{"id":806,"date":"2026-03-12T11:12:10","date_gmt":"2026-03-12T03:12:10","guid":{"rendered":"https:\/\/www.jccncmachining.com\/?post_type=material_model&#038;p=806"},"modified":"2026-03-12T11:12:10","modified_gmt":"2026-03-12T03:12:10","slug":"ultem-2300-30-glass-filled-pei","status":"publish","type":"material_model","link":"https:\/\/www.jccncmachining.com\/ar\/materials\/ultem-pei\/ultem-2300-30-glass-filled-pei\/","title":{"rendered":"Ultem 2300 (PEI \u0645\u0639\u0632\u0632 \u0628\u0623\u0644\u064a\u0627\u0641 \u0632\u062c\u0627\u062c\u064a\u0629 30%)"},"content":{"rendered":"<p><!-- Section: Available Ultem Variants --><\/p>\n<div class=\"available-material-types\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\u0623\u0646\u0648\u0627\u0639 \u0645\u0627\u062f\u0629 Ultem (PEI)<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left;\">\u0627\u0644\u062f\u0631\u062c\u0629<\/th>\n<th style=\"text-align: left;\">\u0627\u0644\u0627\u0633\u0645 \u0627\u0644\u0634\u0627\u0626\u0639<\/th>\n<th style=\"text-align: left;\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u0629<\/th>\n<th style=\"text-align: left;\">\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0646\u0645\u0648\u0630\u062c\u064a\u0629<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Ultem 2300<\/strong><\/td>\n<td>\u0645\u0639\u0632\u0632 \u0628\u0623\u0644\u064a\u0627\u0641 \u0632\u062c\u0627\u062c\u064a\u0629 30%<\/td>\n<td>Highest rigidity and dimensional stability. Opaque tan color. Exceptional strength and heat resistance.<\/td>\n<td>Structural aerospace parts, high-load electrical connectors, automotive engine components.<\/td>\n<\/tr>\n<tr>\n<td><strong>Ultem 1000<\/strong><\/td>\n<td>\u0642\u064a\u0627\u0633\u064a \u063a\u064a\u0631 \u0645\u0639\u0632\u0632<\/td>\n<td>Amber translucent. Best dielectric strength and ductility. FDA compliant.<\/td>\n<td>Electrical insulators, medical manifolds, sight glasses.<\/td>\n<\/tr>\n<tr>\n<td><strong>Ultem 2100<\/strong><\/td>\n<td>10% \u0632\u062c\u0627\u062c\u064a \u0645\u0639\u0632\u0632<\/td>\n<td>Bridge between 1000 and 2300. Better finish than 2300 with increased stiffness.<\/td>\n<td>\u0623\u063a\u0644\u0641\u0629 \u0625\u0644\u0643\u062a\u0631\u0648\u0646\u064a\u0629\u060c \u062d\u0648\u0627\u0645\u0644 \u0635\u0646\u0627\u0639\u064a\u0629.<\/td>\n<\/tr>\n<tr>\n<td><strong>Ultem 9085<\/strong><\/td>\n<td>Aerospace FST Grade<\/td>\n<td>Optimized for high-performance with strict Flame, Smoke, and Toxicity compliance.<\/td>\n<td>Aircraft interior ducting, cabin brackets.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Machining Capabilities for Ultem 2300 --><\/p>\n<div class=\"machining-capabilities\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Ultem 2300 Machining Capabilities<\/h3>\n<table style=\"width: 100%; border-collapse: collapse; margin-bottom: 30px;\" border=\"1\" cellspacing=\"0\" cellpadding=\"10\">\n<thead>\n<tr style=\"background-color: #f2f2f2;\">\n<th style=\"text-align: left; width: 25%;\">\u0627\u0644\u0642\u062f\u0631\u0629<\/th>\n<th style=\"text-align: left; width: 45%;\">\u0627\u0644\u0648\u0635\u0641 \u0627\u0644\u0641\u0646\u064a<\/th>\n<th style=\"text-align: left; width: 30%;\">\u0645\u064a\u0632\u0629 Jucheng<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\u062a\u0641\u0631\u064a\u0632 \u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0643\u0634\u0637<\/strong><\/td>\n<td>The 30% glass fiber content is highly abrasive. We utilize diamond-coated (CVD) or sub-micrograin carbide tools to maintain sharp cutting edges.<\/td>\n<td>Prevents tool blunting and dimensional drift, ensuring consistent +\/- 0.02mm tolerances throughout long production runs.<\/td>\n<\/tr>\n<tr>\n<td><strong>High-Stability Structural Milling<\/strong><\/td>\n<td>Ultem 2300 has extremely low thermal expansion. We machine large structural frames and clips with zero warpage.<\/td>\n<td>Our rigid Haas and Mazak 5-axis centers handle the high-modulus material with ease, delivering superior geometric accuracy.<\/td>\n<\/tr>\n<tr>\n<td><strong>Precision Boring &amp; Drilling<\/strong><\/td>\n<td>Drilling high-tolerance fastener holes and bearing bores in rigid glass-filled PEI.