{"id":811,"date":"2026-03-12T11:39:14","date_gmt":"2026-03-12T03:39:14","guid":{"rendered":"https:\/\/www.jccncmachining.com\/?post_type=material_model&#038;p=811"},"modified":"2026-03-12T11:39:14","modified_gmt":"2026-03-12T03:39:14","slug":"pom-c","status":"publish","type":"material_model","link":"https:\/\/www.jccncmachining.com\/ar\/materials\/pom-delrin-acetal\/pom-c\/","title":{"rendered":"POM-C"},"content":{"rendered":"<p><!-- Section: Available Acetal Variants --><\/p>\n<div class=\"available-material-types\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Acetal \/ POM Material Variants<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left;\">\u0627\u0644\u062f\u0631\u062c\u0629<\/th>\n<th style=\"text-align: left;\">\u0627\u0644\u0627\u0633\u0645 \u0627\u0644\u0634\u0627\u0626\u0639<\/th>\n<th style=\"text-align: left;\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u0629<\/th>\n<th style=\"text-align: left;\">\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0646\u0645\u0648\u0630\u062c\u064a\u0629<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>POM-C<\/strong><\/td>\n<td>Acetal Copolymer<\/td>\n<td>Free of centerline porosity. Better resistance to hot water and strong bases than homopolymer. FDA\/USDA compliant.<\/td>\n<td>Food processing components, medical handles, plumbing fittings, manifolds.<\/td>\n<\/tr>\n<tr>\n<td><strong>Delrin 150<\/strong><\/td>\n<td>POM-H (\u0628\u0648\u0644\u064a\u0645\u0631 \u0645\u062a\u062c\u0627\u0646\u0633)<\/td>\n<td>Higher mechanical strength and stiffness. Superior fatigue resistance but prone to centerline porosity.<\/td>\n<td>Precision gears, high-load bushings, mechanical linkages.<\/td>\n<\/tr>\n<tr>\n<td><strong>Medical Grade POM-C<\/strong><\/td>\n<td>MT Acetal<\/td>\n<td>Specifically tested for biocompatibility (ISO 10993). Available in various colors for surgical sizing.<\/td>\n<td>Surgical trials, pharmaceutical equipment, diagnostic tools.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Machining Capabilities for POM-C --><\/p>\n<div class=\"machining-capabilities\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">POM-C Machining Capabilities<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 25%;\">\u0627\u0644\u0642\u062f\u0631\u0629<\/th>\n<th style=\"text-align: left; width: 45%;\">\u0627\u0644\u0648\u0635\u0641 \u0627\u0644\u0641\u0646\u064a<\/th>\n<th style=\"text-align: left; width: 30%;\">\u0645\u064a\u0632\u0629 Jucheng<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Void-Free Manifold Machining<\/strong><\/td>\n<td>Machining internal fluid channels in POM-C blocks without the risk of leaks through centerline porosity.<\/td>\n<td>Our specialized deep-hole drilling techniques ensure leak-proof performance for complex hydraulic and food-grade manifolds.<\/td>\n<\/tr>\n<tr>\n<td><strong>Food-Grade Precision Milling<\/strong><\/td>\n<td>Utilizing 5-axis CNC machines to produce complex geometries for food processing equipment under sanitary conditions.<\/td>\n<td>Jucheng ensures all POM-C parts are machined using food-safe lubricants, meeting strict FDA and EU 10\/2011 compliance standards.<\/td>\n<\/tr>\n<tr>\n<td><strong>Large Diameter Turning<\/strong><\/td>\n<td>Turning large POM-C bushings and rollers (up to 300mm) with high dimensional stability.<\/td>\n<td>Our rigid CNC lathes prevent material deflection, achieving perfect roundness and surface finishes (Ra 0.8\u03bcm) on large-scale components.<\/td>\n<\/tr>\n<tr>\n<td><strong>Color-Coded Sizer Production<\/strong><\/td>\n<td>Machining medical sizing components in various colors (Blue, Green, Yellow) for orthopedic trials.<\/td>\n<td>We provide high-fidelity surgical trial components with smooth edges and precise dimensions for medical device manufacturers.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Fabrication Guidelines --><\/p>\n<div class=\"fabrication-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Fabrication Guidelines for POM-C (Copolymer)<\/h3>\n<p><strong>Porosity Advantage:<\/strong><br \/>\nUnlike Delrin, POM-C is produced without centerline porosity. <strong>\u0646\u0635\u064a\u062d\u0629:<\/strong> This is critical for parts that require pressure sealing or where bacteria could be trapped in internal voids.<\/p>\n<p><strong>Chemical Resistance:<\/strong><br \/>\nPOM-C offers better resistance to long-term exposure to hot water and high-pH (alkaline) cleaners. <strong>\u0646\u0635\u064a\u062d\u0629:<\/strong> Always specify POM-C for food processing wash-down environments or commercial plumbing components.<\/p>\n<p><strong>\u0627\u0644\u0627\u0633\u062a\u0642\u0631\u0627\u0631 \u0627\u0644\u0623\u0628\u0639\u0627\u062f\u064a:<\/strong><br \/>\nPOM-C exhibits excellent dimensional stability due to low moisture absorption. <strong>\u0646\u0635\u064a\u062d\u0629:<\/strong> To achieve maximum precision, we recommend stress-relieved (annealed) stock, especially for large plates or asymmetrical parts.<\/p>\n<p><strong>Burr Management:<\/strong><br \/>\nWhile easy to machine, copolymer acetal can produce small, &#8220;fuzzy&#8221; burrs. <strong>\u0646\u0635\u064a\u062d\u0629:<\/strong> We utilize ultra-sharp, high-rake tools and optimized feed rates to ensure a clean, burr-free finish directly off the machine.<\/p>\n<\/div>\n<p><!-- Section: Application Scenarios --><\/p>\n<div class=\"application-scenarios\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629<\/h3>\n<p><strong>Food Processing Machinery<\/strong><br \/>\nScraper blades, rollers, manifolds, and wear strips that must be FDA compliant and resistant to hot water cleaning.<\/p>\n<p><strong>Medical Device Components<\/strong><br \/>\nInstrument handles, surgical trials, and diagnostic equipment parts requiring biocompatibility and chemical resistance.<\/p>\n<p><strong>Fluid Handling &amp; Plumbing<\/strong><br \/>\nValve bodies, pump components, and fittings for high-pressure fluid systems where sealing integrity is vital.<\/p>\n<p><strong>Automotive Fuel Systems<\/strong><br \/>\nComponents requiring resistance to fuels, solvents, and environmental moisture over long service lives.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Acetal \/ POM Material Variants Grade Common Name Key Characteristics Typical Applications POM-C Acetal Copolymer Free of centerline porosity. Better resistance to hot water and strong bases than homopolymer. FDA\/USDA compliant. Food processing components, medical handles, plumbing fittings, manifolds. Delrin 150 POM-H (Homopolymer) Higher mechanical strength and stiffness. Superior fatigue resistance but prone to centerline [&hellip;]<\/p>\n","protected":false},"featured_media":812,"template":"","meta":[],"class_list":["post-811","material_model","type-material_model","status-publish","has-post-thumbnail","hentry"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/material_model\/811","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/material_model"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/types\/material_model"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/media\/812"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/media?parent=811"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}