{"id":394,"date":"2026-01-30T02:27:02","date_gmt":"2026-01-30T02:27:02","guid":{"rendered":"https:\/\/www.jccncmachining.com\/?post_type=process&#038;p=394"},"modified":"2026-01-30T02:27:02","modified_gmt":"2026-01-30T02:27:02","slug":"heat-treatment","status":"publish","type":"process","link":"https:\/\/www.jccncmachining.com\/ja\/%e6%a9%9f%e8%83%bd\/heat-treatment\/","title":{"rendered":"\u71b1\u51e6\u7406"},"content":{"rendered":"<p><!-- Section 3: Introduction & Capabilities --><\/p>\n<div class=\"process-introduction\">\n<p><span style=\"font-size: 24px; font-weight: bold;\">\u4e3b\u306a\u4ed5\u69d8<\/span><\/p>\n<\/div>\n<div class=\"key-specifications\">\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left;\">\u4ed5\u69d8<\/th>\n<th style=\"text-align: left;\">\u6280\u8853\u7bc4\u56f2<\/th>\n<th style=\"text-align: left;\">\u5099\u8003<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\u6700\u5927\u90e8\u54c1\u30b5\u30a4\u30ba<\/strong><\/td>\n<td>1000 mm x 800 mm x 800 mm<\/td>\n<td>Depends on furnace capacity<\/td>\n<\/tr>\n<tr>\n<td><strong>Hardness Range<\/strong><\/td>\n<td>20 HRC &#8211; 65 HRC<\/td>\n<td>Material dependent<\/td>\n<\/tr>\n<tr>\n<td><strong>\u6d78\u70ad\u6df1\u3055<\/strong><\/td>\n<td>0.1 mm &#8211; 2.0 mm<\/td>\n<td>For Case Hardening \/ Nitriding<\/td>\n<\/tr>\n<tr>\n<td><strong>\u5bfe\u5fdc\u6750\u6599<\/strong><\/td>\n<td>Carbon Steel, Alloy Steel, Tool Steel, Stainless (17-4PH), Aluminum<\/td>\n<td>Al uses Precipitation Hardening (T6)<\/td>\n<\/tr>\n<tr>\n<td><strong>\u6a19\u6e96\u30ea\u30fc\u30c9\u30bf\u30a4\u30e0<\/strong><\/td>\n<td>3\uff5e5\u65e5<\/td>\n<td>Includes batching and testing<\/td>\n<\/tr>\n<tr>\n<td><strong>Validation<\/strong><\/td>\n<td>Rockwell C (HRC), Brinell (HB)<\/td>\n<td>Hardness report provided<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section 5: Process Types \/ Variants --><\/p>\n<div class=\"process-types\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Heat Treatment Processes<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 20%;\">Process<\/th>\n<th style=\"text-align: left; width: 40%;\">\u8aac\u660e<\/th>\n<th style=\"text-align: left; width: 40%;\">\u4e3b\u306a\u5229\u70b9\u3068\u7528\u9014<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Hardening &amp; Quenching<\/strong><\/td>\n<td>Heating metal to a critical temperature and rapidly cooling (quenching) in oil, water, or air to &#8220;freeze&#8221; the microstructure.<\/td>\n<td><strong>\u5229\u70b9\uff1a<\/strong> Maximum hardness and strength.<br \/>\n<strong>\u7528\u9014\uff1a<\/strong> Tool steel dies, structural steel parts.<\/td>\n<\/tr>\n<tr>\n<td><strong>Case Hardening (Carburizing)<\/strong><\/td>\n<td>Diffusing carbon into the surface of low-carbon steel. Creates a hard outer &#8220;case&#8221; while keeping the core soft and tough.<\/td>\n<td><strong>\u5229\u70b9\uff1a<\/strong> Wear resistant surface + shock resistant core.<br \/>\n<strong>\u7528\u9014\uff1a<\/strong> Gears, shafts, pins, sprockets.<\/td>\n<\/tr>\n<tr>\n<td><strong>Vacuum Hardening<\/strong><\/td>\n<td>Performed in a vacuum environment to prevent oxidation and scaling. Provides a bright, clean finish.<\/td>\n<td><strong>\u5229\u70b9\uff1a<\/strong> Minimal distortion and no surface scale.<br \/>\n<strong>\u7528\u9014\uff1a<\/strong> High-precision medical parts, aerospace components.<\/td>\n<\/tr>\n<tr>\n<td><strong>Annealing \/ Normalizing<\/strong><\/td>\n<td>Heating and slow cooling to soften the metal, relieve internal stresses, and improve grain structure.<\/td>\n<td><strong>\u5229\u70b9\uff1a<\/strong> Makes material easier to machine and prevents warping.<br \/>\n<strong>\u7528\u9014\uff1a<\/strong> Pre-machining stock, welded parts.<\/td>\n<\/tr>\n<tr>\n<td><strong>Nitriding<\/strong><\/td>\n<td>Diffusing nitrogen into the surface to create a hard, wear-resistant layer without quenching. Low distortion.<\/td>\n<td><strong>\u5229\u70b9\uff1a<\/strong> High surface hardness (up to 70 HRC equivalent) and corrosion resistance.