{"id":641,"date":"2026-02-26T06:50:45","date_gmt":"2026-02-26T06:50:45","guid":{"rendered":"https:\/\/www.jccncmachining.com\/material\/\/"},"modified":"2026-02-26T06:50:45","modified_gmt":"2026-02-26T06:50:45","slug":"1018-%ea%b0%95","status":"publish","type":"material_model","link":"https:\/\/www.jccncmachining.com\/ko\/%ec%9e%ac%eb%a3%8c\/%ea%b0%95%ec%b2%a0\/1018-%ea%b0%95\/","title":{"rendered":"1018 \uac15"},"content":{"rendered":"<p><!-- Section: Machining Capabilities for 1018 Steel --><\/p>\n<div class=\"machining-capabilities\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">1018 \uac15 \uac00\uacf5 \uc5ed\ub7c9<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 25%;\">\uc5ed\ub7c9<\/th>\n<th style=\"text-align: left; width: 45%;\">\uae30\uc220 \uc124\uba85<\/th>\n<th style=\"text-align: left; width: 30%;\">Jucheng\uc758 \uac15\uc810<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\ub300\ub7c9 \ubc00\ub9c1<\/strong><\/td>\n<td>1018\uc740 \ube44\uc6a9 \ud6a8\uc728\uc801\uc778 \uc18c\uc7ac\uc785\ub2c8\ub2e4. \ub300\ud615 \uad6c\uc870\ubb3c \ubc30\uce58 \uc0dd\uc0b0\uc744 \uc704\ud574 \uace0\ud6a8\uc728 \uacf5\uad6c \uacbd\ub85c\ub97c \ud65c\uc6a9\ud558\uc5ec \uc2e0\uc18d\ud558\uac8c \uc18c\uc7ac\ub97c \uc81c\uac70\ud569\ub2c8\ub2e4.<\/td>\n<td>\ucd5c\uc801\ud654\ub41c \ud669\uc0ad \uc0ac\uc774\ud074 \ub355\ubd84\uc5d0 \ubc94\uc6a9 \uac15 \ube0c\ub798\ud0b7 \ubc0f \uc7a5\ucc29 \ud50c\ub808\uc774\ud2b8\uc5d0 \ub300\ud574 \ubd80\ud488\ub2f9 \ucd5c\uc800 \ube44\uc6a9\uc744 \uc81c\uacf5\ud569\ub2c8\ub2e4.<\/td>\n<\/tr>\n<tr>\n<td><strong>\uc6a9\uc811 \ubc0f \uc81c\uc791<\/strong><\/td>\n<td>1018\uc740 \uac00\uc7a5 \uc6a9\uc811\uc131\uc774 \ub6f0\uc5b4\ub09c \uac15\uc785\ub2c8\ub2e4. \ub2f9\uc0ac\ub294 \uc774\ud6c4 \ub354 \ud070 \ud504\ub808\uc784\uc774\ub098 \uc5b4\uc148\ube14\ub9ac\uc5d0 \uc6a9\uc811\ub418\ub294 \ubd80\ud488\uc744 \uac00\uacf5\ud569\ub2c8\ub2e4.<\/td>\n<td>\ub2f9\uc0ac\ub294 \uc6d0\uc2a4\ud1b1 \uc11c\ube44\uc2a4\ub97c \uc81c\uacf5\ud569\ub2c8\ub2e4: CNC \uac00\uacf5 \ud6c4 \uc778\uc99d\ub41c MIG\/TIG \uc6a9\uc811\uc73c\ub85c \ubcf5\uc7a1\ud55c \uc100\uc2dc\ub97c \uc81c\uc791\ud569\ub2c8\ub2e4.<\/td>\n<\/tr>\n<tr>\n<td><strong>\ud3c9\uba74 \uc5f0\uc0ad<\/strong><\/td>\n<td>1018\uc740 \ub192\uc740 \uc790\uae30 \ud22c\uc790\uc728 \ub355\ubd84\uc5d0 \ud3c9\ud589\ud55c \ud3c9\uba74 \uc5f0\uc0ad\uc744 \uc704\ud574 \uc790\uae30 \ucc99\uc5d0 \uace0\uc815\ud558\uae30 \uc27d\uc2b5\ub2c8\ub2e4.