\ub9cc \ubd88\uac00\uc0ac\uc758\ud55c \uac83\uc740 \uc544\ub2d9\ub2c8\ub2e4. \uc18c\uc7ac\uc758 \ud2b9\uc131\uc744 \uc774\ud574\ud558\uace0 \ud55c\uacc4\ub97c \uc874\uc911\ud558\uba74 \uc608\uce21 \uac00\ub2a5\ud558\uac8c \uac70\ub3d9\ud569\ub2c8\ub2e4. \uc62c\ubc14\ub978 \uc9c0\uc2dd, \uacf5\uad6c, \uacf5\uc815\uc744 \uac16\ucd94\uba74 \uac00\uc7a5 \uae4c\ub2e4\ub85c\uc6b4 \uc751\uc6a9 \uc694\uad6c \uc0ac\ud56d\uc744 \ucda9\uc871\ud558\ub294 \uace0\ud488\uc9c8 \ubc84\uc9c4 PEEK \ubd80\ud488\uc744 \uc77c\uad00\ub418\uac8c \uc0dd\uc0b0\ud560 \uc218 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<p>\uc758\ub8cc\uc6a9 \uc784\ud50c\ub780\ud2b8, \ud56d\uacf5\uc6b0\uc8fc \ubd80\ud488 \ub610\ub294 \ubc18\ub3c4\uccb4 \uc7a5\ube44\ub97c \uc124\uacc4\ud558\ub4e0, \uc131\uacf5\uc758 \uc5f4\uc1e0\ub294 \ubc84\uc9c4 PEEK\ub97c \ub9c8\ub545\ud788 \ubc1b\uc544\uc57c \ud560 \uc874\uc911\uc73c\ub85c \ub300\ud558\uace0, \uc774 \ud2b9\ubcc4\ud55c \uc18c\uc7ac\ub97c \ub2e4\ub8e8\ub294 \uae30\uc220\uacfc \uacfc\ud559\uc744 \ud130\ub4dd\ud55c \uac00\uacf5 \uc804\ubb38\uac00\uc640 \ud611\ub825\ud558\ub294 \ub370 \uc788\uc2b5\ub2c8\ub2e4.<\/p>\n<hr \/>\n<p><strong>\ubc84\uc9c4 PEEK \uac00\uacf5 \ud504\ub85c\uc81d\ud2b8\uc5d0 \ub300\ud574 \ub17c\uc758\ud560 \uc900\ube44\uac00 \ub418\uc168\uc2b5\ub2c8\uae4c?<\/strong> \uc8fc\uccad \ud504\ub9ac\uc2dc\uc804\uc758 PEEK \uac00\uacf5 \uc804\ubb38\uac00 \ud300\uc774 \uadc0\ud558\uc758 \uc124\uacc4\ub97c \uac80\ud1a0\ud558\uace0, \ucd5c\uc801\uc758 \ub4f1\uae09\uacfc \uacf5\uc815\uc744 \ucd94\ucc9c\ud558\uba70, \uadc0\ud558\uc758 \uc815\ud655\ud55c \uc0ac\uc591\uc744 \ucda9\uc871\ud558\ub294 \uc815\ubc00 \ubd80\ud488\uc744 \uc81c\uacf5\ud560 \uc900\ube44\uac00 \ub418\uc5b4 \uc788\uc2b5\ub2c8\ub2e4. <a href=\"https:\/\/www.jccncmachining.com\/ko\/\" rel=\"nofollow\">\uc9c0\uae08 \uc8fc\uccad \ud504\ub9ac\uc2dc\uc804\uc5d0 \ubb38\uc758\ud558\uc2ed\uc2dc\uc624<\/a> \ubc84\uc9c4 PEEK\ub97c \ucc98\uc74c\ubd80\ud130 \uc81c\ub300\ub85c \uac00\uacf5\ud558\ub294 \ub370 \ud544\uc694\ud55c \ubaa8\ub4e0 \uac83\uc744 \uc774\ud574\ud558\ub294 \ud30c\ud2b8\ub108\uc640 \ud568\uaed8 \ud504\ub85c\uc81d\ud2b8\ub97c \uc2dc\uc791\ud558\uc2ed\uc2dc\uc624.<\/p>","protected":false},"excerpt":{"rendered":"<p>You have spent weeks designing a critical component\u2014a surgical instrument handle, an aerospace sensor housing, or a semiconductor wafer carrier. The material specification calls for Virgin PEEK, and you have sourced the expensive raw stock. Then the CNC machining begins, and within hours, the part warps, the surface finish looks like sandpaper, and the tool [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":1898,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1],"tags":[],"class_list":["post-1896","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-blog"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/posts\/1896","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/comments?post=1896"}],"version-history":[{"count":2,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/posts\/1896\/revisions"}],"predecessor-version":[{"id":1899,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/posts\/1896\/revisions\/1899"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/media\/1898"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/media?parent=1896"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/categories?post=1896"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/tags?post=1896"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}