{"id":421,"date":"2026-01-30T02:23:09","date_gmt":"2026-01-30T02:23:09","guid":{"rendered":"https:\/\/www.jccncmachining.com\/?post_type=process&#038;p=421"},"modified":"2026-11-05T13:11:32","modified_gmt":"2026-11-05T05:11:32","slug":"%e5%86%86%e7%ad%92%e7%a0%94%e5%89%8a","status":"publish","type":"process","link":"https:\/\/www.jccncmachining.com\/ja\/%e6%a9%9f%e8%83%bd\/%e5%86%86%e7%ad%92%e7%a0%94%e5%89%8a\/","title":{"rendered":"\u5186\u7b52\u7814\u524a\uff08\u5916\u5f84\u7814\u524a\uff09"},"content":{"rendered":"<p><!-- Section 3: Introduction & Capabilities --><\/p>\n<div class=\"process-introduction\"><\/div>\n<div class=\"key-specifications\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\u4e3b\u306a\u4ed5\u69d8<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left;\">\u4ed5\u69d8<\/th>\n<th style=\"text-align: left;\">\u6280\u8853\u7bc4\u56f2<\/th>\n<th style=\"text-align: left;\">\u5099\u8003<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\u6700\u5927\u90e8\u54c1\u76f4\u5f84<\/strong><\/td>\n<td>300 mm<\/td>\n<td>\u5916\u5f84\uff08OD\uff09<\/td>\n<\/tr>\n<tr>\n<td><strong>\u6700\u5927\u90e8\u54c1\u9577\u3055<\/strong><\/td>\n<td>1000 mm<\/td>\n<td>\u30bb\u30f3\u30bf\u9593\u8ddd\u96e2<\/td>\n<\/tr>\n<tr>\n<td><strong>\u76f4\u5f84\u516c\u5dee<\/strong><\/td>\n<td>+\/- 0.002 mm<\/td>\n<td>\u9ad8\u7cbe\u5ea6\u306f\u3081\u3042\u3044<\/td>\n<\/tr>\n<tr>\n<td><strong>\u771f\u5186\u5ea6\uff0f\u5186\u5f62\u5ea6<\/strong><\/td>\n<td>&lt; 0.001 mm\uff081\u30df\u30af\u30ed\u30f3\uff09<\/td>\n<td>\u9ad8\u901f\u30b7\u30e3\u30d5\u30c8\u306b\u4e0d\u53ef\u6b20<\/td>\n<\/tr>\n<tr>\n<td><strong>\u8868\u9762\u7c97\u3055\uff08Ra\uff09<\/strong><\/td>\n<td>0.2 \u00b5m \u2013 0.4 \u00b5m<\/td>\n<td>\u93e1\u9762\u4ed5\u4e0a\u3052<\/td>\n<\/tr>\n<tr>\n<td><strong>\u5bfe\u5fdc\u6750\u6599<\/strong><\/td>\n<td>\u713c\u5165\u308c\u92fc\uff0850 HRC\u4ee5\u4e0a\uff09\u3001\u8d85\u786c\u5408\u91d1\u3001\u30af\u30ed\u30e0\u3081\u3063\u304d\u30b7\u30e3\u30d5\u30c8<\/td>\n<td>\u8edf\u8cea\u6750\u6599\u306f\u30db\u30a4\u30fc\u30eb\u3092\u76ee\u8a70\u307e\u308a\u3055\u305b\u308b<\/td>\n<\/tr>\n<tr>\n<td><strong>\u52a0\u5de5\u30d0\u30ea\u30a8\u30fc\u30b7\u30e7\u30f3<\/strong><\/td>\n<td>\u4e21\u30bb\u30f3\u30bf\u3001\u30bb\u30f3\u30bf\u30ec\u30b9<\/td>\n<td>\u90e8\u54c1\u306e\u5f62\u72b6\u306b\u3088\u308b<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section 5: Process Types \/ Variants --><\/p>\n<div