<br \/>\n<strong>\u7528\u9014\uff1a<\/strong> Mold cavities, precision screws.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section 6: Design Guidelines & Material Compatibility --><\/p>\n<div class=\"design-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Design Guidelines for Heat Treatment<\/h3>\n<p><strong>Leave Grinding Stock:<\/strong><br \/>\nHeat treatment causes internal stress release, leading to dimensional distortion (warping) and slight size changes. <strong>\u30d2\u30f3\u30c8:<\/strong> Always leave 0.2mm &#8211; 0.5mm of extra material (&#8220;grinding stock&#8221;) on critical features to be ground to final size <em>\u786c\u5316\u30b5\u30a4\u30af\u30eb<\/em> hardening.<\/p>\n<p><strong>Sharp Corners:<\/strong><br \/>\nAvoid sharp internal corners. They act as stress concentrators during the rapid cooling of quenching and can cause the part to crack. Use radiused corners whenever possible.<\/p>\n<p><strong>Uniform Cross-Sections:<\/strong><br \/>\nParts with drastic changes in thickness (e.g., a thick block connected to a thin fin) cool at different rates, leading to cracking. Design for uniform wall thickness or gradual transitions.<\/p>\n<p><strong>Thread Protection:<\/strong><br \/>\nFine threads can become brittle or distorted during hardening. It is often best to mask threads (if nitriding) or machine them after heat treat if the material isn&#8217;t too hard.<\/p>\n<\/div>\n<p><!-- Section 7: Industry Applications --><\/p>\n<div class=\"industry-applications\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\u696d\u754c\u5225\u7528\u9014<\/h3>\n<p><strong>Automotive Powertrain<\/strong><br \/>\nTransmission gears and crankshafts are Case Hardened to withstand constant friction wear while absorbing high torque loads without snapping.<\/p>\n<p><strong>Tool &amp; Die Making<\/strong><br \/>\nInjection molds made from H13 or P20 steel are Vacuum Hardened to withstand millions of cycles of high-pressure plastic injection without deforming.<\/p>\n<p><strong>\u822a\u7a7a\u5b87\u5b99<\/strong><br \/>\n17-4PH Stainless Steel parts are Precipitation Hardened (H900 condition) to achieve the maximum strength-to-weight ratio for flight control components.<\/p>\n<p><strong>\u91cd\u6a5f<\/strong><br \/>\nAxles and drive shafts undergo Induction Hardening (local heating) to harden just the bearing surfaces while leaving the rest of the shaft tough.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Heat Treatment is a controlled heating and cooling process used to alter the physical and mechanical properties of a metal without changing its shape. It is essential for increasing strength, hardness, toughness, or ductility. At Jucheng Precision, we manage a comprehensive range of heat treatment processes through our certified partners to ensure your CNC machined parts meet strict metallurgical requirements.<\/p>\n<p>From Annealing to improve machinability before cutting, to Vacuum Hardening for finishing high-precision mold components, we oversee the entire lifecycle. We verify all treated parts with HRC (Rockwell) hardness testing to ensure they meet your specifications (e.g., 58-60 HRC for tool steels) before final precision grinding.<\/p>","protected":false},"featured_media":395,"template":"","process_category":[38],"class_list":["post-394","process","type-process","status-publish","has-post-thumbnail","hentry","process_category-surface-finishes"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/process\/394","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/process"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/types\/process"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/media\/395"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/media?parent=394"}],"wp:term":[{"taxonomy":"process_category","embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ja\/wp-json\/wp\/v2\/process_category?post=394"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}