{"id":795,"date":"2026-03-12T09:40:01","date_gmt":"2026-03-12T01:40:01","guid":{"rendered":"https:\/\/www.jccncmachining.com\/?post_type=material_model&#038;p=795"},"modified":"2026-03-12T09:40:01","modified_gmt":"2026-03-12T01:40:01","slug":"virgin-peek-unfilled","status":"publish","type":"material_model","link":"https:\/\/www.jccncmachining.com\/ko\/materials\/peek\/virgin-peek-unfilled\/","title":{"rendered":"\ubc84\uc9c4 PEEK (\ubb34\ucda9\uc804)"},"content":{"rendered":"<p><!-- Section: Machining Capabilities for Virgin PEEK --><\/p>\n<div class=\"machining-capabilities\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Virgin PEEK Machining Capabilities<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 25%;\">\uc5ed\ub7c9<\/th>\n<th style=\"text-align: left; width: 45%;\">\uae30\uc220 \uc124\uba85<\/th>\n<th style=\"text-align: left; width: 30%;\">Jucheng\uc758 \uac15\uc810<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\ubb34\uc751\ub825 \uac00\uacf5<\/strong><\/td>\n<td>Implementing in-process annealing cycles to relieve internal stresses caused by material removal.<\/td>\n<td>Prevents Virgin PEEK parts from warping or dimensional shifting over time, ensuring long-term precision for medical implants.<\/td>\n<\/tr>\n<tr>\n<td><strong>High-Precision Micro-Milling<\/strong><\/td>\n<td>Milling tiny, intricate features such as 0.3mm holes and micro-fluidic channels.<\/td>\n<td>Our high-speed 5-axis machines achieve burr-free edges on delicate PEEK components, eliminating the need for manual deburring.<\/td>\n<\/tr>\n<tr>\n<td><strong>\uc2a4\uc704\uc2a4\uc2dd \uc120\ubc18 \uac00\uacf5<\/strong><\/td>\n<td>Turning small-diameter dental implants and bone screws with high-precision thread whirling.<\/td>\n<td>We hold ISO 13485 certification, guaranteeing contamination-free production and full traceability for all medical-grade PEEK parts.<\/td>\n<\/tr>\n<tr>\n<td><strong>Surface Smoothing<\/strong><\/td>\n<td>Achieving Ra 0.4\u03bcm surface finishes through optimized tool paths and fine-grain carbide tooling.<\/td>\n<td>Critical for sealing surfaces in analytical instruments and smooth contact faces in orthopedic devices.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Fabrication Guidelines --><\/p>\n<div class=\"fabrication-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Fabrication Guidelines for Virgin PEEK<\/h3>\n<p><strong>Thermal Management:<\/strong><br \/>\nPEEK has low thermal conductivity. Heat generated during cutting stays in the part. <strong>\ud301:<\/strong> We use sharp tools and high-flow clean coolant (or air blast) to prevent the plastic from softening or expanding during the cut.<\/p>\n<p><strong>Annealing Requirements:<\/strong><br \/>\nTo achieve tight tolerances, we recommend rough machining, followed by a secondary annealing cycle, and then final finishing. <strong>\ud301:<\/strong> This is essential for large PEEK parts to ensure they remain dimensionally stable throughout their service life.<\/p>\n<p><strong>\uacf5\uad6c \uc120\ud0dd:<\/strong><br \/>\nVirgin PEEK is not as abrasive as filled grades, but it is hard. <strong>\ud301:<\/strong> We use polished, high-rake carbide tools to slice the material cleanly, preventing the &#8220;smearing&#8221; effect that ruins surface quality.<\/p>\n<p><strong>\ud074\ub7a8\ud551 \uc804\ub7b5:<\/strong><br \/>\nWhile hard, PEEK is still a plastic. <strong>\ud301:<\/strong> We use vacuum tables or soft-jaws with regulated pressure to hold delicate parts securely without leaving clamp marks or distorting the geometry.<\/p>\n<\/div>\n<p><!-- Section: Application Scenarios --><\/p>\n<div class=\"application-scenarios\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\uc8fc\uc694 \uc751\uc6a9 \ubd84\uc57c<\/h3>\n<p><strong>\uc758\ub8cc\uc6a9 \uc784\ud50c\ub780\ud2b8 (ISO 13485)<\/strong><br \/>\nSpinal cages, suture anchors, and dental implants. Virgin PEEK is biocompatible, radiolucent, and has a bone-like modulus.<\/p>\n<p><strong>\ud56d\uacf5\uc6b0\uc8fc \ubc0f \ud56d\uacf5<\/strong><br \/>\nConnectors, bushings, and manifolds where weight reduction and high-temperature resistance (up to 250\u00b0C) are required.<\/p>\n<p><strong>Analytical Instrumentation<\/strong><br \/>\nFluidic manifolds, rotor valves, and HPLC components requiring extreme chemical resistance to solvents and acids.<\/p>\n<p><strong>Semiconductor Equipment<\/strong><br \/>\nWafer handling tools and vacuum wand tips that require high purity, low outgassing, and excellent dielectric properties.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Virgin PEEK Machining Capabilities Capability Technical Description Jucheng Advantage Stress-Free Machining Implementing in-process annealing cycles to relieve internal stresses caused by material removal. Prevents Virgin PEEK parts from warping or dimensional shifting over time, ensuring long-term precision for medical implants. High-Precision Micro-Milling Milling tiny, intricate features such as 0.3mm holes and micro-fluidic channels. Our high-speed [&hellip;]<\/p>\n","protected":false},"featured_media":796,"template":"","meta":[],"class_list":["post-795","material_model","type-material_model","status-publish","has-post-thumbnail","hentry"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/material_model\/795","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/material_model"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/types\/material_model"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/media\/796"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/media?parent=795"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}