<\/td>\n<td>\ub2f9\uc0ac\ub294 \uacf5\uad6c\uac15\ubcf4\ub2e4 \ub0ae\uc740 \ube44\uc6a9\uc73c\ub85c \uc6b0\uc218\ud55c \ud3c9\ud0c4\ub3c4\ub97c \uac00\uc9c4 \ube14\ub79c\ucc28\ub4dc \uc5f0\uc0ad(Blanchard-ground) \ubca0\uc774\uc2a4 \ud50c\ub808\uc774\ud2b8\uc640 \uace0\uc815\uad6c \ud14c\uc774\ube14\uc744 \uc0dd\uc0b0\ud569\ub2c8\ub2e4.<\/td>\n<\/tr>\n<tr>\n<td><strong>\uce68\ud0c4 \uacbd\ud654<\/strong><\/td>\n<td>\ud45c\uba74\uc744 \uce68\ud0c4\uc2dc\ucf1c \ub2e8\ub2e8\ud558\uace0 \ub0b4\ub9c8\ubaa8\uc131\uc774 \uc6b0\uc218\ud55c \u201c\ucf00\uc774\uc2a4\u201d\ub97c \ud615\uc131\ud558\uba74\uc11c\ub3c4 \uc778\uc131\uc774 \uac15\ud558\uace0 \uc5f0\uc131 \uc788\ub294 \ucf54\uc5b4\ub97c \uc720\uc9c0\ud569\ub2c8\ub2e4.<\/td>\n<td>\ud558\uc911\uc744 \ubc1b\uc544\ub3c4 \ubd80\ub7ec\uc9c0\uc9c0 \uc54a\uace0 \ud45c\uba74 \ub9c8\ubaa8\uc5d0 \uacac\ub38c\uc57c \ud558\ub294 \ub0b4\uad6c\uc131 \uc788\ub294 \ud540, \ubd80\uc2f1, \ucea0 \uc81c\uc870\uc5d0 \uc774\uc0c1\uc801\uc785\ub2c8\ub2e4.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Fabrication Guidelines --><\/p>\n<div class=\"fabrication-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">1018 \uac15\uc758 \uc81c\uc791 \uac00\uc774\ub4dc\ub77c\uc778<\/h3>\n<p><strong>\uce69 \uc81c\uc5b4:<\/strong><br \/>\n\uc800\ud0c4\uc18c\uac15\uc740 \ubb34\ub974\uace0 \u201c\ub048\uc801\uac70\ub9ac\ub294\u201d \ud2b9\uc131\uc774 \uc788\uc2b5\ub2c8\ub2e4. \uae38\uace0 \uc2e4\ucc98\ub7fc \ub298\uc5b4\ub098\ub294 \uce69\uc774 \ubc1c\uc0dd\ud558\uc5ec \uacf5\uad6c\uc5d0 \uac10\uae30\ub294 \uacbd\ud5a5\uc774 \uc788\uc2b5\ub2c8\ub2e4. <strong>\ud301:<\/strong> \uce69 \ube0c\ub808\uc774\ud0b9 \uc778\uc11c\ud2b8\uc640 \uace0\uc555 \uc808\uc0ad\uc720\ub97c \uc0ac\uc6a9\ud558\uc5ec \uce69 \ubc30\ucd9c\uc744 \uad00\ub9ac\ud569\ub2c8\ub2e4.<\/p>\n<p><strong>\ub179 \ubc29\uc9c0:<\/strong><br \/>\n1018\uc740 \ub0b4\uc2dd\uc131\uc774 \uc804\ud600 \uc5c6\uc2b5\ub2c8\ub2e4. \uc2b5\uae30\uc5d0 \ub178\ucd9c\ub418\uba74 \uc989\uc2dc \ub179\uc774 \uc2ac\uac8c \ub429\ub2c8\ub2e4. <strong>\ud301:<\/strong> \uac00\uacf5 \uc9c1\ud6c4 \ubd80\ud488\uc5d0 \ubc18\ub4dc\uc2dc \uc624\uc77c\uc744 \ubc14\ub974\uac70\ub098, \ud751\uc0c9 \uc0b0\ud654 \ud53c\ub9c9 \ucc98\ub9ac, \uc544\uc5f0 \ub3c4\uae08, \ub610\ub294 \ub3c4\uc7a5\uc744 \ud574\uc57c \ud569\ub2c8\ub2e4.<\/p>\n<p><strong>\uc644\uc804 \uacbd\ud654 \ubd88\uac00:<\/strong><br \/>\n1018\uc740 4140\ucc98\ub7fc \uc804\uccb4\ub97c \uacbd\ud654\uc2dc\ud0a4\ub294 \uc5f4\ucc98\ub9ac\ub97c \ud560 \uc218 \uc5c6\uc2b5\ub2c8\ub2e4. \uc624\uc9c1 <strong>\uce68\ud0c4 \uacbd\ud654<\/strong> (\ud45c\uba74 \uacbd\ud654)\ub9cc \uac00\ub2a5\ud569\ub2c8\ub2e4. \uc774 \ud569\uae08\uc5d0\ub294 \u201c\uc644\uc804 \uacbd\ud654\u201d\ub97c \uc9c0\uc815\ud558\uc9c0 \ub9c8\uc2ed\uc2dc\uc624.