class=\"process-types\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\u7814\u524a\u65b9\u6cd5<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 20%;\">\u65b9\u6cd5<\/th>\n<th style=\"text-align: left; width: 40%;\">\u8aac\u660e<\/th>\n<th style=\"text-align: left; width: 40%;\">\u4e3b\u306a\u5229\u70b9\u3068\u7528\u9014<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\u4e21\u30bb\u30f3\u30bf<\/strong><\/td>\n<td>\u90e8\u54c1\u306f\u4e21\u7aef\u306e\u30bb\u30f3\u30bf\u7a74\u3067\u4fdd\u6301\u3055\u308c\u308b\u3002\u7825\u77f3\u304c\u6750\u6599\u3092\u9664\u53bb\u3059\u308b\u9593\u3001\u90e8\u54c1\u304c\u56de\u8ee2\u3059\u308b\u3002.<\/td>\n<td><strong>\u5229\u70b9\uff1a<\/strong> \u8907\u6570\u306e\u76f4\u5f84\u9593\u3067\u6700\u9ad8\u306e\u540c\u5fc3\u5ea6\u3002\u53d6\u308a\u5916\u3057\u3068\u518d\u88c5\u7740\u3092\u9ad8\u7cbe\u5ea6\u306b\u884c\u3048\u308b\u3002.<br \/>\n<strong>\u7528\u9014\uff1a<\/strong> \u7cbe\u5bc6\u30c9\u30e9\u30a4\u30d6\u30b7\u30e3\u30d5\u30c8\u3001\u30bf\u30fc\u30d3\u30f3\u30b9\u30d4\u30f3\u30c9\u30eb\u3002.<\/td>\n<\/tr>\n<tr>\n<td><strong>\u30bb\u30f3\u30bf\u30ec\u30b9\u7814\u524a<\/strong><\/td>\n<td>\u90e8\u54c1\u306f\u30bb\u30f3\u30bf\u3067\u4fdd\u6301\u3055\u308c\u305a\u3001\u7825\u77f3\u3068\u8abf\u6574\u30db\u30a4\u30fc\u30eb\u306e\u9593\u306b\u914d\u7f6e\u3055\u308c\u308b\u3002.<\/td>\n<td><strong>\u5229\u70b9\uff1a<\/strong> \u5927\u91cf\u751f\u7523\u306e\u5358\u7d14\u90e8\u54c1\u306b\u6975\u3081\u3066\u9ad8\u901f\u3002\u30bb\u30f3\u30bf\u7a74\u4e0d\u8981\u3002.<br \/>\n<strong>\u7528\u9014\uff1a<\/strong> \u30ce\u30c3\u30af\u30d4\u30f3\u3001\u30cb\u30fc\u30c9\u30eb\u30ed\u30fc\u30e9\u30fc\u3001\u5c0f\u578b\u30d4\u30b9\u30c8\u30f3\u3002.<\/td>\n<\/tr>\n<tr>\n<td><strong>\u30d7\u30e9\u30f3\u30b8\u7814\u524a<\/strong><\/td>\n<td>\u7825\u77f3\u306f\u90e8\u54c1\u306b\u6cbf\u3063\u3066\u30c8\u30e9\u30d0\u30fc\u30b9\u3059\u308b\u306e\u3067\u306f\u306a\u304f\u3001\u534a\u5f84\u65b9\u5411\u306b\u5207\u308a\u8fbc\u3080\uff08\u30d7\u30e9\u30f3\u30b8\u30ab\u30c3\u30c8\u306e\u3088\u3046\u306b\uff09\u3002.<\/td>\n<td><strong>\u5229\u70b9\uff1a<\/strong> \u7825\u77f3\u3092\u5f62\u72b6\u306b\u30c9\u30ec\u30c3\u30b7\u30f3\u30b0\u3059\u308c\u3070\u3001\u80a9\u90e8\u3084\u8907\u96d1\u306a\u30d7\u30ed\u30d5\u30a1\u30a4\u30eb\u3082\u7814\u524a\u3067\u304d\u308b\u3002.<br \/>\n<strong>\u7528\u9014\uff1a<\/strong> \u6bb5\u4ed8\u304d\u30b7\u30e3\u30d5\u30c8\u3001\u30d9\u30a2\u30ea\u30f3\u30b0\u30ec\u30fc\u30b9\u3002.