<\/td>\n<td>Advanced tool geometry prevents &#8220;chipping&#8221; or splintering at the exit of the hole, ensuring clean, sharp edges.<\/td>\n<\/tr>\n<tr>\n<td><strong>In-Process Stress Relief<\/strong><\/td>\n<td>Utilizing proprietary annealing cycles between roughing and finishing passes.<\/td>\n<td>Crucial for maintaining absolute flatness on large Ultem 2300 plates used in semiconductor and aerospace equipment.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p><!-- Section: Fabrication Guidelines --><\/p>\n<div class=\"fabrication-guidelines\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">Fabrication Guidelines for Ultem 2300<\/h3>\n<p><strong>\u0625\u062f\u0627\u0631\u0629 \u062a\u0622\u0643\u0644 \u0627\u0644\u0623\u062f\u0648\u0627\u062a:<\/strong><br \/>\nThe glass fiber content acts like a grinding wheel. <strong>\u0646\u0635\u064a\u062d\u0629:<\/strong> We use high-speed spindles and lower feed rates to minimize friction heat while frequently inspecting tool sharpness to prevent material smearing.<\/p>\n<p><strong>Surface Finish Note:<\/strong><br \/>\nDue to the 30% glass reinforcement, Ultem 2300 will have a matte, tan appearance. <strong>\u0646\u0635\u064a\u062d\u0629:<\/strong> It cannot be polished to transparency like Ultem 1000. The focus should be on dimensional accuracy rather than optical clarity.<\/p>\n<p><strong>\u0627\u0633\u062a\u0631\u0627\u062a\u064a\u062c\u064a\u0629 \u0627\u0644\u062a\u0628\u0631\u064a\u062f:<\/strong><br \/>\nUltem is sensitive to petroleum-based fluids. <strong>\u0646\u0635\u064a\u062d\u0629:<\/strong> We use high-purity water-soluble coolants or specialized air-blast cooling to prevent chemical stress cracking and ensure environmental safety.<\/p>\n<p><strong>Workholding Rigidity:<\/strong><br \/>\nThe material is extremely stiff and can be brittle. <strong>\u0646\u0635\u064a\u062d\u0629:<\/strong> We use custom soft-jaws and vacuum tables to distribute clamping forces evenly, preventing the part from cracking under localized pressure.<\/p>\n<\/div>\n<p><!-- Section: Application Scenarios --><\/p>\n<div class=\"application-scenarios\">\n<h3 style=\"font-size: 24px; font-weight: bold; margin-bottom: 15px;\">\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629<\/h3>\n<p><strong>\u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u0641\u0636\u0627\u0626\u064a\u0629<\/strong><br \/>\nStructural airframe brackets, clips, and engine-zone components that require high strength-to-weight ratios and flame resistance.<\/p>\n<p><strong>High-Power Electronics<\/strong><br \/>\nConnector housings and standoff insulators for high-voltage systems where dimensional stability under heat is critical.<\/p>\n<p><strong>Medical Equipment (Reusable)<\/strong><br \/>\nInstrument housings and sterilization trays that must withstand repeated autoclaving without loss of mechanical strength.<\/p>\n<p><strong>Semiconductor Components<\/strong><br \/>\nWafer handling tools and test sockets that require high rigidity, low thermal expansion, and excellent chemical resistance.<\/p>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Ultem (PEI) Material Variants Grade Common Name Key Characteristics Typical Applications Ultem 2300 30% Glass Filled Highest rigidity and dimensional stability. Opaque tan color. Exceptional strength and heat resistance. Structural aerospace parts, high-load electrical connectors, automotive engine components. Ultem 1000 Standard Unfilled Amber translucent. Best dielectric strength and ductility. FDA compliant. Electrical insulators, medical manifolds, [&hellip;]<\/p>\n","protected":false},"featured_media":807,"template":"","meta":[],"class_list":["post-806","material_model","type-material_model","status-publish","has-post-thumbnail","hentry"],"_links":{"self":[{"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/material_model\/806","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/material_model"}],"about":[{"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/types\/material_model"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/media\/807"}],"wp:attachment":[{"href":"https:\/\/www.jccncmachining.com\/ar\/wp-json\/wp\/v2\/media?parent=806"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}