<\/p>\n<\/div>\n<p><!-- Section: Application Scenarios --><\/p>\n<div class=\"application-scenarios\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\uc8fc\uc694 \uc751\uc6a9 \ubd84\uc57c<\/h3>\n<p><strong>\uae30\uacc4 \uace0\uc815\uad6c<\/strong><br \/>\n\uac00\uacf5 \uc911 \ub2e4\ub978 \ubd80\ud488\uc744 \uace0\uc815\ud558\ub294 \ub370 \uc0ac\uc6a9\ub418\ub294 \ubca0\uc774\uc2a4 \ud50c\ub808\uc774\ud2b8, \ud074\ub7a8\ud504 \ubc0f \ube14\ub85d. \uc800\ube44\uc6a9\uc774\uba70 \uc548\uc815\uc131\uc774 \ub192\uc2b5\ub2c8\ub2e4.<\/p>\n<p><strong>\uad6c\uc870\uc6a9 \ube0c\ub798\ud0b7<\/strong><br \/>\n\uc6a9\uc811\uc131\uacfc \uc778\uc131\uc774 \uc911\uc694\ud55c \uc5d4\uc9c4, \ubaa8\ud130 \ubc0f \uc911\uc7a5\ube44\uc6a9 \uc7a5\ucc29 \ud558\ub4dc\uc6e8\uc5b4.<\/p>\n<p><strong>\ud540 \ubc0f \ubd80\uc2f1<\/strong><br \/>\n\uce68\ud0c4 \uacbd\ud654\ub41c 1018\uc740 \ub18d\uc5c5 \ubc0f \uac74\uc124 \uc7a5\ube44\uc758 \ub9c8\ubaa8 \ubd80\ud488\uc5d0 \ub300\ud55c \ud45c\uc900\uc785\ub2c8\ub2e4.<\/p>\n<p><strong>\uc18c\ube44\uc7ac<\/strong><br \/>\n\uac00\uad6c \ud504\ub808\uc784\uc774\ub098 \uc6b4\ub3d9 \uae30\uad6c\uc640 \uac19\uc774 \ubd84\uccb4 \ub3c4\uc7a5 \ub610\ub294 \ub3c4\uc7a5 \ucc98\ub9ac\ub420 \ub2e8\uc21c\ud55c \ubbf8\uad00\uc6a9 \ubd80\ud488.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>1018 Steel Machining Capabilities Capability Technical Description Jucheng Advantage High-Volume Milling 1018 is a cost-effective material. We utilize high-efficiency tool paths to remove material quickly for large structural batches. We offer the lowest cost-per-part for general purpose steel brackets and mounting plates due to our optimized roughing cycles. Welding &amp; Fabrication 1018 is the most [&hellip;]<\/p>\n","protected":false},"featured_media":642,"template":"","meta":[],"class_list":["post-641","material_model","type-material_model","status-publish","has-post-thumbnail","hentry"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/material_model\/641","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/material_model"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/types\/material_model"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/media\/642"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/ko\/wp-json\/wp\/v2\/media?parent=641"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}