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section 6: Design Guidelines & Material Compatibility --><\/p>\n<div class=\"design-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\u5186\u7b52\u7814\u524a\u306e\u8a2d\u8a08\u30ac\u30a4\u30c9\u30e9\u30a4\u30f3<\/h3>\n<p><strong>\u30bb\u30f3\u30bf\u7a74\uff1a<\/strong><br \/>\n\u300c\u4e21\u30bb\u30f3\u30bf\u300d\u7814\u524a\uff08\u6700\u3082\u7cbe\u5ea6\u306e\u9ad8\u3044\u65b9\u6cd5\uff09\u3067\u306f\u3001\u30b7\u30e3\u30d5\u30c8\u306f <strong>\u5fc5\u305a<\/strong> \u65cb\u524a\u6bb5\u968e\u3067\u4e21\u7aef\u306b\u30bb\u30f3\u30bf\u7a74\uff08\u901a\u5e3860\u00b0\uff09\u3092\u30c9\u30ea\u30eb\u52a0\u5de5\u3059\u308b\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002. <strong>\u30d2\u30f3\u30c8:<\/strong> \u56f3\u9762\u306b\u30bb\u30f3\u30bf\u7a74\u3092\u6307\u5b9a\u3057\u3001\u524a\u9664\u3057\u306a\u3044\u3067\u304f\u3060\u3055\u3044\u3002.<\/p>\n<p><strong>\u30b3\u30fc\u30ca\u30fcR\uff1a<\/strong><br \/>\n\u7814\u524a\u7825\u77f3\u306f\u92ed\u3044\u89d2\u3067\u76ee\u3053\u307c\u308c\u3092\u8d77\u3053\u3057\u307e\u3059\u3002\u30b7\u30e7\u30eb\u30c0\u30fc\u306b\u5bfe\u3057\u3066\u5b8c\u5168\u306a\u92ed\u89d290\u00b0\u306e\u89d2\u3092\u7dad\u6301\u3059\u308b\u3053\u3068\u306f\u4e0d\u53ef\u80fd\u3067\u3059\u3002. <strong>\u30d2\u30f3\u30c8:<\/strong> \u7825\u77f3\u304c\u9003\u3052\u3089\u308c\u308b\u3088\u3046\u3001\u30b7\u30e7\u30eb\u30c0\u30fc\u90e8\u306b\u30a2\u30f3\u30c0\u30fc\u30ab\u30c3\u30c8\uff08\u9003\u3052\u6e9d\uff09\u307e\u305f\u306f\u5927\u304d\u306a\u30d5\u30a3\u30ec\u30c3\u30c8\u534a\u5f84\u3092\u8a2d\u8a08\u3057\u3066\u304f\u3060\u3055\u3044\u3002.<\/p>\n<p><strong>\u65ad\u7d9a\u5207\u524a\uff1a<\/strong><br \/>\n\u30ad\u30fc\u6e9d\u3084\u30af\u30ed\u30b9\u7a74\u306e\u3042\u308b\u30b7\u30e3\u30d5\u30c8\u306e\u7814\u524a\u306f\u300c\u65ad\u7d9a\u5207\u524a\u300d\u3092\u5f15\u304d\u8d77\u3053\u3057\u3001\u7825\u77f3\u3092\u640d\u50b7\u3057\u305f\u308a\u632f\u52d5\u3092\u767a\u751f\u3055\u305b\u305f\u308a\u3059\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002. <strong>\u30d2\u30f3\u30c8:<\/strong> \u53ef\u80fd\u3067\u306f\u3042\u308a\u307e\u3059\u304c\u3001\u30b3\u30b9\u30c8\u304c\u5897\u52a0\u3057\u307e\u3059\u3002\u7814\u524a\u524d\u306b\u3053\u308c\u3089\u306e\u5f62\u72b6\u306e\u30d0\u30ea\u53d6\u308a\u3092\u78ba\u5b9f\u306b\u884c\u3063\u3066\u304f\u3060\u3055\u3044\u3002.<\/p>\n<p><strong>\u53d6\u308a\u4ee3\uff1a<\/strong><br \/>\n\u901a\u5e38\u3001\u76f4\u5f84\u306b0.2mm\uff5e0.4mm\u306e\u4f59\u8089\u3092\u6b8b\u3059\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002 <a href=\"https:\/\/www.jccncmachining.com\/ja\/%e6%a9%9f%e8%83%bd\/%e7%86%b1%e5%87%a6%e7%90%86\/\">\u71b1\u51e6\u7406<\/a> \u3053\u308c\u306f\u9178\u5316\u5c64\u3084\u8131\u70ad\u5c64\u306e\u4e0b\u307e\u3067\u7814\u524a\u3067\u304d\u308b\u3088\u3046\u306b\u3059\u308b\u305f\u3081\u3067\u3059\u3002.<\/p>\n<\/div>\n<p><!-- Section 7: Industry Applications --><\/p>\n<div class=\"industry-applications\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\u696d\u754c\u5225\u7528\u9014<\/h3>\n<p><strong>\u6cb9\u5727\u6a5f\u5668<\/strong><br \/>\n\u6cb9\u5727\u30b7\u30ea\u30f3\u30c0\u30fc\u7528\u30d4\u30b9\u30c8\u30f3\u30ed\u30c3\u30c9\u306f\u7814\u524a\u3055\u308c\u3001 <a href=\"https:\/\/www.jccncmachining.com\/ja\/%e6%a9%9f%e8%83%bd\/%e3%82%81%e3%81%a3%e3%81%8d\/\">\u30af\u30ed\u30e0\u30e1\u30c3\u30ad<\/a> \u9ad8\u5727\u4e0b\u3067\u5b8c\u5168\u306a\u30b7\u30fc\u30eb\u3092\u78ba\u4fdd\u3059\u308b\u305f\u3081\u3002.<\/p>\n<p><strong>\u81ea\u52d5\u8eca<\/strong><br \/>\n\u30ab\u30e0\u30b7\u30e3\u30d5\u30c8\u3068\u30af\u30e9\u30f3\u30af\u30b7\u30e3\u30d5\u30c8\u306f\u3001\u30a8\u30f3\u30b8\u30f3\u306e\u30bf\u30a4\u30df\u30f3\u30b0\u3068\u5186\u6ed1\u306a\u52d5\u4f5c\u3092\u78ba\u4fdd\u3059\u308b\u305f\u3081\u306b\u3001\u30ab\u30e0\u3068\u30b8\u30e3\u30fc\u30ca\u30eb\u306e\u7cbe\u5bc6\u306a\u5186\u7b52\u7814\u524a\u3092\u5fc5\u8981\u3068\u3057\u307e\u3059\u3002.<\/p>\n<p><strong>\u96fb\u52d5\u30e2\u30fc\u30bf\u30fc<\/strong><br \/>\n\u30e2\u30fc\u30bf\u30fc\u30b7\u30e3\u30d5\u30c8\u306f\u3001\u30ed\u30fc\u30bf\u304c\u30b9\u30c6\u30fc\u30bf\u306e\u30a8\u30a2\u30ae\u30e3\u30c3\u30d7\u3068\u5b8c\u5168\u306b\u540c\u5fc3\u3067\u56de\u8ee2\u3059\u308b\u3088\u3046\u306b\u7814\u524a\u3055\u308c\u3001\u9a12\u97f3\u3068\u632f\u52d5\u3092\u4f4e\u6e1b\u3057\u307e\u3059\u3002.<\/p>\n<p><strong>\u30d9\u30a2\u30ea\u30f3\u30b0<\/strong><br \/>\n\u30dc\u30fc\u30eb\u30d9\u30a2\u30ea\u30f3\u30b0\u306e\u5185\u8f2a\u3068\u5916\u8f2a\u306f\u3001\u6469\u64e6\u3092\u6700\u5c0f\u9650\u306b\u6291\u3048\u308b\u305f\u3081\u306b\u30df\u30af\u30ed\u30f3\u30ec\u30d9\u30eb\u306e\u771f\u5186\u5ea6\u516c\u5dee\u3067\u7814\u524a\u3055\u308c\u307e\u3059\u3002.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>\u5186\u7b52\u7814\u524a\uff08\u4e00\u822c\u306b\u5916\u5f84\u7814\u524a\u3068\u547c\u3070\u308c\u308b\uff09\u306f\u3001\u4e2d\u5fc3\u8ef8\u3092\u4e2d\u5fc3\u306b\u56de\u8ee2\u3059\u308b\u7269\u4f53\u306e\u5916\u9762\u3092\u6210\u5f62\u3059\u308b\u305f\u3081\u306b\u7528\u3044\u3089\u308c\u307e\u3059\u3002\u5b8c\u5168\u306a\u771f\u5186\u5ea6\uff08\u5186\u5f62\u5ea6\uff09\u3001\u540c\u5fc3\u5ea6\u3001\u7cbe\u5bc6\u306a\u76f4\u5f84\u7ba1\u7406\u304c\u6c42\u3081\u3089\u308c\u308b\u30b7\u30e3\u30d5\u30c8\u3001\u30a2\u30af\u30b9\u30eb\u3001\u30ed\u30fc\u30e9\u30fc\u306a\u3069\u306e\u5186\u7b52\u90e8\u54c1\u306e\u4ed5\u4e0a\u3052\u306b\u304a\u3051\u308b\u6700\u9069\u306a\u65b9\u6cd5\u3067\u3059\u3002.<\/p>\n<p>Jucheng Precision\u3067\u306f\u3001CNC\u5186\u7b52\u7814\u524a\u76e4\u3092\u4f7f\u7528\u3057\u3066\u713c\u5165\u308c\u92fc\u3084\u8d85\u786c\u5408\u91d1\u306e\u90e8\u54c1\u3092\u52a0\u5de5\u3057\u3066\u3044\u307e\u3059\u3002\u5de5\u5177\u5727\u529b\u306e\u75d5\u304c\u6b8b\u308b\u65cb\u524a\u3068\u306f\u7570\u306a\u308a\u3001\u7814\u524a\u3067\u306fRa 0.2\u00b5m\u3068\u3044\u3046\u5fae\u7d30\u306a\u8868\u9762\u4ed5\u4e0a\u3052\u3092\u5b9f\u73fe\u3057\u3001\u76f4\u5f84\u516c\u5dee\u3092+\/- 0.002mm\u306b\u4fdd\u3064\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002\u300c\u4e21\u30bb\u30f3\u30bf\u300d\u7814\u524a\u306b\u3088\u308b\u5358\u54c1\u8a66\u4f5c\u304b\u3089\u300c\u30bb\u30f3\u30bf\u30ec\u30b9\u300d\u7814\u524a\u306b\u3088\u308b\u5927\u91cf\u751f\u7523\u307e\u3067\u3001\u56de\u8ee2\u90e8\u54c1\u306e\u632f\u308c\u3084\u632f\u52d5\u3092\u6291\u3048\u3066\u6b63\u78ba\u306b\u52d5\u4f5c\u3059\u308b\u3053\u3068\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002.<\/p>","protected":false},"featured_media":422,"template":"","process_category":[40],"class_list":["post-421","process","type-process","status-publish","has-post-thumbnail","hentry","process_category-precision-grinding"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/process\/421","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/process"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/types\/process"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/media\/422"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/media?parent=421"}],"wp:term":[{"taxonomy":"process_category","embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/process_category?post=421"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}